To improve vanadium leaching and yield rates during wet vanadium extraction processes, the crystallization behavior and growth mechanism of spinel crystals in vanadium-containing slags were investigated by the mathematical models and high temperature experiments. The results show that the suitable temperature range for spinel crystallization was 1473–1573 K. And the spinels’ crystallization abilities were ranked FeCr2O4 → FeV2O4 → Fe2TiO4. Although the concentration of chromium in the vanadium-containing slags was relatively low, the crystallization rate of all spinel crystals was greatly affected by the chromium spinels. The distribution of spinel diameters differed under the actual smelting condition, with the most common diameter range being 10–15 µm. In addition, the mean diameter and volume fraction of spinels increased with prolonging holding time and decreasing temperature in the actual smelting temperature range. Spinel crystals grew rapidly with time at 1623 K, the mean crystal diameter changed from 15.0 µm at 0 min to 24.9 µm at 60 min. And the mean diameter and volume fraction of spinels treated at 1523 K for 30 min were 28.1 µm and 46.3%, respectively. The mean diameter and volume fraction of spinel crystals increased with prolonging holding time and by decreasing the temperature in the actual smelting temperature range (1573–1673 K). Thus, the remaining slag process is beneficial to spinels growth in industrial vanadium-extraction process.
22 January 2020 in International Journal of Applied Ceramic Technology
To effectively separate the valuable minerals in ludwigite, this study investigated the grinding fineness behaviour and liberation characteristics. The results indicated that the particle yield of −75 μm with a microwave power of 4 kW for 40 s was increased by 18.22% in comparison to that of raw ore. The D(50) and D(90) raw-ore grinding products reached 53.52 and 215.16 μm, both of which were larger than microwave-treated samples. The particle-size distribution of the grinding products for treated ore was more uniform, and the amount of coarse and over-ground particles decreased significantly. The specific surface area, pore volume and pore diameter of the large particles were effectively increased after microwave heating, which improved the crushing and grinding characteristics of the grinding products by lowering the relevant mechanical properties. The monomer liberations of magnetite, ascharite and serpentine of microwave-treated ore samples were 55.33%, 35.48% and 74.98%, respectively, which represented an increase of 12.06%, 9.37% and 6.22% in comparison to untreated ore samples. The bonding characteristics among different minerals were altered through microwave treatment to weaken the bonding force and reduce the proportion of interlocked minerals, which allows these complex minerals to easily liberate after secondary grinding.
10 September 2020 in Metallurgical Research & Technology
The crystallization and separation behaviors of the V-spinel phase in the FeO-SiO2-V2O3-TiO2 system as the main components of vanadium slag were investigated to effectively concentrate and separate vanadium from the vanadium slag. Fine V-spinel precipitates were transformed into large lumps and strip crystals by decreasing the temperature from 1773 K to 1723 K. Ti-spinel phases began to crystallize from the molten slag by further decreasing the temperature to 1673 K. In order to adequately precipitate a single V-spinel phase with suitable grain size in the crystals from the molten slag, the temperature was chosen as 1723 K. With introduction of supergravity technology, the Ti-containing slag melt went through the filter to form the Ti-containing slag, while V-spinel crystals were intercepted by the filter to form the V-enriched slag. Consequently, with G = 700 at 1723 K for 10 minutes, the mass fraction of V2O3 was increased from 17.00 wt% before separation to 32.98 wt% in the enriched slag; the recovery ratio of V2O3 reached about 86.50%. In addition, the mass fraction of TiO2 reached about 19.41 wt% in the Ti-containing slag, which could be recycled as a titanium-bearing material in the metallurgical industry.
To effectively separate the valuable minerals in ludwigite, this study investigated the mineralogy of ore, particle-size distribution and mineral liberation characteristics. Most of the magnetite was intergrown with ascharite and serpentine. Nearly half of the serpentine existed in a dense, massive body. Most of the ascharite was encased in magnetite, and a small amount was embedded in the serpentine phase. After the microwave radiation, some intergranular and through cracks were formed to improve mineral liberation during the grinding process. The mass fractions for the +75 μm range decreased from 43.16 wt% for untreated samples to 24.31 wt% for treated samples with a microwave power of 3 kW for 40 s. By contrast, the mass fractions of particles in the −75 μm range increased from 56.84 wt% for untreated samples to 75.69 wt% for treated samples. D50 decreased from 53.54 µm for the untreated sample to 21.58 µm for the treated sample. The liberation degrees after the treated samples clearly improved and increased by 26.64% for magnetite, 18.92% for ascharite and 14.10% for serpentine.