This study describes the fabrication of nanocomposites using electrospinning technique from poly lactic acid (PLA) and nano-hydroxyapatite (n-HAp). The prepared electrospun PLA-nHAP nanocomposite is intended to be used for drug delivery application. A hydrogen bond in between nHAp and PLA was confirmed by Fourier transform infrared (FT-IR) spectroscopy. Degradation study of the prepared electrospun PLA-nHAp nanocomposite was conducted for 30 days both in phosphate buffer solution (PBS) of pH 7.4 and deionized water. The degradation of the nanocomposite occurred faster in PBS in comparison to water. Cytotoxicity analysis was conducted on both Vero cells and BHK-21 cells and the survival percentage of both cells was found to be more than 95%, which indicates that the prepared nanocomposite is non-toxic and biocompatible. Gentamicin was loaded in the nanocomposite via an encapsulation process and the in vitro drug delivery process was investigated in phosphate buffer solution at different pHs. An initial burst release of the drug was observed from the nanocomposite after 1 to 2 weeks for all pH media. After that, a sustained drug release behavior was observed for the nanocomposite for 8 weeks with a release of 80%, 70% and 50% at pHs 5.5, 6.0 and 7.4, respectively. It can be suggested that the electrospun PLA-nHAp nanocomposite can be used as a potential antibacterial drug carrier for sustained drug release in dental and orthopedic sector.
15 October 2019 in Journal of Applied Polymer Science
In this study, hyperbranched polymers were explored as matrix modifiers to create E‐glass fiber (GF) reinforced polymer composites with enhanced mechanical properties. Hyperbranched polymers have lower viscosities than their linear equivalents, potentially providing enhanced fiber wet out leading to improved stress transfer. Hyperbranched (HB), hydrogenated hyperbranched (H‐HB), and linear functional (LF) divinyl benzene were blended with linear polystyrene (LP) to form a range of composite matrix formulations. Blends of the HB and LP polymers were used since the neat hyperbranched polymers alone proved to be highly brittle when formed into a film. A neat LP‐GF composite was also prepared as control. Of the three matrix modifiers considered, only the H‐HB provided an improvement in mechanical properties in comparison to LP‐GF. With the addition of 10 and 20 wt% H‐HB, respectively, the flexural modulus increased by 25% (p < 0.05) and 36% (p < 0.05) and flexural strength increased by 15% (p < 0.05) and 31% (p < 0.005). The enhanced mechanical properties were attributed to better fiber wetting along with crystallization observed with the addition of 20 wt% H‐HB. The non‐reactive ethyl (CH2CH3) chain end group of the macromolecular H‐HB resulted in a plasticizing effect, which in turn improved its wettability. The LP:HB polymer blends, on the other hand, underwent crosslinking due to the presence of the vinyl (CHCH2) chain ends leading to poor wettability in comparison to the LP:H‐HB and LP:LF blended films and hence lower mechanical properties.
Microwave (MW) assisted rapid synthesis procedure was implemented to prepare polyvinyl alcohol/n-hydroxyapatite bio-composite scaffolds (PVA/agarose/n-HAp (PAH)) using agarose as a crosslinker. The MW-assisted synthesis with two heating cycles (600 and 900 W) allowed the fastest formation and homogenous distribution of n-HAp within the polymeric matrix. The freeze-drying process was used to fabricate a porous bio-composite. The average crystallite size of the synthesized n-HAp was 9.7 nm. The MW-assisted method took only 8–10 min to synthesize n-HAp, while the conventional method took 24 h. The obtained bio-composites were highly porous and the porosity obtained for PAH1 and PAH3 were 62 % and 65 %, respectively. However, the porosity decreased to nearly half (31 % and 38 % for PAH2 and PAH4, respectively) while doubling the n-HAp content. The highest swelling was obtained for PAH3 in both water and PBS at 167 % and 498 %. The highest tensile strength and modulus were obtained for PAH1 at 29 MPa and 1.4 Gpa which is higher than the tensile strength and modulus of Conv. PAH (20 MPa and 0.74 GPa, respectively) and many porous PVA/HAp scaffolds reported. The fabricated scaffolds are biocompatible, porous, possess good mechanical properties, and are suitable for application in bone tissue engineering.