The article presents the possibility of increasing the water resistance of gypsum binders (GBs) obtained based on synthetic gypsum by introducing additives derived from industrial wastes. Regularities were obtained for the influence of the type and amount of additives on the water/gypsum ratio (W/G), strength indicators and water resistance of high-strength GB. The introduction of a single-component additive to improve water resistance does not have a significant effect. Complex additives based on Portland cement, granulated blast-furnace slag, electric steel-smelting slag, expanded clay dust and granite screenings of various fractions have been developed that make the maximum contribution to improving the water resistance of a high-strength GB based on synthetic calcium sulphate dihydrate, which made it possible to increase the water-resistance coefficient from 0.39 to 0.82.
In this study, hard wear-resistant Ti-Si-C coatings were deposited on Cu-Cr materials to improve their performance as sliding electrical contact materials. A ceramic disk composed of Ti3SiC2 and TiC phases was used as a target for DC magnetron sputtering to deposit the coatings. The influence of the power supplied to the magnetron on the chemical composition, structure, and friction coefficient of the coatings was examined. The coatings demonstrated high hardness (23–25 GPa), low wear rate (1–3 × 10−5 mm3/N/m) and electrical resistance (300 μOhm·cm), and fair resistance to electroerosion. The coating deposited at 450 W for 30 min displayed optimal properties for protecting the Cu-Cr alloy from the arc effect.
In the present study, a powder of Ti-18Zr-15Nb biomedical alloy with spongy morphology and with more than 95% vol. of β-Ti was obtained by reducing the constituent oxides with calcium hydride. The influence of the synthesis temperature, the exposure time, and the density of the charge (TiO2 + ZrO2 + Nb2O5 + CaH2) on the mechanism and kinetics of the calcium hydride synthesis of the Ti-18Zr-15Nb β-alloy was studied. Temperature and exposure time were established as crucial parameters with the help of regression analysis. Moreover, the correlation between the homogeneity of the powder obtained and the lattice microstrain of β-Ti is shown. As a result, temperatures above 1200 °C and an exposure time longer than 12 h are required to obtain a Ti-18Zr-15Nb powder with a single β-phase structure and uniformly distributed elements. The analysis of β-phase growth kinetics revealed that the formation of β-Ti occurs due to the solid-state diffusion interaction between Ti, Nb, and Zr under the calcium hydride reduction of TiO2 + ZrO2 + Nb2O5, and the spongy morphology of reduced α-Ti is inherited by the β-phase. Thus, the results obtained provide a promising approach for manufacturing biocompatible porous implants from β-Ti alloys that are believed to be attractive candidates for biomedical applications. Moreover, the current study develops and deepens the theory and practical aspects of the metallothermic synthesis of metallic materials and can be compelling to specialists in powder metallurgy.