This paper presents the results of the study on the development of a methodology for the production of pure amorphous silicon dioxide containing up to 99.8 wt.% of SiO2. As a starting material, a silica gel with a moisture content of up to 55 wt.% and an SiO2/AlF3 ratio of 4 was used. The silica gel was purified using alkaline and acidic solutions in concentrations ranging from 0.1 to 25 wt.%. The analysis of the experimental data allowed to identify the most suitable purification parameters of the starting material. The initial silica gel and the reaction products were studied using the methods of X-ray fluorescence, X-ray phase analysis, electron scanning microscopy, EDS microanalysis, and particle-size analysis. Amorphous silicon dioxide obtained according to the methodology developed by the authors forms agglomerates of spherical silicon dioxide particles up to 1 μm in size. Amorphous silicon dioxide was involved in the preparation of catalyst supports in order to consider the possibility of replacing part of the expensive raw material in the form of aluminum hydroxide. In the work, the characteristics of the addition of this amorphous silicon dioxide and the supports obtained from the traditionally used raw materials were evaluated.
The article is devoted to the neutralization of the harmful effects of aluminochrome catalyst sludge. Catalyst sludge is a waste product from petrochemical production and poses a serious threat to the environment and humans because of the toxic hexavalent chromium it contains. The emissions of Russian petrochemical enterprises’ alumochrome sludge is 10,000–12,000 tons per year. In this paper, research related to the possibility of reducing the harmful effects of sludge by converting hexavalent chromium to a less dangerous trivalent state is presented. The reduction of hexavalent chromium was carried out with different reagents: Na2SO3, FeSO4, Na2S2O3, and Na2S2O5. Then, a comparative analysis was carried out, and sodium metabisulfite was chosen as the most preferred reagent. The peculiarity of the reducing method was carrying out the reaction in a neutral medium, pH = 7.0. The reduction was carried out in the temperature range of 60–85 °C and under standard conditions. The maximum recovery efficiency of chromium from the catalyst sludge (100%) was achieved at 85 °C and 10 min. This method did not involve the use of concentrated sulfuric acid, as in a number of common techniques, or additional reagents for the precipitation of chromium in the form of hydroxide.