A series of Ce-doped α-MnO2 catalysts (CeXMn1−XO2, x = 0.04, 0.07, 0.10) were synthesized by a simple in situ hydrothermal method. It was confirmed by characterization methods such as XRD, Raman, N2 adsorption–desorption and SEM confirmed that the introduction of Ce significantly regulated the microstructure of α-MnO2, specifically manifested as the reduction in grain size, the increase in defect sites, the increase in Mn-O bond length and altered morphological structure. H2-TPR, O2-TPD and XPS analyses further revealed the strong interaction between Mn and Ce, accompanied by significant electron transfer (Ce3+ + Mn4+ → Ce4+ + Mn3+), thereby promoting the formation of Mn3+ species. In the test of toluene catalytic oxidation performance, Ce0.07Mn0.93O2 exhibited the most excellent catalytic activity (T100 = 280 °C), while also having good thermal stability and water resistance. Furthermore, the degradation pathways of toluene were analyzed by TD-GC-MS technology: Toluene → Benzene → Benzaldehyde → Maleic anhydride → CO2 and H2O.
CeVO4-V2O3 composites were prepared by simple hydrothermal method, and the effects of ethylene glycol(EG) on the products were studied by XRD, N2 adsorption–desorption, SEM, EDS, XPS, PL and UV-vis spectra. The characterization reveals a slight decrease in surface area and a slight enhancement of visible light absorption in the final sample, while the crystalline phase, morphology and separation efficiency of the collective carriers are severely affected by the EG. At the same time, the photocatalytic effect of CeVO4-V2O3 composites was evaluated by the degradation rate of methylene blue (MB) under simulated visible light. The sample for 10 mL EG obtained the highest efficiency of 96.9%, while the one for 15 mL EG showed the lowest efficiency of 67.5% within 300 min. The trapping experiments and ESR experiment showed that the contribution of active species to the photocatalytic degradation of MB was ∙OH > h+ > ∙O2− in descending order, and a possible degradation mechanism was proposed.
The design of efficient catalysts is vital for the application of catalytic oxidation technology in the removal of gaseous pollutants. Herein, a series of MnOx catalysts with the typical Mn2O3 crystal structure was synthesized via the high-temperature pyrolysis method by using Mn-based metal–organic frameworks (Mn-MOFs) with various morphologies as the precursors. The physicochemical properties of these Mn-MOF-derived MnOx samples were investigated by various characterization techniques, including X-ray diffraction (XRD), thermogravimetry (TG), N2 adsorption–desorption, scanning electron microscope (SEM), and H2 temperature-programmed reduction (H2-TPR), and their catalytic activity was evaluated for catalytic CO degradation. The results showed that the Mn-MOF with leaf-like morphology, derived MnOx-Leaf, presented the optimal catalytic CO oxidation performance (T98 = 214 °C), stability, and reusability. Characterization results showed that the different Mn-MOF-derived MnOx catalysts possessed different physical–chemical properties. The superior catalytic activity of MnOx-Leaf for CO degradation was ascribed to its large surface area and pore size, better low-temperature redox properties, and high H2 consumption, which promoted the adsorption and activation of the CO and gaseous oxygen molecules, improving CO oxidation. Finally, the possible CO degradation pathway was evaluated by in situ diffuse reflectance Fourier transform infrared spectroscopy (DRIFTS), which showed that gaseous CO and O2 were adsorbed on the surface of the catalyst and oxidized to form surface carbon-related species (bicarbonate and carbonate), and finally converted to CO2.
The regulation of the active sites of a catalyst is important for its application. Herein, a series of Ag1Cux/SBA-15 catalysts with different molar ratios of Ag to Cu were synthesized via the impregnation method, and the active sites of Ag1Cux were regulated via various pretreatment conditions. These as-prepared Ag1Cux/SBA-15 catalysts were characterized by many technologies, and their catalytic performance was estimated through CO catalytic oxidation. Among these catalysts, Ag1Cu0.025/SBA-15, with a Ag/Cu molar ratio of 1:0.025 and pretreated under the condition of 500 °C O2/Ar for 2 h, followed by 300 °C H2 for another 2 h, presented optimal CO degradation performance, which could realize the oxidation of 98% CO at 34 °C (T98 = 34 °C). Meanwhile, Ag1Cu0.025/SBA-15 also displayed great reusability. Characterization results, such as X-ray diffraction (XRD), ultraviolet–visible diffuse reflectance spectra (UV-vis DRS), temperature-programmed H2 reduction (H2-TPR), and physical adsorption, suggested that the optimal catalytic performance of Ag1Cu0.025/SBA-15 was ascribed to its high interspersion of Ag nanoparticles, better low-temperature reduction ability, the interaction between Ag and Cu, and its high surface area and large pore volume. This study provides guidance for the regulation of active sites for low-temperature catalytic degradation.
In this work, a series of defective Co3O4 catalysts (Al@Co3O4−x, x = 4, 6, 8 mmol/L, representing the NaOH concentration) were prepared by Al doping and NaOH etching via hydrothermal method for ethyl acetate degradation. The results indicated that the Al@Co3O4-6 catalyst presented the optimal catalytic performance for ethyl acetate degradation (T90 = 207 °C). The results of many characterizations, such as X-ray diffraction (XRD), scanning electron microscope (SEM), Fourier transform infrared (FT-IR) spectra, Raman, and temperature-programmed H2 reduction (H2-TPR), etc., showed that the Al doping and NaOH etching induced the production of defects and oxygen vacancies in the catalyst, improved the surface area, boosted the low-temperature reducibility, and promoted the low-temperature oxygen species desorption, which enhanced ethyl acetate oxidation over Al@Co3O4-6. Importantly, the possible ethyl acetate degradation pathway was revealed by in situ diffuse reflectance infrared Fourier transform spectroscopy (DRIFTS), in the sense that the adsorbed ethyl acetate was gradually oxidized to ethanol and acetaldehyde, acetic acid, formate, and finally to CO2 and H2O.