In this study, the physicochemical behaviors of the (110), (100), as well as (001) of SnO2 were investigated by using high-resolution direct force spectroscopy. The measurements were conducted between a silica sphere and sample surfaces in 10 mmol/L KCl between pH 3.1 and 6.2 using colloidal probe atomic force microscopy (cp-AFM-hydrophilic). Dissimilar interactions were detected on different-oriented surfaces. The pH values where the force switched from positive to negative can be clearly distinguished and be ordered as SnO2(100) < SnO2(001) ≈ SnO2(110). By fitting the force curves in the Derjaguin–Landau–Verwey–Overbeck theory framework, anisotropic surface potentials were computed between the three sample surfaces following a similar trend as force interaction. To study the implication of crystallographic orientation to surfactant adsorption, we used Aerosol 22 (sulfosuccinamate) as an anionic collector for cassiterite flotation to functionalize the different samples at pH 3. The contact angle measurements, the topography visualizations by AFM, and the force measurement using cp-AFM with hydrophobized spheres (cp-AFM-hydrophobized) have shown that Aerosol 22 was adsorbed on the sample surfaces inhomogeneously. The adsorption followed the range of SnO2(110) > SnO2(100) > SnO2(001) in the concentration from 1 × 10–6 to 1 × 10–4 mol/L.
In this study, a range of miniaturized Ag/AgCl reference electrodes with various layouts were successfully fabricated on wafer-level silicon-based substrates with metallic intermediate layers by precisely controlling the electrochemical deposition of Ag, followed by electrochemical chlorination of the deposited Ag layer. The structure, as well as the chemical composition of the electrode, were characterized with SEM & EDS. The results showed that the chlorination is very sensitive to the applied electric field and background solution. Potentiostatic chlorination, in combination with an adjusted mushroom-shaped Ag sealing deposition, enabled the formation of electrochemical usable Ag/AgCl layers. The stability of the electrodes was tested using open circuit potential (OCP) measurement. The results showed that the reference electrodes stayed stable for 300 s under 3 M KCl solution. The first stage study showed that the stability of the Ag/AgCl reference electrode in a chip highly depends on chip size design, chlorination conditions, and a further protection layer.
7 June 2019 in Geostandards and Geoanalytical Research
In this study, synthetic pure cassiterite and cassiterite doped with two different Fe contents were successfully recrystallized by means of sintering. Their crystal structure and chemical compositions were characterized by X-ray powder diffraction (XRD) as well as scanning electron microscopy (SEM) combined with energy-dispersive X-ray (EDX) analysis. Their floatability was studied by microflotation with a diphosphonic acid surfactant named Lauraphos301 as a collector. Unlike the addition of ferric ions in solution, which strongly depressed the floatability of all of the cassiterite samples, a much higher flotation efficiency of the Fe-doped cassiterite samples was found especially at lower collector concentrations. The cassiterite floatability is proportional to the Fe content in cassiterite at a broad range of pH, and the recovery has the following order: cassiterite with 1417 ppm Fe > cassiterite with 1165 ppm Fe > pure cassiterite. The electrokinetic behavior of the cassiterite samples with and without the collector was studied by electrophoretic measurements and revealed that the chemical interaction dominated the adsorption. With the help of the particle shape analysis, a more angular shape was found for the Fe-doped cassiterite samples. Moreover, without the influence of particle shape, much abundant adsorption of Lauraphos301 was found on the Fe-doped cassiterite samples by AFM topography imaging. The minor amount of Fe in the cassiterite lattice and a more angular shape of the Fe-doped cassiterite samples were believed to enhance floatability collectively. The study reveals that the influence of the chemical composition of the minerals on flotation was almost inextricably bound up with particle morphology and emphasizes the importance of considering both factors and investigating them individually for the flotation study.