A redox cycle between Ce4+ and Ce3+ is an elementary step in water gas shift (WGS) mechanism. By facilitating the redox cycle between +4 and +3 of cerium, a formation of oxygen vacancy can be enhanced. It is considered to be a dominating factor in developing the WGS performance and the stability of ceria in this work. We have facilitated the redox cycle in CeO2 to enrich the WGS activity. The WGS reaction was carried out on Ni catalyst supported by Gd-doped ceria (GDC) from Daiichi. Ni and Re were added onto GDC by impregnation method to examine the role of Re addition on surface, structural and reducibility, which affected upon their catalytic activities. Rhenium has an influence on increasing the water gas shift performance of Ni/GDC catalysts because it facilitates the redox process at the surface of ceria, disperses Ni particles and enhances oxygen vacancy formation. The results indicate that the water gas shift activity of 1%Re4%Ni/GDC is higher than that of 5%Ni/GDC. The dispersion of active site on the surface of catalyst results in an increase of CO molecule adsorption and acceleration of the redox cycle between Ce4+ and Ce3+ of ceria support via oxygen vacancy generation. Therefore, using a combination of these two effects can enhance the WGS performance.
The water–gas shift (WGS) performance of 10%Ni/Al2O3, 20%Ni/Al2O3 and 10%Ni/CaO-Al2O3 catalysts was studied to reduce CO concentration and produce extra hydrogen. Ni was added onto the Al2O3 support by an impregnation method. The physicochemical properties of nickel catalysts that influence their catalytic activity were examined. The most influential factors in increasing the CO conversion for the water–gas shift reaction are Ni dispersion and surface acidity. Ni metal sites were identified as the active sites for CO adsorption. The main effect of nickel metal was reducing the adsorbed CO amount by reducing the active site concentration. The 10%Ni/Al2O3 catalyst was more active for the WGS reaction than other catalysts. This catalyst presents a high CO conversion rate (75% CO conversion at 800 °C), which is due to its high Ni dispersion at the surface (6.74%) and surface acidity, thereby favoring CO adsorption. A high Ni dispersion for more surface-active sites is exposed to a CO reactant. In addition, favored CO adsorption is related to the acidity on the catalyst surface because CO reactant in the WGS reaction is a weak base. The total acidity can be evaluated by integrating the NH3-Temperature-Programmed Desorption curves. Therefore, an enhancement of surface acidity is identified as the favored CO adsorption.
Water gas shift reactions (WGS) were evaluated over Ni/CeO2 and Ni/CeSmO catalysts for hydrogen production. The effects of catalyst preparation method and Sm loading were investigated. The Ni/ceria and Ni/CeSmO catalysts were synthesized by combustion, sol gel and sol gel-combustion method. After WGS tests, the catalysts were determined the carbon deposition by thermogravimetric analysis. The thermogravimetric analysis and temperature programmed NH3 desorption showed that addition of Sm promoter made higher the weak acid sites and lower the amount of carbon deposition than the unpromoted catalyst due to it being easily removed. CO chemisorption result indicated that Ni/Ce5%SmO catalyst prepared by combustion method has the highest Ni metal dispersion and metallic surface area compared to the other catalysts. The enhancement of WGS activity of this catalyst is due to more surface active sites being exposed to reactants. Furthermore, H2-temperature programmed reduction analysis confirmed an easiest reduction of this catalyst. This behavior accelerates the redox process at the ceria surface and enhances the oxygen vacancy concentration. The catalytic activity measurements exhibited that the optimum Sm loading was 5% wt. and the best catalyst preparation was the combustion method. The high surface area and small crystallite size of the 5%Ni/Ce5%SmO (combustion) catalyst resulted in sufficient dispersion, which closely related to the WGS activity of the catalyst.
