In order to promote the sustainable use of resources and reduce the waste of waste glass and tailings resources. The present study focuses on a fluorite mine as the research subject, utilizing coarse tailings, fine tailings, cement substitute-curing agent, and recycled waste glass as the primary raw materials. It investigates the changes in compressive strength of coarse tailing with varying sand- binder ratios and glass content at 3-day, 7-day, and 28-day intervals when the filling slurry concentration is set at 77% and the ratio of coarse tailings to fine tailings is maintained at 2:1. The findings indicate that there is minimal impact on the compressive strength of test blocks when using a sand binder ratio of 4:1 and a glass sand content below 10%. However, once the glass sand content exceeds 10%, a significant decline in compressive strength occurs. Scanning electron microscope (SEM) images reveal ettringite crystal formation in test blocks with both 0% and 25% glass sand content due to high levels of Na2O in the glass sand. This leads to internal expansion within test blocks resulting in reduced strength. Notably, when using a sand-binder ratio of 8:1 along with a glass sand content of 25%, early strength characteristics are observed for test blocks. Furthermore, incorporating glass sand has little influence on late-stage strength for backfill when employing either an 8:1 or 12:1 sand-binder ratio. Based on this experiment conducted under conditions including mass concentration of 77%, the optimal waste-glass-to-mine-tailings-filling-sand-binder-ratio is determined as 8:1with a corresponding glass content of 25%.
In the process of continuous and high-intensity mining in soft rock coal mines, high-quality filling treatment is required for the goaf. A nondestructive acoustic velocimetry method is an excellent way to measure the quality of filling body to effectively maintain the rock stability of the mining area and decrease industrial solid waste. In this study, the gangue and fine sand are used as the filling aggregates, and the uniaxial compression test and acoustic wave test are conducted in the cementitious gangue-sand filling body with different gangue-sand ratio. The results show that the longitudinal wave velocity of the filling body is basically between 1.556 km/s and 2.413 km/s. When the gangue-sand ratio is small, and the slurry concentration is high, the early strength of the cementitious gangue-sand filling body is low, but the later strength has a good growth trend. For specimens with higher strength-filled bodies, the propagation speed of sound waves inside them is also faster, indicating a certain positive correlation between the strength of the filled body and the speed of sound waves. A mathematical equation using longitudinal wave velocity to predict the strength of filling body is established. This equation can be used to predict and judge the quality of the filling body in the mining area.
16 September 2023 in Advances in Civil Engineering
Three groups of filling materials with different mix proportions were prepared. PO42.5 grade cement was selected as the binding material, mechanized granular coal gangue and fine sand were used as the filling aggregate, and then the specimens were curing at room temperature and 95% moisture. Through the uniaxial compression test, the influence of gangue–sand ratio, the mass fraction, and curing age on the mechanical properties of filling materials was analyzed. The microstructure analysis of SEM was conducted to explore the internal mechanism of the strength difference of filling materials. The results show that the gangue–sand ratio dramatically influences the uniaxial compressive strength. The strength increases first and then decreases with the gangue–sand ratio increase. The mass fraction of filling paste is positively correlated with specimen strength. When the sand–cement ratio, gangue–sand ratio, and the mass fraction remain unchanged, the longer the curing age, the greater the uniaxial compressive strength of specimens. The specimens with a sand–cement ratio of 3.5 : 1, a gangue–sand ratio of 5 : 5, and a mass fraction of 86% reach the maximum value of 11.03 MPa at a curing age of 10 days. It can be seen that when the gangue–sand ratio is 5 : 5, the filling material has the best mechanical properties, so it can be recommended as the optimal mix proportion for goaf filling. Thus, it provides a solid technical guarantee for the treatment of mine surface collapse disasters and the utilization of bulk coal gangue resources.