Chengde chromium-bearing vanadium–titanium magnetite (CCVTM) has been used as an important mineral resource in sinter making. The MgO content of this sinter can be enhanced by adding dolomite, which improved operation of the blast furnace. The effects of MgO in the form of dolomite on metallurgical properties, microstructure and mineral compositions of CCVTM sinter were studied by a sinter pot test, X-Ray Diffraction (XRD), Scanning Electron Microscope (SEM), and mineral phase microanalysis. The results were as follows: The flame front speed and sinter coefficient decreased with an increase in MgO content from 2.66 to 3.86% by adding dolomite. With an increase in MgO content from 2.66 to 3.86%, the flame front speed, sintering utilization factor, and the value of RI decreased, while RDI and the softening–melting properties improved. In addition, the value of sinter strength (TI) reached a maximum value at MgO = 3.56%. In addition, an increase in the abundance of magnetite, magnesium ferrite, and silicate phase, as well as a decrease in hematite, was found with an increase in MgO content. We concluded that the most appropriate MgO content in the sinter is 3.56%.
High-chromium vanadium and titanium magnetite (HCVTM) sinter has poor properties. The coke ratio has an important effect on the behavior of HCVTM sintering as it affects the mineral phases in the high-chromium vanadium and titanium sinter (HCVTS) via changing the sintering temperature and atmosphere. In this work, the sintering behavior of HCVTM mixed with varying coke ratios was investigated through sintering pot tests, X-ray diffraction (XRD), gas chromatographic analysis, and mineral phase analysis. The results show that, with the increase of the coke ratio from 4.0% to 6.0%, leading to the increase of the combustion ratio of the flue gas, the vertical sintering rate and sinter productivity decrease. Meanwhile, with the change of the coke ratio, the content of magnetite, silicate, and perovskite increase, while the hematite and calcium ferrite decrease. In addition, the tumble strength and reduction ability of HCVTS decrease, and its degradation strength increase. It was found that the appropriate coke ratio for the sintering process was 5.0 wt %.