The role of dopants (Sm, Tb and Pr) on the water–gas shift performance of CeO2-based materials was studied. Modification of CeO2 with Sm significantly improved the water–gas shift performance. The catalytic activities of doped CeO2 were increased when compared with the catalytic activities of pure ceria (65% conversion at 600 °C for Ce5%SmO and 50% conversion at 600 °C for CeO2). The key factors driving the water–gas shift performance were reduction behavior and oxygen vacancy concentration. In the redox mechanism of the WGS reaction, CeO2 plays a crucial role in transferring oxygen to CO through changes in the oxidation state. Therefore, Sm is effective in catalyzing the water–gas shift activity because the addition of Sm into CeO2 decreases the surface reduction temperature and alters the oxygen transportation ability through the redox mechanism. XRD results suggested that Mn+ (M = Sm, Tb and Pr) incorporate into ceria lattice to form a solid solution resulting in unit cell enlargement. The defect structure inside the CeO2 lattice generates a strain on the oxide lattice and facilitates the generation of oxygen vacancies. XANES analysis revealed that Sm reduced CeO2 easily by transporting its electron into the d-orbitals of Ce, thus giving rise to more Ce3+ at the CeO2 surface. The presence of Ce3+ is a result of oxygen vacancy. Therefore, the high content of Ce3+ provides more oxygen vacancies. The oxygen vacancy formation results in easy oxygen exchange. Thus, reactive oxygen species can be generated and easily reduced by CO reactant, which enhances the WGS activity.
Water–gas shift (WGS) reaction was performed over 5% Ni/CeO2, 5% Ni/Ce-5% Sm-O, 5% Ni/Ce-5% Gd-O, 1% Re 4% Ni/Ce-5% Sm-O and 1% Re 4% Ni/Ce-5% Gd-O catalysts to reduce CO concentration and produce extra hydrogen. CeO2 and M-doped ceria (M = Sm and Gd) were prepared using a combustion method, and then nickel and rhenium were added onto the mixed oxide supports using an impregnation method. The influence of rhenium, samarium and gadolinium on the structural and redox properties of materials that have an effect on their water–gas shift activities was investigated. It was found that the addition of samarium and gadolinium into Ni/CeO2 enhances the surface area, reduces the crystallite size of CeO2, increases oxygen vacancy concentration and improves Ni dispersion on the CeO2 surface. Moreover, the addition of rhenium leads to an increase in the WGS activity of Ni/CeMO (M = Sm and Gd) catalysts. The results indicate that 1% Re 4% Ni/Ce-5% Sm-O presents the greatest WGS activity, with the maximum of 97% carbon monoxide conversion at 350 °C. An increase in the dispersion and surface area of metallic nickel in this catalyst results in the facilitation of the reactant CO adsorption. The result of X-ray absorption near-edge structure (XANES) analysis suggests that Sm and Re in 1% Re 4% Ni/Ce-5% Sm-O catalyst donate some electrons to CeO2, resulting in a decrease in the oxidation state of cerium. The occurrence of more Ce3+ at the CeO2 surface leads to higher oxygen vacancy, which alerts the redox process at the surface, thereby increasing the efficiency of the WGS reaction.
A single-bed and dual-bed catalyst system was studied to maximize H2 production from the combination of partial oxidation of CH4 and water gas shift reaction. In addition, the different types of catalysts, including Ni, Cu, Ni-Re, and Cu-Re supported on gadolinium-doped ceria (GDC) were investigated under different operating conditions of temperature (400–650 °C). Over Ni-based catalysts, methane can easily dissociate on a Ni surface to give hydrogen and carbon species. Then, carbon species react with lattice oxygen of ceria-based material to form CO. The addition of Re to Ni/GDC enhances CH4 dissociation on the Ni surface and increases oxygen storage capacity in the catalyst, thus promoting carbon elimination. In addition, the results showed that a dual-bed catalyst system exhibited catalytic activity better than a single-bed catalyst system. The dual-bed catalyst system, by the combination of 1%Re4%Ni/GDC as a partial oxidation catalyst and 1%Re4%Cu/GDC as a water gas shift catalyst, provided the highest CH4 conversion and H2 yield. An addition of Re onto Ni/GDC and Cu/GDC caused an increase in catalytic performance because Re addition could improve the catalyst reducibility and increase metal surface area, as more of their surface active sites are exposed to reactants.
About Me
Department of Chemistry, Faculty of Science and Technology, Thammasat University.
Department of Chemistry, Faculty of Science and Technology, Thammasat University.