Aluminum is a significant impurity in the ion-adsorption rare earth ore. The changes in the occurrences of aluminum have a great influence on the leaching of the rare earth ore. In this paper, the column leaching method was employed using magnesium sulfate as a leaching agent to investigate the effects of pH and magnesium sulfate concentration in the leaching agent on the leaching of aluminum and rare earths. The results show that at low magnesium sulfate concentrations, the leaching of rare earths is greatly enhanced, while the leaching of aluminum is not significantly affected by a decrease in the pH of leaching agent. At high magnesium sulfate concentrations, a slight increase in the leaching of rare earths is observed, accompanied by a significant increase in the leaching of aluminum upon decreasing the pH of the leaching agent. The leaching behavior of aluminum is related to the changes in the occurrences of aluminum during the leaching process. At low magnesium sulfate concentrations, low pH promotes the transition of Hy-Al to Sol-Al, but due to the low Mg2+ concentration in the leaching agent, Sol-Al is back-adsorbed onto the clays and transformed into Ex-Al, resulting in no significant increase in the aluminum content in the leach solution. However, at higher magnesium sulfate concentrations, aluminum in the leach solution comes mainly from the transformation of Ex-Al. Lowering the pH of the leaching agent can significantly promote the transition of Hy-Al to Sol-Al, thereby greatly increasing the aluminum content in the leach solution. The above results provide theoretical support for the optimization of the in situ leaching of ion-adsorption rare earth ore using magnesium sulfate.
The precipitation process of rare earth from a rare earth chloride solution using magnesium bicarbonate yields a dilute magnesium chloride (MgCl2) solution. The dilute MgCl2 solution can only be concentrated to a maximum concentration of about 70 g/L by conventional reverse osmosis (RO), which is insufficient for recycling. Low-salt-rejection reverse osmosis (LSRRO) allows for a higher concentration of brine while operating at moderate pressures. However, research on LSRRO for the concentration of MgCl2 solution is still at an initial stage. In this study, polyamide RO membranes were treated with sodium hypochlorite (NaClO) to prepare low-salt-rejection membranes. The effects of NaClO concentration, pH, and chlorination time on the membrane properties were investigated. Under alkaline chlorination conditions, the membrane’s salt rejection decreased, and water flux increased with increasing NaClO concentration and chlorination time. This can be explained by the hydrolysis of polyamide in the alkaline solution to form carboxylic acids and amines, resulting in a decrease in the crosslinking degree of polyamide. The low-salt-rejection membrane was prepared by exposing it to a NaClO solution at a concentration of 15 g/L and a pH of 11 for 3 h, and the salt rejection of MgCl2 was 50.7%. The MgCl2 solution with a concentration of 20 g/L was concentrated using multi-stage LSRRO at the pressure of 5 MPa. The concentration of the concentrated brine reached 120 g/L, which is 87% higher than the theoretical maximum concentration of 64 g/L for conventional RO at the pressure of 5 MPa. The specific energy consumption (SEC) was 4.17 kWh/m3, which decreased by about 80% compared to that of mechanical vapor recompression (MVR). This provides an alternative route for the efficient concentration of a diluted MgCl2 solution with lower energy consumption.