In this research, single phase delafossite CuCrO2 thin films were successfully synthesized using dual sputtering technique. A DC source was employed for the copper target, whereas the chromium target was sputtered using an RF source with oxygen acting as the reactive gas. The films were sputtered on a quartz substrate at 400 °C. The sputtering power for chromium was maintained at 100 W, while the power for copper ranged from 10 W to 40 W. Following deposition, the films were annealed in a nitrogen environment for 10 hours at 800 °C. XRD examination confirmed that single-phase CuCrO2 was achieved with a copper target power of 20 W. The findings of the XRD investigation were further validated by XPS analysis. Cu : Cr at% composition ratio of 1 : 1 : 04 was obtained when deposited at a power of 20 W. SEM grain sizes ranged from 100 nm to 150 nm optical studies indicated an optical transmission of 57.5% and a bandgap of 3.08 eV. The single-phase film demonstrated a resistivity of 28.6 Ω cm.
For the first time, the deposition of CuCrO2 thin films was carried out using a dual-target RF magnetron sputtering technique using Cu2O and Cr2O3 targets. The deposited films were subsequently annealed in N2 ambiance from 600–900 °C. This work reports that the electrical, optical, structural, and morphological properties of CuCrO2 thin films are significantly affected due to the variation in the annealing temperature. XRD analysis confirms the presence of single-phase CuCrO2 in the films annealed at 650 °C. The presence of Cu in the 1+ oxidation state in the phase pure CuCrO2 thin films was confirmed through XPS analysis. Further, through XPS analysis, the oxidation states of Cu and Cr, the full-width half maximum (FWHM), the peak positions, and their respective binding energies have been elucidated. SEM analysis confirms the promotion of nanocrystalline growth in the thin films as the annealing temperature was increased from 600 °C. The average grain size increased from 40.22 nm to 105.31 nm as the annealing temperature was increased from 600 to 900 °C. Optical studies conducted in the wavelength range of 200 nm to 800 nm revealed a decrease in the optical transmission and optical bandgap with an increase in the annealing temperature. The highest optical transmission of ~81% and an optical bandgap of 3.21 eV were obtained for the films depicting the delafossite nature of CuCrO2. The optical bandgap was found to vary between 3.16 eV and 3.74 eV for the films studied in this research. The lowest resistivity of 0.652 Ω cm was obtained for the films annealed at 650 °C. Transparent heterojunction diodes involving p-type delafossite copper chromium oxide (CuCrO2) and n-type indium tin oxide (ITO) were fabricated. The best diode depicted a cut-in voltage of 0.85 V, a very low leakage current of 1.24 x 10-8, an ideality factor of 4.13, and a rectification ratio of 2375.
For the first time, the effect of Cuprous Oxide (Cu2O) sputtering power variation on the radio frequency sputtered Copper Chromium Oxide (CuCrO2) thin films was studied. In this work, the sputtering power of Cr2O3 was held constant at 200 W while the sputtering power of the Cu2O target was varied from 10 to 100 W. The films were subsequently annealed at 650 °C in N2 ambiance. The effects of Cu2O sputtering power variation on the structural, optical, and electrical properties of the films have been reported in this work. X-ray diffractometer (XRD) study revealed that the single-phase delafossite structure of CuCrO2 was only obtained at Cu2O sputtering power of 50 W. X-ray photoelectron spectroscopy (XPS) analysis further established the results of XRD study where Cu in 1+ oxidation state was identified in thin films obtained at 50 W of Cu2O sputtering power. The optical studies were conducted in this work on all the post-deposition annealed films in the wavelength range of 200–800 nm. The energy dispersive x-ray spectroscopy (EDS) study revealed a near stoichiometric composition ratio of 1:1.06 of Cu:Cr at% obtained in the films sputtered with 50 W of Cu2O sputtering power. The highest optical transmission of ~81% and the highest optical bandgap of 3.21 eV were observed for single-phase CuCrO2 thin films. The optical transmission and the optical bandgap were found to decrease with an increase in the Cu2O sputtering power. The electrical study performed on all the post-deposition annealed films revealed that the lowest resistivity of 0.652 Ω-cm was identified for single-phase CuCrO2 thin films obtained at 50 W of Cu2O sputtering power.
CuGaO2 thin films were deposited using the RF magnetron sputtering technique using Cu2O and Ga2O3 targets. The films were deposited at room temperature onto a quartz slide. The sputtering power of Cu2O remained constant at 50 W, while the sputtering power of Ga2O3 was systematically varied from 150 W to 200 W. The films were subsequently subjected to annealing at temperatures of 850 °C and 900 °C in a nitrogen atmosphere for a duration of 5 h. XRD analysis on films deposited with a Ga2O3 sputtering power of 175 W annealed at 900 °C revealed the development of nearly single-phase delafossite CuGaO2 thin films. SEM images of films annealed at 900 °C showed an increasing trend in grain size with a change in sputtering power level. Optical studies performed on the film revealed a transmission of 84.97% and indicated a band gap of approximately 3.27 eV. The film exhibited a refractive index of 2.5 within the wavelength range of 300 to 450 nm.
Single-phase delafossite CuCrO2 thin films were successfully synthesized for the first time using a dual sputtering method involving Cu and Cr2O3 targets. The films were deposited on quartz substrates at 400 °C, with the copper target power varied between 5 W and 20 W, while the chromium oxide target power was fixed at 200 W. Post-deposition annealing was conducted in a nitrogen atmosphere at 650 °C for 5 hours. XRD and XPS analysis confirmed the formation of single-phase CuCrO2 films at a copper sputtering power of 10 W. SEM analysis showed an increasing trend in grain size with an increase in copper sputtering power. The optical studies showed a transmission rate of 57.36% along with a bandgap of 3.19 eV. The four-point probe measurement indicated the lowest resistivity of 18.6 Ω cm.