Applying transmission Kikuchi diffraction (TKD) allows us to fundamentally investigate the Si-doped-hafnium-oxide (HSO) microstructure that results from the interface layer present in ferroelectric field-effect transistors. In addition to the predominant orthorhombic phase, dendritic HSO grains larger than 100 nm govern the microstructure composition. Furthermore, the observed strong out-of-plane texture aligned along the [110] and [011] axis clearly differs from features found in hafnium oxide thin films grown on TiN layers. Our TKD analysis shows that the texture intensity strongly varies for samples annealed at different temperatures. Additionally, intra-granular misorientation and chemical composition analyses of the layers provide insight into the crystallization process of these ferroelectric thin films.
The rising interest in increased manufacturing maturity of quantum processing units is pushing the development of alternative superconducting materials for semiconductor fab process technology. However, these are often facing CMOS process incompatibility. In contrast to common CMOS materials, such as Al, TiN, and TaN, reports on the superconductivity of other suitable transition-metal nitrides are scarce, despite potential superiority. Here, we demonstrate fully CMOS-compatible fabrication of HfN and ZrN thin films on state-of-the-art 300 mm semiconductor process equipment, utilizing reactive DC magnetron sputtering on silicon wafers. Measurement of mechanical stress and surface roughness of the thin films demonstrates process compatibility. We investigated the materials phase and stoichiometry by structural analysis. The HfN and ZrN samples exhibit superconducting phase transitions with critical temperatures up to 5.84 and 7.32 K, critical fields of 1.73 and 6.40 T, and coherence lengths of 14 and 7 nm, respectively. A decrease in the critical temperature with decreasing film thickness indicates mesoscopic behavior due to geometric and grain-size limitations. The results promise a scalable application of HfN and ZrN in quantum computing and related fields.
The study presented investigates the fatigue strength of the (α+β) Ti-6Al-4V-ELI titanium alloy processed by laser cutting with and without mechanical post-processing. The surface quality and possible notch effects as a consequence of non-optimized intermediate cutting parameters are characterized and evaluated. The microstructural changes in the heat-affected zone (HAZ) are documented in detail and compared to samples with a mechanically post-processed (barrel grinding, mechanical polishing) surface condition. The obtained results show a significant increase (≈50%) in fatigue strength due to mechanical post-processing correlating with decreased surface roughness and minimized notch effects when compared to the surface quality of the non-optimized laser cutting. The martensitic α’-phase is detected in the HAZ with the formation of distinctive zones compared to the initial equiaxial α+β microstructure. The HAZ could be removed up to 50% by means of barrel grinding and up to 100% through mechanical polishing. A fracture analysis revealed that the fatigue cracks always initiate on the laser-cut edges in the as-cut surface condition, which could be assigned to an irregular macro and micro-notch relief. However, the typical characteristics of the non-optimized laser cutting process (melting drops and significant higher surface roughness) lead to early fatigue failure. The fatigue cracks solely started from the micro-notches of the surface relief and not from the dross. As a consequence, the fatigue properties are dominated by these notches, which lead to significant scatter, as well as decreased fatigue strength compared to the surface conditions with mechanical finishing and better surface quality. With optimized laser-cutting conditions, HAZ will be minimized, and surface roughness strongly decreased, which will lead to significantly improved fatigue strength.
This study examined the fatigue properties of a newly developed cast and thermomechanical processed (β)-Ti-40Nb alloy for a possible application as biomedical alloy due to exceptional low Young’s modulus (64-73 GPa), high corrosion resistance and ductility (20-26%). Focusing on the influence of two microstructural states with fully recrystallized β-grain structure as well as an aged condition with nanometer-sized ω-precipitates, tension-compression fatigue tests (R=-1) were carried out under lab-air and showed significant differences depending on the β-phase stability under cyclic loading. Present ω- precipitates stabilized the β-phase against martensitic α’’ phase transformations leading to an increased fatigue limit of 288 MPa compared to the recrystallized state (225 MPa), where mechanical polishing and subsequent cyclic loading led to formation of α’’-phase due to the metastability of the β-phase. Additional studied commercially available (β)-Ti-45Nb alloy revealed slightly higher fatigue strength (300 MPa) and suggest a change in the dominating cyclic deformation mechanisms according to the sensitive dependence on the Nb-content. Further tests in simulated body fluid (SBF) at 37°C showed no decrease in fatigue strength due to the effect of corrosion and prove the excellent corrosion fatigue resistance of this alloy type under given test conditions.
In this study, a range of miniaturized Ag/AgCl reference electrodes with various layouts were successfully fabricated on wafer-level silicon-based substrates with metallic intermediate layers by precisely controlling the electrochemical deposition of Ag, followed by electrochemical chlorination of the deposited Ag layer. The structure, as well as the chemical composition of the electrode, were characterized with SEM & EDS. The results showed that the chlorination is very sensitive to the applied electric field and background solution. Potentiostatic chlorination, in combination with an adjusted mushroom-shaped Ag sealing deposition, enabled the formation of electrochemical usable Ag/AgCl layers. The stability of the electrodes was tested using open circuit potential (OCP) measurement. The results showed that the reference electrodes stayed stable for 300 s under 3 M KCl solution. The first stage study showed that the stability of the Ag/AgCl reference electrode in a chip highly depends on chip size design, chlorination conditions, and a further protection layer.
1 October 2017 in International Journal of Fatigue