With the fast-growing global water crisis, the development of novel technologies for water remediation and reuse is crucial. Industrial wastewater especially contains various toxic pollutants that pose an additional threat to the environment; thus, efficient removal of such contaminants can ensure safe reprocessing of industrial wastewater, thereby alleviating the demand for fresh water. Herein, we describe a novel and efficient approach for preparing porous polycaprolactone (PCL) membranes with a hierarchical architecture via a simple solvent/non-solvent methodology. A mixed-matrix membrane (MMM) was further constructed utilizing an amine-functionalized metal–organic framework as the sorbent filler nanoparticles and PCL as the polymer support matrix (MOF@PCL) for wastewater treatment applications. The MOF@PCL MMM demonstrated homogeneous morphology as well as exceptional performance towards the removal of both cationic (methylene blue, MB) and anionic (methyl orange, MO) organic dyes, where the maximum adsorption capacities reached 309 mg g−1 and 208 mg g−1, respectively. Kinetic and thermodynamic investigations revealed that the adsorption process was endothermic with a fast intraparticle diffusion rate constant. The MOF@PCL MMM also displayed excellent mechanical stability and recyclability, where the removal efficiency was maintained after 10 cycles.
A green, water-based synthesis of thiol-decorated, Zr-carboxylate metal–organic framework is reported. A mixture of capping and bridging, thiol containing, organic linker approach utilizing mercaptoacetic acid (MA) and mercaptosuccinic acid (MSA) resulted in an open Zr-based MOF with thiol-decorated cages (Zr-MSA-MA MOF). Tailoring the nanospace within the micropores of water-synthesized and water-stable MSA-MOF led to several desirable attributes including: (i) chemical stability in aqueous media due to strong –CO2–Zr(IV) linkage, (ii) tight pore system leading to optimized electronic interactions with guest ions, and (iii) thiol-functionalized cages that affect selective capture of soft metal ions. The Zr-MSA-MA MOF demonstrated exceptionally high capacity for Cd (370.4 (±35.5) mg g−1, 3.29 mmol g−1) and Pb (500 (±16.8) mg g−1, 2.41 mmol g−1). It also exhibited remarkable stability indicated by its ability to regenerate and reuse the MSA-MOF for 10 consecutive cycles with nearly 95% retention of initial activity towards heavy metal removal. Moreover, the thiol-decorated MOF demonstrated high selectivity for Pb and Cd in the presence of competing Cu, Zn, Ni, Mn, Fe, and Co ions. These findings highlight the potential of Zr-MSA-MA MOF as a highly efficient, selective, and regenerable sorbent for heavy metal remediation.
The development of cationic-decorated polymeric electrospun fibers is a promising approach for removing soluble anionic contaminants in wastewater treatment applications. Ionomers exhibit excellent performance in binding and capturing ionic contaminants, but preventing their dissolution in aqueous environments necessitates cross-linking the ionomeric chains. However, cross-linked ionomeric networks do not lend themselves well to various polymer-processing techniques, which restricts their utilization as membranes and fibers for water treatment. Herein, we report the successful formulation of dispersed cross-linked ionomer into linear polymer solution to construct a spinning matrix for fiber electrospinning. The generation of water-permeable electrospun fibers decorated with a cationic network demonstrated high adsorption capacities and a selective affinity towards anionic pollutants, including methyl orange, phenol red, eosin yellow, and Congo red. The electrostatic interactions between the cationic fibers and the anionic contaminants resulted in removal efficiencies up to 99%, with adsorption capacities reaching 500 mg g−1, in contrast to cationic pollutants (≤5%). Moreover, comparative studies revealed that the fibers incorporating the cationic cross-linked polymer outperformed a control fiber membrane utilizing the linear polymer polycaprolactone, confirming the critical role of the cationic surface charges in achieving the recorded uptake. Interestingly, the adsorption isotherms highlighted the influence of the contaminant size and structure on the adsorption mechanism, where small molecules demonstrated adsorption isotherms best fitted by the Langmuir model, while bulky, long-chain contaminants, such as Congo red, followed the Freundlich model. Additionally, the nanofibers demonstrated outstanding regeneration and reusability, maintaining removal efficiencies of 99% for MO and 78% for PR after ten adsorption–desorption cycles. The data collectively highlight the potential of this approach for practical applications in sustainable water treatment.
1 December 2025 in ECS Journal of Solid State Science and Technology
We address the regulated synthesis of silica/magnetite core–shell nanoparticles and demonstrate their application in in situ monitoring of methylene blue (MB) in water. MB was selected in this due to its widespread industrial application and consequent environmental significance. The synthesized core/shell nanostructures exhibited significant sensitivity and quick response in detecting MB when integrated with quartz crystal microbalance technology. Atomic force microscopy measurements revealed a surface roughness of 11.07 ± 0.4 nm, providing abundant active sites for adsorption. The nanocrystallites of the magnetite shell offered a large surface area with distinct active sites that promoted effective adsorption of MB molecules. The solution pH was found to be a critical parameter that governed the sensing performance. Optimal sensitivity was achieved at alkaline pH because of the intense electrostatic interaction between the negatively charged surface and MB cations. Under neutral pH, strong and efficient response was obtained, whereas acidic pH suppressed the adsorption because of molecular aggregation and protonation at the surface. The detection limits were 62.2 μg l −1 and 35.83 μg l −1 for neutral and alkaline pH conditions, respectively. At alkaline pH, the nanoparticles maintained 95% efficiency after 30 days and achieved 97% recovery over five regeneration cycles.