Surface coating has become an effective approach to improve the electrochemical performance of Ni-rich cathode materials. In this study, we investigated the nature of an Ag coating layer and its effect on electrochemical properties of the LiNi0.8Co0.1Mn0.1O2 (NCM811) cathode material, which was synthesized using 3 mol.% of silver nanoparticles by a facile, cost-effective, scalable and convenient method. We conducted structural analyses using X-ray diffraction, Raman spectroscopy, and X-ray photoelectron spectroscopy, which revealed that the Ag nanoparticle coating did not affect the layered structure of NCM811. The Ag-coated sample had less cation mixing compared to the pristine NMC811, which could be attributed to the surface protection of Ag coating from air contamination. The Ag-coated NCM811 exhibited better kinetics than the pristine one, which is attributed to the higher electronic conductivity and better layered structure provided by the Ag nanoparticle coating. The Ag-coated NCM811 delivered a discharge capacity of 185 mAh·g−1 at the first cycle and 120 mAh·g−1 at the 100th cycle, respectively, which is better than the pristine NMC811.
Elemental doping for substituting lithium or oxygen sites has become a simple and effective technique to improve the electrochemical performance of layered cathode materials. Compared with single-element doping, this work presents an unprecedented contribution to the study of the effect of Na+/F− co-doping on the structure and electrochemical performance of LiNi1/3Mn1/3Co1/3O2. The co-doped Li1-zNazNi1/3Mn1/3Co1/3O2-zFz (z = 0.025) and pristine LiNi1/3Co1/3Mn1/3O2 materials were synthesized via the sol–gel method using EDTA as a chelating agent. Structural analyses, carried out by X-ray diffraction, Raman spectroscopy, and X-ray photoelectron spectroscopy, revealed that the Na+ and F− dopants were successfully incorporated into the Li and O sites, respectively. The co-doping resulted in larger Li-slab spacing, a lower degree of cation mixing, and the stabilization of the surface structure, which substantially enhanced the cycling stability and rate capability of the cathode material. The Na/F co-doped LiNi1/3Mn1/3Co1/3O2 electrode delivered an initial specific capacity of 142 mAh g−1 at a 1C rate (178 mAh g−1 at 0.1C), and it maintained 50% of its initial capacity after 1000 charge–discharge cycles at a 1C rate.
This work deals with the comparative analysis of fluoride coatings, i.e., 5 wt.% AlF3 and LiF, applied as surface layer of Li-rich Li1.2Ni0.13Co0.13Mn0.54O2 (LNCM) layered oxides synthesized via facile and cost-effective sol–gel route. The detailed structural and morphological characterizations demonstrate that AlF3 and LiF deposits have a pivotal role in enhancing the electrochemical properties of LNCM. These electrochemical properties include galvanostatic charge–discharge (GCD), differential capacity (dQ/dV), electrochemical impedance spectroscopy (EIS), and area-specific impedance (ASI). A much lower decay of the discharge capacity of 0.22 and 0.25 mAh g−1 per cycle was obtained for AlF3- and LiF-coated LMNC, respectively, after 100 charge/discharge cycles at 0.1 C compared with 0.42 mAh g−1 per cycle for pristine LNCM. Results evidence the non-evolution of the charge transfer resistance, enhanced lithium-ion kinetics and stabilization of electrode/electrolyte interface during cycling.
This study throws more light on the new Co-free and Ni-rich LiNi0.8Mn0.1Fe0.1O2 cathode material for lithium-ion batteries. This cobalt-free cathode material is prepared using a two-step process: the formation of an oxalate precursor by co-precipitation followed by a solid-state reaction with lithium hydroxide and iron citrate. The physico-chemical properties of LiNi0.8Mn0.1Fe0.1O2 are characterized using X-ray diffraction, Raman spectroscopy, scanning electron microscopy, thermal gravimetric analysis, and energy dispersive X-ray spectroscopy, respectively. The LiNi0.8Mn0.1Fe0.1O2 electrode tested at at C/2 rate within voltage window of 3.0-4.4 V vs. Li+/Li delivers a specific capacity of ~80 mAh g-1 and retain about 45% of its initial capacity after 100 cycles.