Connections made with laterally loaded dowel-type fasteners are important details in timber structures. According to Eurocode 5, their load-carrying capacity can be calculated with the so-called European Yield Model (EYM) and simplified rules for the determination of slip-moduli are given. The slip modulus is given as a mean value for the serviceability limit state and a simple reduction of slip modulus in the ultimate limit state is given in addition. Despite these simple regulations, it is well known that connections with dowel-type fasteners show a considerable non-linear load-deformation behaviour with different degrees of ductility. This ductility can enable the load redistribution in complex and statically undetermined structures and allow to achieve higher capacities compared to linear elastic design. In the paper, the deformation behaviour of connections with laterally loaded dowels dowel-type fasteners is studied based on more than 750 test results of bolted connections. The parameters influencing the slip-modulus, ductility ratio, and ultimate deformation are evaluated. It is focused on the effects of these parameters and the resulting variability in deformation behaviour. Recommendations are given on how different levels of ductility and deformation capacity can be achieved in dependency of the spacing of fasteners and other geometrical parameters.
This paper describes results and analysis of experimental testing of entire and partial compression strength and stiffness parallel to the grain of solid timber (Japanese cedar). To investigate the spreading effects, the size effect of strength and stiffness, and the mechanism of the damage zone located close to the loading plates, tests on 90 specimens were performed. As a result, it was observed that damage zones existed near the loading plates. The observed spreading effects in the compression parallel to the grain were very small which justifies neglecting them regarding strength and stiffness. Although a presence of a size effect of the compression strength parallel to the grain of glulam specimens with knots was reported, the compression strength parallel to the grain of solid wood specimens without knots does not have a size effect. The height and width of the cross-section of the specimens have an influence on the damage zones and, hence, on the effective modulus of elasticity of the full height of the specimens. The compression strength has a correlation with the density of the timber and the width of the annual rings.
Dowel-type connections in timber structures should be typically designed in a way that, if the load bearing capacity is exceeded, desirable ductile failure should likely occur, i.e. yielding of the metal dowel or embedment of the timber. However, the probability of brittle failures cannot be completely avoided in many cases. If the connection is loaded parallel to the grain direction, splitting, row-shear, plug/block shear and tensile failure are examples of such brittle failure modes. To ensure a beneficial structural performance locally and sufficient structural robustness globally, the probability of such brittle failures should be kept at a sufficiently low level. However, in the current version of EN1995, the probability of such failure is not considered explicitly. The final aim of the presented research study is to develop a rational approach for the consideration of brittle failure in timber connections with dowel-type fasteners and steel plates loaded parallel to the grain, consistently with the partial factor method. As a first step, a probabilistic model has been used to study the susceptibility to brittle failure and provide a rational basis for the calibration of a “brittle overstrength factor”. The results of this study are reported in the current contribution.
This paper describes results and analysis of experiment of compression behavior parallel to grain of glulam (Norway Spruce, Japanese cedar, and Japanese cypress), especially in damage zones near loading plates and joints. To investigate the influence factors of physical properties and the mechanism of the damage zone near the loading plates or the joints, compression tests on 90 specimens and surface-measurement tests on 48 specimens were performed. As a result, it was observed that damage zones existed near the loading plates and the joints. The lengths of the damage zone of wood–wood joints are larger than that of wood–steel joints. The length of the damage zone was independent of the load and the height of the specimens. However, the length of the damage zone and its scatter increase as the width of the cross-section increases, as does the roughness on the contact surface. It was considered that the cause of the damage zone is the roughness on the contact surface and the length of the damage zone depends on the roughness on the contact surface. Therefore, the length of the damage zone depends on the processing accuracy on the contact surface and has an increasing trend as the contact-surface area increases. There was the size effect of the height of the specimens on the compressive strength because of knots.