28 August 2022 in Materials and Manufacturing Processes
Verified
Journal Article
Closed access
GCGuddakesh kumar chandan
Guddakesh kumar chandan
CSChinmaya Kumar Sahoo
Chinmaya Kumar Sahoo
A low-power fiber laser system was utilized for machining a scalable surface area on the Ti-6Al-4V alloy surface through the track overlapping process. The effect of laser power and track overlapping on laser machined surfaces was investigated. The experimental results revealed that the laser machined surface characteristics, i.e. machining depth, resolidified layer thickness, heat affected zone (HAZ) size, and surface roughness, depend on the average laser power and track overlapping. The increased laser power from 30 W to 50 W at 50% track overlapping increases the machining depth from 88 µm to 981 µm due to a higher energy supply. Further, laser processing at higher power, i.e. 50 W, shows a significant increase in resolidified layer (up to 727 µm). The laser machined surface generated at higher power and track overlapping increases the surface roughness. The laser machined surface developed at 30 W and 50% track overlapping indicates surface roughness (Ra) of 2.9 µm and increases to 6.5 µm for surface processing at 80% track overlapping. Further, the surface roughness of the laser machined increases up to 14 µm for laser processing at higher power (50 W) and high track overlapping (80%).

27 July 2023 in Proceedings of the Institution of Mechanical Engineers, Part E: Journal of Process Mechanical Engineering
Verified
Journal Article
Closed access
GCGuddakesh kumar chandan
Guddakesh kumar chandan
CSChinmaya Kumar Sahoo
Chinmaya Kumar Sahoo
Traditional machining faces technical barriers in producing microfeatures when the workpiece poses high-strength and temperature-resistance characteristics. Laser is a possible machining approach that works effectively in the aforementioned conditions. The present study utilized a low-power fiber laser system machining of the Ti-6Al-4V alloy surface. The influence of laser processing parameters, for example average power, scanning speed, and pulse frequency, were analyzed on the laser-machined microgroove profiles using the full factorial design of the experiment. The results revealed that the fabricated microgroove profile characteristics, that is, depth, width, heat-affected zone (HAZ), surface roughness, etc. of laser-processed zone strongly depend on the laser processing parameters. Furthermore, the laser microgroove size, that is, depth and width, increases with the increment in laser power combined with low scan speed and low frequency. High laser power (50 W), low scan speed (0.1 mm/s), and low frequency (50 kHz) produce a microgroove with high depth (754.28 µm) and width (285.71 µm). It has been also observed that average power has the most significant impact on the machined surface profile, HAZ, and surface roughness. Moreover, it has also been observed that crack forms at the center of the machined surface is by decreasing scanning speed. Further, lower surface roughness is found at the highest pulse frequency. Hence, the present study recommends laser processing at lower power, high scanning speed, and high pulse frequency to generate a smooth and uniform machined surface.

31 August 2023 in Proceedings of the Institution of Mechanical Engineers, Part C: Journal of Mechanical Engineering Science
Verified
Journal Article
Closed access
GCGuddakesh kumar chandan
Guddakesh kumar chandan
CSChinmaya Kumar Sahoo
Chinmaya Kumar Sahoo
The present study aims to investigate the deep machining of Ti-6Al-4V alloy using a nanosecond (ns) laser through multi-pass and gas pressure. Experiments were conducted based on Full factorial design (FFD) by varying gas pressure and laser process parameters (LPP). Results showed that deeper grooves could be achieved through multi-pass laser scanning support with appropriate gas flow rate and laser parameters. A higher gas flow rate leads to more efficient removal of material and a faster machining rate. Further, the present findings revealed the substantial influence of laser power on the depth and width of the machined features, accounting for 41.28% and 7.11% of the variations, respectively. Moreover, power exhibited a significant impact on the taper angle (20.69%) and the heat-affected zone (HAZ) (12.04%) during the machining process. Additionally, the utilization of a multi-pass laser scan demonstrated a remarkable effect on the depth (1.89%), width (3.3%), HAZ (9.96%), and taper angle (8.78%). Furthermore, the assisted gas flow rate displayed a significant influence on the machined groove profile, that is, depth (41.97%), width (67.6%), HAZ (65.48%), and taper angle (30.15%). To achieve optimized results for high-depth machining with minimal defect, the present study recommends employing an average power of 40 W, an assisted gas flow rate of 25 L/min, and conducting four passes. These parameters develop laser machined surface with a high depth (~1499 µm) while simultaneously minimizing Taper (1.87°) and narrow HAZ (83 µm). Further, these conditions are suitable for laser cutting, trepanning, and surface texturing using a low-power laser system of Ti-6Al-4V alloy.

22 December 2023 in Proceedings of the Institution of Mechanical Engineers, Part E: Journal of Process Mechanical Engineering
Verified
Journal Article
Closed access
GCGuddakesh kumar chandan
Guddakesh kumar chandan
MAMohd Aslam
Mohd Aslam
BKBrajesh Kumar Kanchan
Brajesh Kumar Kanchan
Microchannel research has emerged significantly in the last decade due to its several applications, viz., heat exchanger, pharmaceutical, etc. Although several micro-machining processes have been developed in the previous few decades, the contemporary utilization of laser micromachining is minimal. In this context, the current research investigates the material characterization and thermal analysis of corrugated aluminum channels using an experimental and numerical approach. Herein, the types of equipment used are pulsed laser, scanning electron microscope, and energy-dispersive X-ray spectroscopy for experimental analysis. Moreover, the numerical investigation has been conducted using the finite-element method. The current study developed a numerical model for transient thermal analysis utilizing a Gaussian heat source. After that, the output data value is comparable to laser micromachining for experimental inquiry. The results of laser micromachining are shown in terms of heat affected zone (HAZ), depth, and width. The microstructural analysis revealed that the coarser grains are formed near HAZ, whereas finer grains with cracks are located near the laser focal point.

11 January 2021
Verified
Book Chapter
Closed access
PDF file
GCGuddakesh kumar chandan
Guddakesh kumar chandan
CSChinmaya Kumar Sahoo
Chinmaya Kumar Sahoo

25 November 2022 in Proceedings of the Institution of Mechanical Engineers, Part E: Journal of Process Mechanical Engineering
Verified
Journal Article
Closed access
MAMohd Aslam
Mohd Aslam
GCGuddakesh kumar chandan
Guddakesh kumar chandan
BKBrajesh Kumar Kanchan
Brajesh Kumar Kanchan
In the present paper, plasma-assisted physical vapor depositions (PAPVDs) have been used to extract the TiN and titanium aluminum nitride (TiAlN). Further, plasma nitriding (PN) has been used prior to thin-film deposition of TiN on AISI 304 stainless steel material using intentional biasing (in the coating). PAPVD is integrated to investigate the thermal resistant effect coating of AISI 304 stainless steel by TiN coating using finite-element analysis. The morphology of elements on the coating was studied by field emission scanning electron microscopy, X-ray diffraction (XRD), and energy-dispersive X-ray spectroscopy. From XRD analysis, it has been observed that at the coated zone Ti, TiN was found on the AISI 3O4 stainless steel. The results in microhardness through the Vickers microhardness tester have been measured up to 350 Hv for the base sample at a 10 g load. Moreover, TiN/(PN + TiN) coated samples were measured with an average microhardness of 2220, 963, and 720 Hv for the nitride sample. In addition to this, the microhardness of TiAlN was found up to 1890 and 2400 Hv for different samples. The thickness of the film is around 1.4279 µm (TiN) and 1.888 µm (TiAlN) in 1 h of deposition.