Tyre–pavement contact stress distribution has a significant effect on mechanical responses in thin asphalt pavements and responses at near-surface of thick asphalt pavements. To achieve a more accurate tyre–pavement contact stress distribution considering tyre types, tyre loads and tyre inflation pressures for pavement design and analysis, three-dimensional (3D) finite element (FE) tyre–pavement models were developed. Two common tyre types (bias ply tyre and radial tyre) were considered in the models. Then, models were verified through the comparison between the predicted and measured tyre contact stresses. Excellent agreement between predicted and measured contact stresses was achieved. Then, the contact stress distributions between different tyres and pavement were analysed under different tyre loads and tyre inflation pressures combinations (nine working conditions). Results indicated that with the increase of vertical load, the location of maximum contact stress between bias ply tyre and pavement changed from inside to outside of tread while the maximum contact stress between radial tyre and pavement always appeared in the centre of tread. And under a same working condition, the maximum contact stress between radial tyre and pavement was larger than that between bias ply tyre and pavement. Besides, in the lateral direction, the variation range of the contact stresses under different ribs of a bias ply tyre was less than that of a radial tyre.
17 January 2018 in Road Materials and Pavement Design
To evaluate the transverse crack on a semi-rigid pavement rapidly by a falling weight deflectometer (FWD), three-dimensional dynamic finite-element (FE) models were developed to calculate the deflection response of a transverse-cracked semi-rigid pavement under an FWD load. Models were validated by deflection basin data acquired from in situ FWD tests. Then, the effects of thermal cracking and reflective cracking on deflection basin data were analysed. Four loading locations and seven crack widths were considered in the analysis. Results showed that deflection basins calculated by dynamic FE models coincided well with that measured by in situ FWD test. The largest per cent difference between calculated deflections and measured values was less than 9%. When the distance between loading centre and crack was within 1050 mm, load transfer efficiency (LTE) indexes showed a good performance for distinguishing a reflective crack from a thermal crack. A practical field test method placing the transverse crack between sensor S300 and sensor S600 was recommended and LTE300–600 was proposed as the evaluation index for the rapid determination of crack type.
27 April 2012 in Journal of Central South University
A pavement structural survey plays a vital role in road maintenance and management. This study was intended to explore the feasibility of a non-stop pavement structure assessment method by analyzing the vibration data from a vehicle sensor. In this study, three falling weight deflectometer (FWD) tests and four vehicle vibration tests were conducted on five pavement structures. The FWD test results show that the continuously reinforced composite pavement has a higher structural stiffness than the semi-rigid base asphalt pavement. According to the statistical distribution of vehicle acceleration, a distribution parameter, the peak probability density (PPD), was proposed. The correlation coefficient (−0.722) of the center deflection (D1) and PPD indicates a strong correlation between the two variables. Therefore, PPD is strongly correlated with pavement structural stiffness. This study proposed a novel characterization method for pavement structural conditions based on the distribution parameter of the vehicle vibration signal.
9 April 2013 in Journal of Central South University