With the increasing demand for eco-friendly, non-petroleum-based natural rubber (NR) products, sepiolite, a naturally abundant, one-dimensional clay mineral, has been identified as a suitable material for reinforcing NR through the latex compounding method. To create superior NR/sepiolite composites, three silane coupling agents with different functional groups were used to modify sepiolite in situ via grafting or adsorption during the disaggregation and activation of natural sepiolite, which were subsequently mixed with natural rubber latex (NRL) to prepare the composites. The results showed that the modified sepiolite improved the dispersion and interfacial bonding strength with the rubber matrix. VTES-modified sepiolite containing C=C groups slightly improved the performance but retarded the vulcanization of the NR composites, and MPTES and TESPT-modified sepiolites containing -SH and −S4− groups, respectively, effectively accelerated vulcanization, inducing the composites to form a denser crosslink network structure, and exhibiting excellent dynamic and static properties, such as the modulus at a 300% increase from 8.82 MPa to 16.87 MPa, a tear strength increase from 49.6 N·mm−1 to 60.3 N·mm−1, as well as an improved rolling resistance and abrasive resistance of the composites. These findings demonstrate that modified sepiolite can be used to produce high-quality NR/sepiolite composites with enhanced properties.
Zinc oxide is a crucial component in rubber products, but its excessive usage can lead to environmental damage. As a result, reducing the amount of zinc oxide in products has become a critical issue that many researchers aim to address. This study employs a wet precipitation method to prepare ZnO particles with different nucleoplasmic materials, resulting in ZnO with a core–shell structure. The prepared ZnO underwent XRD, SEM, and TEM analysis, indicating that some of the ZnO particles were loaded onto the nucleosomal materials. Specifically, ZnO with a silica core–shell structure demonstrated 11.9% higher tensile strength, 17.2% higher elongation at break, and 6.9% higher tear strength compared to the indirect method of ZnO preparation. The core–shell structure of ZnO also helps reduce its application in rubber products, thereby achieving the dual objective of protecting the environment and improving the economic efficiency of rubber products.
Nowadays, waste tires have emerged as one of the most significant sources of environmental pollution. To address this issue, pyrolysis has become a widely adopted method. The continuous rotary kiln reactor has particularly gained popularity in industrial production for pyrolysis due to its suitability. In order to guide the development of new industrial continuous rotary kiln reactors and achieve high-performance pyrolytic carbon black (CBp), this study was conducted to investigate the relationship between the physical and chemical characteristics of CBp and pyrolysis temperature. The elevated-temperature procedure led to a reduction in DBP values from 90 to 70 mL/100 mg, accompanied by a rise in the specific surface area from 63 to 77 m2/g. The augmentation of pyrolysis temperature was noted to induce the agglomeration of CBp particles, thereby negatively impacting their dispersion within polymer matrices. CBp particles at 550 °C exhibited greater structural order, as determined by Raman spectroscopy, which can be attributed to the elevated temperature proximate to the cylinder wall surface. Furthermore, the potential of CBp for reinforcement in natural rubber (NR) was taken into consideration. The pronounced propensity of high-temperature CBps to agglomerate led to uneven dispersion within the polymer, consequently causing heightened heat accumulation and the emergence of the Payne effect. Based on a thorough analysis of the outcomes, the optimal pyrolysis temperature for CBp synthesis within the continuous reactor was ascertained.
To address the pronounced self-aggregation of highly loaded silica in the aqueous phase and the substantial filler loss occurring during the flocculation stage of latex compounding, this study introduces disaggregated and activated sepiolite possessing a spatial confinement effect as both a suspension stabilizer and a synergistic reinforcing component. On this basis, a multiscale natural rubber (NR)/silica/sepiolite composite system was constructed via a latex compounding route. Rheological characterization combined with static sedimentation observations revealed that the percolation threshold of the sepiolite is approximately 0.8 wt%. When the sepiolite content exceeds 1.0 wt%, its fibrous morphology enables the formation of a continuous three-dimensional network, which physically constrains silica particles and effectively suppresses their sedimentation and self-aggregation in the aqueous medium. Guided by this percolation behavior, a stable silica/sepiolite hybrid slurry was subsequently wet-mixed with natural rubber latex, and the influence of sepiolite loading on silica retention during flocculation, as well as on the resulting composite properties, was systematically examined. The results demonstrate that incorporation of sepiolite reduces filler loss during flocculation, with the loss rate decreasing from 4.7% to 1.1%. The Payne effect, SEM, dynamic and static mechanical analyses indicate that an appropriate sepiolite dosage promotes dispersion of silica within the rubber matrix while simultaneously strengthening filler–rubber interfacial interactions. Accordingly, tensile and tear strengths are increased from 32.1 to 35.5 MPa and from 92.3 to 133.4 N·mm−1, respectively, while wet skid resistance is preserved and both rolling resistance and wear resistance are further improved. The findings of this work establish a practical and efficient strategy for the wet preparation of high-performance NR/silica composites.
Based on temperature–stress coupling simulation, a thermal source model for nanosecond pulsed hollow cathode electron beam surface modification is proposed. Dynamic thermal-stress changes from beam–surface interaction and their influence on micro–nano characteristics were systematically investigated. By analyzing maximum temperature/stress dynamics, cross-sectional remelted layer variations, and heating/cooling rates, the temperature and stress distribution in the micron-scale surface layer was comprehensively revealed, validating the model’s rationality. Combined with low, medium, and high pulse count experiments, the effects of thermal and stress factors on surface morphology and grain refinement were studied, elucidating underlying mechanisms through numerical correspondence. Results show irradiation effects confined to a 1.5–2 mm localized region, with extreme temperature changes (~103 K) and stress variations (103–104 MPa) within tens of nanoseconds. Heating rates reached 1011 K/s, cooling rates 109–1010 K/s, exceeding microsecond pulsed beams by one to two orders. Simulated remelting zone diameter and thickness agreed well with experiments, confirming model validity. Grain refinement is primarily driven by rapid temperature distribution, generating instant solidification nucleation sites, with a secondary contribution from high-stress-induced plastic deformation forming sub-grains.
31 August 2026 in Journal of Applied Polymer Science