Metallic Cr and multilayer CrN/Cr coatings with a thickness of 2.5 µm were deposited onto E110 alloy by magnetron sputtering. Oxidation tests in air were performed at 1100 °C for 10–40 min. The gravimetric measurements showed better protective properties of multilayer CrN/Cr coatings in comparison with metallic Cr coating. Multilayer coating prevented fast Cr–Zr inter-diffusion by the formation of a ZrN layer beneath the coating. The appearance of ZrN is caused by interaction with nitrogen formed from the decomposition of CrN to Cr2N phases. Optical microscopy revealed a residual Cr layer for the multilayer CrN (0.25 µm)/Cr (0.25 µm) coating for all the oxidation periods. Additional in situ X-ray diffraction (XRD) studies of coated alloy during linear heating up to 1400 °C showed that the formation of the Cr2Zr phase in the case of multilayer coatings occurred at a higher (~150 °C) temperature compared to metallic Cr. Multilayer coatings can decrease the nitrogen effect for Zr alloy oxidation. Uniform and thinner oxide layers of Zr alloy were observed when the multilayer coatings were applied. The highest oxidation resistance belonged to the CrN/Cr coating with a multilayer step of 0.25 µm.
In the present work, porous composites were fabricated from pure Al2O3 and mixed Ti3AlC2/Al2O3 powder by slip casting and sintering. The effect of sintering temperature and different composition ratio on microstructure, phase composition, porosity and gas permeation flux of the fabricated materials was investigated. The microstructure and phase composition of the samples were analyzed by scanning electron microscopy and X-ray diffraction, respectively. The gas permeation experiments were performed using pure hydrogen at 0.1–0.9 MPa pressure. It is shown that a decrease in sintering temperature from 1500 to 1350 °C results in an increase in hydrogen permeation flux of the alumina from 5 to 25 mol/(m2 × s), which is due to higher pore size and overall porosity of the samples. Sintering of Ti3AlC2/Al2O3 powder mixtures leads to the formation of Al2O3, Al2TiO5 and TiO2 phases as a result of oxidation of the Ti3AlC2 phase, resulting in an increased pore size in the composites compared with pure alumina. The open porosity of composites increases from 3.4 to 40% with an increasing Ti3AlC2/Al2O3 ratio from 1/10 to 1/2, respectively. The composites with the highest porosity (40%) had a maximum permeation flux of 200 mol/(m2 × s). The changes in the bending strength of the alumina and composite samples, depending on the microstructure and porosity, were also discussed. The investigated composites are considered promising materials for hydrogen separation membrane supports.
This article considers the possibility of using a magnetron-deposited coating for the protection of hafnium hydrides at high temperatures as a material for neutron control rods. We describe the role of TiC coating in the high-temperature behavior of hafnium hydrides in a vacuum. A 1 µm thick TiC coating was deposited through magnetron sputtering on the outer surface of disk HfHx samples, and then in situ X-ray diffraction (XRD) measurements of both the uncoated and TiC-coated HfHx samples were performed using synchrotron radiation (at a wavelength of 1.64 Å) during linear heating, the isothermal stage (700 and 900 °C), and cooling to room temperature. Quadrupole mass spectrometry was used to identify the hydrogen release from the uncoated and TiC-coated hafnium hydride samples during their heating. We found the decomposition of the HfH1.7 phase to HfH1.5 and Hf and following hafnium oxidation after the significant decrease in hydrogen flow in the uncoated HfHx samples. The TiC coating can be used as a protective layer for HfHx under certain conditions (up to 700 °C); however, the fast hydrogen release can occur in the case of a coating failure. This study shows the temperature range for the possible application of TiC coatings for the protection of hafnium hydride from hydrogen release.