Nanocellulose has recently gained a significant level of attention from academic and industrial researchers due to its non-toxic, biocompatible, bio-degradable, low-cost, and easy availability that connects many applications. In this research, cellulose extracted from betel nut husk fiber (BNHF) was converted to nanocellulose by chemical technique to examine their potential for use as reinforcement in bio-composite applications. The cellulose isolated from BNHF was subjected to acid hydrolysis using 62% sulfuric acid under ultrasonic treatment to convert cellulose into nanocellulose. The particle size of nanocellulose was determined by particle size analyzer. The morphology, structure and thermal properties of nanocellulose were also determined by scanning electron microscope (SEM) and Fourier-transform infrared (FTIR), thermogravimetric analysis (TGA), and differential scanning calorimetric (DSC) analysis. The bio-composites of nanocellulose–polyvinyl alcohol (PVA) and cellulose–PVA were prepared with different weight percentages (1–5%) of nanocellulose and cellulose via casting methods. The tensile, thermal and morphological properties were characterized for all composites. Enhancement in the tensile, thermal, and morphological properties was found in the nanocellulose–PVA biocomposites.
Conductive polymer composites are becoming more important and useful in many electrical applications. This paper reports on the carbon black (CB) reinforced polyvinyl chloride (PVC) conductive composites. Conductive filler CB was reinforced with thermoplastic PVC by compression molding technique to make conductive composites. The particle size of CB was measured, as it affects the electrical conductivity of the composites. Different types of CB-PVC compression-molded composites were prepared, using CB contents from 5 to 30 wt %. The electrical and tensile properties of these composites were studied and compared. Improved electrical properties were obtained for all CB-PVC conductive polymer composites compared to virgin PVC composite. However, the tensile properties of the CB-PVC composites increased up to 15 wt % CB loading, and then decreased, and elongation at break decreased with increasing CB loading. The structure of the CB, PVC and CB-PVC composites were studied by attenuated total reflection-Fourier transform infrared (ATR-FTIR) spectroscopic analysis. ATR-FTIR spectra provide evidence of the formation of CB-PVC composites. The microstructural analyses showed a good dispersion of CB in PVC matrix.
22 March 2007 in Polymer-Plastics Technology and Engineering
In the present work, effects of oxidation and fiber content (from 20 to 35 wt. %) on the physicomechanical properties of jute-polypropylene (PP) composites were studied. Mechanical properties (tensile strength, tensile modulus, elongation at break, flexural strength, flexural modulus, and charpy impact strength) were measured for all raw and oxidized jute-PP composites. Improved mechanical properties were obtained for oxidized jute-PP composites. Interfacial adhesion and bonding between the fiber and PP matrix were investigated by scanning electron micrograph analysis. Improved interfacial interactions and reduced water absorption were found for oxidized jute-PP composites. Water absorption tests of all composites were also performed.
Eco-friendly dyeing of jute packaging fabrics was evaluated using aqueous extraction of factory tea (Camellia sinensis) wastes. Jute and factory tea wastes are available in Bangladesh and jute bags are used for packaging of various exportable agricultural commodities. The extract of factory tea waste (FTW) is dark coffee colored and it was characterized by attenuated total reflection-fourier transform infrared (ATR-FTIR) and microbial analysis. Nontoxic, non-allergic and eco-friendly natural dyeing process of jute packaging fabrics using extract of FTW were developed and optimized. Metal mordants 10 % on the weight of fabric was used to get the fastness properties of dyed jute fabric. The methods of application of mordants were pre-mordanting, simultaneous or meta-mordanting and post-mordanting. The color fastness and tensile properties were measured for all jute packaging fabrics and it is found that the dyed jute packaging fabrics showed a slight decrease in tensile breaking force (N) than undyed jute packaging fabric. The highest color fastness obtained with the meta mordanting method with ferrous sulfate mordant in a shade of dark coffee. The results of the color fastness for light and washing showed an excellent value of grade 4–5.