Using both broadband ferromagnetic resonance (FMR) spectroscopy and ab initio calculations, we study the magnetodynamic properties of permalloy and films with M as platinum (Pt), gold (Au), or silver (Ag). From the uniform FMR mode, we extract the saturation magnetization , damping , and inhomogeneous broadening ; from the first perpendicular standing spin-wave (PSSW) mode, we extract the exchange stiffness . and are found to decrease with increasing alloying, most strongly for Au and less so for Pt. On the other hand, increases rapidly with both Pt and Au content, while being virtually independent of Ag content. The physical origins of the observed trends in , , and are analyzed and explained using density functional theory calculations in the coherent potential approximation. The calculated trends quantitatively agree with the experimental observations. The drastically different impacts of Pt, Au, and Ag on the various fundamental magnetodynamic properties will allow for significant design freedom, where different properties can be varied independently of others through careful combinations of the Pt, Au, and Ag contents of films. By empirical approximations of each property's concentration dependence, we can dial in any desired combination of magnetodynamic properties within this parameter space. As a proof-of-principle demonstration we design a set of films, where the saturation magnetization stays constant throughout the set and the damping can be tuned by a factor of 4.
For spintronics application, which requires fast field switching, it is important to have a kind of soft magnetic material with large damping coefficient. Here, we present the studies of the Nd dopant-level-dependent damping coefficient of Nd-Py thin films (30 nm) in a dilute region utilizing ferromagnetic resonance (FMR). With the Nd content increasing, the film structure was found to be changing from polycrystalline to amorphous when the Nd content is around 3.4%. Meanwhile, the magnetization decreases linearly. Interestingly, we find that along the easy axis, both low coercivity and high hysteresis squareness are simultaneously maintained in the system; i.e., the magnetic softness has been well kept. By theoretical fitting of the angular dependence of the FMR field, the first- and second-order magnetic anisotropy constants, and , and the Lande factor are obtained and discussed quantitatively. The measurements of angular and frequency dependence of the ferromagnetic resonance linewidth, as well as the theoretical fitting by considering the contributions of Gilbert damping, two-magnon scattering, and inhomogeneous broadening, show that the damping coefficient increases rapidly (about 25-fold) as the Nd content increases to 11.6%, which is mainly due to the enhanced spin-orbit coupling by the Nd additives, supported by x-ray magnetic circular dichroism measurements.
10 April 2009 in The Journal of Physical Chemistry C
The clear understanding of exchange interactions between magnetic ions in substituted BiFeO3 is the prerequisite for the comprehensive studies on magnetic properties. BiFe0.5Mn0.5O3 films and BiFeO3/BiMnO3 superlattices have been fabricated by pulsed laser deposition on (001) SrTiO3 substrates. Using piezoresponse force microscopy (PFM), the ferroelectricity at room temperature has been inferred from the observation of PFM hysteresis loops and electrical writing of ferroelectric domains for both samples. Spin glass behavior has been observed in both samples by temperature dependent magnetization curves and decay of thermo-remnant magnetization with time. The magnetic ordering has been studied by X-ray magnetic circular dichroism measurements and Fe-O-Mn interaction has been confirmed to be antiferromagnetic (AF). The observed spin glass in BiFe0.5Mn0.5O3 films has been attributed to cluster spin glass due to Mn-rich ferromagnetic (FM) clusters in AF matrix, while spin glass in BiFeO3/BiMnO3 superlattices is due to competition between AF Fe-O-Fe, AF Fe-O-Mn and FM Mn-O-Mn interactions in the well ordered square lattice with two Fe ions in BiFeO3 layer and two Mn ions in BiMnO3 layer at interfaces.