In industry, natural cracks usually exist in complex forms such as adjacent, colony, irregular, and crossing. Mere magnetic field is inadequate to accurately evaluate the complex cracks using eddy current testing. In this study, an improved eddy current imaging method using the signal of rotating eddy current testing (RECT) was proposed to reconstruct the surface profile of complex cracks. A transformation method was adopted to transform the signals of RECT into those under uniform eddy current testing at the desired orientation. The deconvolution of the transformed signals and square current dipole was carried out to obtain eddy current images at eight orientations around complex cracks. By accumulating the eddy current images, the surface profile of the complex cracks was reconstructed. Simulations and experiments were carried out to illustrate, validate, and test the proposed method. The results indicated that the obtained surface profiles were clearer than those obtained by the previous method using uniform eddy current testing. The improved method was effective for artificial complex slits and irregular stress corrosion crack colonies. Moreover, its performance was stable for the cracks with different angles and depths.
3 January 2012 in Nondestructive Testing and Evaluation
This study demonstrates that the reflection of microwave propagating inside a pipe enables one to nondestructively detect and locate wall thinnings appearing inside the pipe. A signal processing method is proposed to compensate for the dispersion of microwave and to make the reflection due to a wall thinning clearer. After fundamental characteristics of the microwave signals were evaluated using 3D finite element simulations, verifications were made by both experiments and numerical simulations using straight brass pipes whose outer diameter and wall thickness were 25 and 3 mm, respectively. The verifications revealed that imposing the signal processing method provided a clear indication of the location of wall thinning, and no significant deterioration was observed even when the pipe was as long as 2000 mm. The verifications also showed that the amplitude of reflection signal was almost proportional to the volume of wall thinning, which agreed with another report, and the reflections were sufficiently clear even when the edge of a flaw was not stepwise but curved like actual wall thinnings.
22 October 2019 in Nondestructive Testing and Evaluation
This study proposes a probability of detection (POD) model for the probabilistic analysis of the detectability of electromagnetic acoustic resonance (EMAR) method for the detection and evaluation of pipe wall thinning. Forty-one carbon steel plate samples with an artificially corroded groove were prepared to simulate pipe wall thinning caused by flow-assisted corrosion. Experiments were performed to gather EMAR signals from the samples, and subsequently the depths of the grooves were evaluated based on the fundamental frequency of the measured signals. The results of the experiments showed that the error in evaluating the depth of a groove tended to increase with the depth. The results also confirmed that the surface roughness of the groove would contribute to the error, and the thickness of a plate without corrosion can be quite accurately evaluated. Analysing the measured EMAR signals using the proposed POD model, which takes these characteristics into consideration, and a conventional one confirmed that the proposed model can more reasonably evaluate the probability of detection against small wall thinning, as well as the false-positive rate.
This study investigated the applicability of detecting pitting corrosions on stainless steel weld overlay cladding using uniform eddy current testing, which is insensitive to surface undulation, and rotating eddy current testing (RECT), which can be considered a superposition of uniform eddy current testing in orthogonal directions. The performance of the two techniques in detecting artificial pitting corrosions on and next to weld beads was compared. The signal distributions revealed that only RECT was capable of describing the surface profiles of pitting corrosions. The results of uniform eddy current testing could not distinguish between pitting corrosions and cracks. The probability of detection curves drawn to quantitatively indicate the detection capabilities of the two techniques revealed that uniform eddy current testing with induced eddy currents parallel and perpendicular to weld beads was better than RECT in detecting pitting corrosions on and next to weld beads, respectively. Scanning twice by uniform eddy current testing at orthogonal orientations may be a better process for detecting pitting corrosion on weld overlay cladding compared with using RECT. The measured signals of the two techniques in normal direction were located around the edges of the pitting corrosions, which only indicated the depth around edges. The results suggested that uniform eddy current testing and RECT with normal direction magnetic field signals may be inadequate for evaluating the maximum depth of pitting corrosions or large corrosions.
2 January 2016 in Nondestructive Testing and Evaluation
This study attempts to estimate the limitations of eddy current testing for evaluating the depth of a crack with the aid of numerical simulations. Three-dimensional finite element simulations were conducted to obtain eddy current signals resulting from a crack in a plate made of Ni-based alloy. The simulations modelled the crack as a sufficiently long rectangular region with a constant width and depth. A uniform conductivity was given inside the modelled crack because actual cracks do not always behave as electrically insulating walls. The conductivity of the modelled crack was chosen on the basis of a recent study reporting how real cracks can be modelled from the viewpoint of electromagnetic non-destructive evaluation. This study considered three conventional eddy current probes: a pancake probe, a vertical pancake probe and a plus point probe. The results of the simulations reveal that lower frequency does not always enhance the evaluation of a deeper crack if the crack is conductive; moreover, the maximum depth of a stress corrosion crack that conventional eddy current testing can evaluate quantitatively should be limited to a few mm at most. In contrast, the simulations also demonstrate that the ability of eddy current testing to size a fatigue crack would not differ significantly from that to size an artificial slit.