Dental amalgam is an alloy consisting of a mixture of fine metallic powder of silver, tin, zinc, copper, and a trace amount of palladium in combination with about fifty percent elemental mercury that forms a matrix phase. Dental amalgams consisting of a high-copper content are the most common types of alloys currently utilized for the restoration of decayed, broken, and fractured posterior human teeth. The present research objective was primarily to improve the material properties by determining and analyzing the amount of mercury vapor released from dental amalgam received from eight different commercial brands. The mechanical hardness of the alloys was found to increase with an increase in copper content in the amalgam. The effect of copper addition on material aging was also studied. During the release of mercury vapor, the corresponding energies associated with the release of mercury vapor from each sample were determined for each successive measurement. The results indicated that increasing the copper content of the amalgam counters the release of mercury vapor from posterior teeth and improves the hardness properties.
Developing active electrocatalysts for water splitting is a great challenge due to slow four-electron transfer oxygen evolution reaction. Here, we report the effect of variable oxygen concentrations in sputtered RuO2 thin films on electrochemical performance. The impact of Ar/O2 ratios on the structural, chemical, and optical properties of sputtered RuO2 films is systematically investigated. The as-deposited amorphous RuO2 showed higher catalytic activity as compared to its annealed crystalline counterparts. The X-ray photoelectron spectroscopy results showed controlled stoichiometry with 20% oxygen. The electrochemical measurements of the RuO2 deposited with a 4:1 Ar:O2 ratio showed superior performance in cyclic voltammetry, linear sweep voltammetry, and Tafel slope. Transformation of as-deposited amorphous RuO2 into polycrystalline films is observed at 400 °C of annealing temperature. Film thickness is increased with increasing O2 concentration during deposition. This study highlights that sputtered RuO2 thin films with varying oxygen concentration during deposition can influence the electrocatalytic activities in water-splitting applications.
Titanium oxynitride (TiNO) thin films represent a multifaceted material system applicable in diverse fields, including energy storage, solar cells, sensors, protective coatings, and electrocatalysis. This study reports the synthesis of TiNO thin films grown at different substrate temperatures using pulsed laser deposition. A comprehensive structural investigation was conducted by X-ray diffraction (XRD), X-ray photoelectron spectroscopy (XPS), Non-Rutherford backscattering spectrometry (N-RBS), and X-ray absorption spectroscopy (XAS), which facilitated a detailed analysis that determined the phase, composition, and crystallinity of the films. Structural control was achieved via temperature-dependent oxygen in-diffusion, nitrogen out-diffusion, and the nucleation growth process related to adatom mobility. The XPS analysis indicates that the TiNO films consist of heterogeneous mixtures of TiN, TiNO, and TiO2 phases with temperature-dependent relative abundances. The correlation between the structure and electrochemical behavior of the thin films was examined. The TiNO films with relatively higher N/O ratio, meaning less oxidized, were more electrochemically active than the films with lower N/O ratio, i.e., more oxidized films. Films with higher oxidation levels demonstrated enhanced crystallinity and greater stability under electrochemical polarization. These findings demonstrate the importance of substrate temperature control in tailoring the properties of TiNO film, which is a fundamental part of designing and optimizing an efficient electrode material.
Two sets of high-quality epitaxial ruthenium oxide (RuO2) thin films with different thicknesses were synthesized in situ on cost-competitive sapphire substrates by using a pulsed laser deposition technique. The first set of films, with a thickness of 40 nm and a sheet resistance of 15.7 Ω/□, was prepared using 2100 laser pulses, while the second set of films, with a thickness of 87 nm and a sheet resistance of 6.7 Ω/□, was prepared using 4800 laser pulses. All other deposition parameters were kept the same. The post-deposition structural and morphological measurements showed that both sets of films grew at the same growth rate, had the same crystallinity, similar grain boundary density, and slightly different surface roughness. The thicker RuO2 films achieved an overpotential of 280 mV for the oxygen evolution reaction at a current density of 100 μA/cm2, comparable to or exceeding the performance of films grown on more expensive substrates. Comparatively, the thinner RuO2 films, which have a significantly higher charge transfer resistance (250 Ω versus 100 Ω for thick films), display a higher overpotential of 320 mV. These results indicate that the lower electrical resistance of thicker films promotes charge transfer through the film body, leading to superior electrocatalytic properties.
This study investigates the electrochemical properties of ruthenium dioxide RuO2 (100) thin films to understand the effect of varying oxygen deposition ambience on the activity-stability compromise and the degradation pathways consisting of the Lattice Oxygen Mechanism (LOM) and Adsorption Evolution Mechanism (AEM). Electrochemical evaluation of the RuO2 films in the oxygen evolution reaction (OER) in both alkaline and acidic media shows a lower overpotential for less oxygenated films than for more oxygenated films. Stability analysis reveals that, under alkaline conditions, the less oxygenated RuO2 thin-film samples experience a ∼16.5% reduction in current density, while the more oxygenated films experience a ∼9% reduction after 3 h. In acidic conditions, a higher current reduction of ∼21% was observed for the less oxygenated samples, whereas an improved current output of up to 17% was observed for the more oxygenated samples. The Ru dissolution trend for less oxygenated and more oxygenated films showed more than an order of magnitude variation under alkaline conditions and less than 1 order of magnitude under acidic conditions. Additionally, Ru metal dissolution increased by an average of 2 orders of magnitude under acidic conditions compared to alkaline conditions. Faradaic efficiency (FE) was considerably low for the more oxygenated films under both acidic and alkaline conditions. Based on the observed high current density, low overpotential, and high FE, we hypothesize that while LOM is operative in less oxygenated samples, AEM is operative in more oxygenated samples.
High-quality, multifunctional two-dimensional (2D) titanium oxynitide (TiNO) thin films and one-dimensional (1D) TiNO nanowires have been synthesized using a pulsed laser deposition, a simple, fast, and congruent evaporation method. First-principles calculations as a function of surface orientation and termination indicate that surface oxidation of TiNO nanowires can stabilize the (110) orientation observed experimentally. The specific capacitance value for the TiNO nanowire samples (2725 mF/cm2) has been found to be nearly six times more than that of the TiNO thin film samples (400 mF/cm2), which is attributed to the high packing density of TiNO nanowires over a given area. The nanowire samples have also been found to exhibit a significantly higher energy density (1.35 μWh/cm2) than the TiNO thin-film samples (0.33 μWh/cm2). Thus, the TiNO material system in thin-film and nanowire forms has been demonstrated to be a promising candidate for use as an electrode material in supercapacitors and other charge-storage applications.