Qi Chen

Mr. Qi Chen


Research Focus & Metrics

Academic Career Length

1Year (2026-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
15 April 2026 in Polymers
Verified
Journal Article
Open access
PDF file
ZHZhanfeng Hou Zhanfeng Hou
Zhanfeng Hou Zhanfeng Hou
YHYahe Hou
Yahe Hou
QCQi Chen
Qi Chen
HYHui Yang
Hui Yang
HWHongzhen Wang
Hongzhen Wang
ZXZhenxiang Xin
Zhenxiang Xin
To address the pronounced self-aggregation of highly loaded silica in the aqueous phase and the substantial filler loss occurring during the flocculation stage of latex compounding, this study introduces disaggregated and activated sepiolite possessing a spatial confinement effect as both a suspension stabilizer and a synergistic reinforcing component. On this basis, a multiscale natural rubber (NR)/silica/sepiolite composite system was constructed via a latex compounding route. Rheological characterization combined with static sedimentation observations revealed that the percolation threshold of the sepiolite is approximately 0.8 wt%. When the sepiolite content exceeds 1.0 wt%, its fibrous morphology enables the formation of a continuous three-dimensional network, which physically constrains silica particles and effectively suppresses their sedimentation and self-aggregation in the aqueous medium. Guided by this percolation behavior, a stable silica/sepiolite hybrid slurry was subsequently wet-mixed with natural rubber latex, and the influence of sepiolite loading on silica retention during flocculation, as well as on the resulting composite properties, was systematically examined. The results demonstrate that incorporation of sepiolite reduces filler loss during flocculation, with the loss rate decreasing from 4.7% to 1.1%. The Payne effect, SEM, dynamic and static mechanical analyses indicate that an appropriate sepiolite dosage promotes dispersion of silica within the rubber matrix while simultaneously strengthening filler–rubber interfacial interactions. Accordingly, tensile and tear strengths are increased from 32.1 to 35.5 MPa and from 92.3 to 133.4 N·mm−1, respectively, while wet skid resistance is preserved and both rolling resistance and wear resistance are further improved. The findings of this work establish a practical and efficient strategy for the wet preparation of high-performance NR/silica composites.