It is well-known that the mining industry in Chile and the world is searching for eco-friendly, highly efficient mineral treatments. This is because the content of toxic elements such as arsenic, antimony, and bismuth have increased in the copper concentrates in the last years. This trend has affected the market of this metal, as well as increased the potential of producing solid wastes that represent a threat to the environment. In this paper, a review on the fundamentals of the current treatments aimed at removing arsenic, antimony, and bismuth from copper concentrates under roasting conditions is presented. The literature survey included the research conducted from 2000 until now and is focused on the different types of roasting of copper concentrates reported in the literature. A summary of the experimental conditions and major findings of each work is discussed. Depending on the type of roasting, the behavior of arsenic, antimony, and bismuth species during the experiments is analyzed.
The accelerating global demand for cobalt, driven primarily by lithium-ion batteries, has intensified the search for alternative sources of supply. Mine tailings represent a promising secondary resource, particularly in regions with extensive mining histories such as Chile. This study evaluates cobalt leaching from copper tailings using a deep eutectic solvent (DES), choline chloride–citric acid (ChCl–CA), with controlled addition of hydrogen peroxide. The tailings were subjected to pretreatments (froth flotation, chlorination, and thermal roasting) and then leached with choline chloride–citric acid-based DES or H2SO4. Temperature, leaching time, and solid–liquid ratio were evaluated. Results show that roasting significantly enhanced cobalt recovery when followed by citric acid or DES leaching, reaching up to 100% Co recovery. Under optimized conditions, DES-based leaching was effective and selective in a polymetallic matrix and achieved recoveries comparable to or better than acid leaching without generating toxic emissions. Although flotation and chlorination had limited effects on overall recovery, the results demonstrate the viability of integrated and cleaner technologies for valorizing tailings that contain critical metals such as cobalt.
In this work, the roasting of an enargite mix was carried out in oxidative conditions. The temperature range of the study was 773–973 K. The mixture had a 4:6:6 molar ratio of enargite, magnetite and coal, respectively. The roasting was made in an open atmosphere. The time was 1 h for each isothermal test. The effect of temperature and weight loss were studied. The results indicate that the temperature affects the products. At 773–873 K, the copper phases were sulfates. When the temperature was increased to 973 K, all the present phases were oxidized, and no arsenic phase was encountered in the XRDs. Therefore, this process is an excellent alternative for roasting copper concentrates with enargite, removing arsenic in the gas phase and generating a calcine that could then go to lixiviation to finally recover the copper through electrowinning.