Zeyu Bian

Zeyu Bian


Research Focus & Metrics

Academic Career Length

5Years (2022-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
10 June 2023 in Materials
Verified
Journal Article
Open access
PDF file
KWKangbao Wang
Kangbao Wang
LMLitao Ma
Litao Ma
CYChen Yang
Chen Yang
ZBZeyu Bian
Zeyu Bian
DZDongdong Zhang
Dongdong Zhang
Xifeng LiXifeng Li
Xifeng Li
With the rising demand for nuclear energy, the storage/transportation of radioactive nuclear by-products are critical safety issues for humans and the environment. These by-products are closely related to various nuclear radiations. In particular, neutron radiation requires specific protection by neutron shielding materials due to its high penetrating ability to cause irradiation damage. Herein, a basic overview of neutron shielding is presented. Since gadolinium (Gd) has the largest thermal neutron capture cross-section among various neutron absorbing elements, it is an ideal neutron absorber for shielding applications. In the last two decades, there have been many newly developed Gd-containing (i.e., inorganic nonmetallic-based, polymer-based, and metallic-based) shielding materials developed to attenuate and absorb the incident neutrons. On this basis, we present a comprehensive review of the design, processing methods, microstructure characteristics, mechanical properties, and neutron shielding performance of these materials in each category. Furthermore, current challenges for the development and application of shielding materials are discussed. Finally, the potential research directions are highlighted in this rapidly developing field.

27 April 2024 in Materials
Verified
Journal Article
Open access
PDF file
MWMingliang Wang
Mingliang Wang
QWQian Wang
Qian Wang
ZBZeyu Bian
Zeyu Bian
SCSiyi Chen
Siyi Chen
YGYue Gong
Yue Gong
HWHaowei Wang
Haowei Wang
The wide size range and high tendency to agglomerate of in-situ TiB2 particles in reinforced Al matrix composites introduce great difficulties in their size characterization. In order to use a nanoparticle size analyzer (NSA) to obtain the precise size distribution of TiB2 particles, a controlled size characterization process has been explored. First, the extraction and drying processes for TiB2 particles were optimized. In the extraction process, alternated applications of magnetic stirring and normal ultrasound treatments were proven to accelerate the dissolution of the Al matrix in HCl solution. Furthermore, freeze-drying was found to minimize the agglomeration tendency among TiB2 particles, facilitating the acquisition of pure powders. Such powders were quantitatively made into an initial TiB2 suspension. Second, the chemical and physical dispersion technologies involved in initial TiB2 suspension were put into focus. Chemically, adding PEI (M.W. 10000) at a ratio of mPEI/mTiB2 = 1/30 into the initial suspension can greatly improve the degree of TiB2 dispersion. Physically, the optimum duration for high-energy ultrasound application to achieve TiB2 dispersion was 10 min. Overall, the corresponding underlying dispersion mechanisms were discussed in detail. With the combination of these chemical and physical dispersion specifications for TiB2 suspension, the bimodal size distribution of TiB2 was able to be characterized by NSA for the first time, and its number-average diameter was 111 ± 6 nm, which was reduced by 59.8% over the initial suspension. Indeed, the small-sized and large-sized peaks of the TiB2 particles characterized by NSA mostly match the results obtained from transmission electron microscopy and scanning electron microscopy, respectively.

6 December 2022 in Metals
Verified
Journal Article
Open access
PDF file
PRPeng Rong
Peng Rong
XFXin Fang
Xin Fang
YXYakai Xiao
Yakai Xiao
QWQian Wang
Qian Wang
ZBZeyu Bian
Zeyu Bian
Zhe ChenZhe Chen
Zhe Chen
Strong obstacles can greatly impede the motion or transmission of dislocations, which can be reflected by strain rate sensitivity and activation volume. In this study, the strain rate sensitivity and activation volume of overaged Al-Zn-Mg-Cu alloys with a grain size of 3.1 μm fabricated by powder metallurgy were measured by two different methods: a stress relaxation test and strain rate jump test. It was found that the former method gave much higher strain rate sensitivity values. After reviewing the conventional theory of stress relaxation test, it is unreasonable that the activation volume at each cycle during the stress relaxation test is a constant. At a strain rate higher than 10−5 s−1, ∂lnε˙/∂τ*, which is proportional to the activation volume in the conventional theory of the stress relaxation test, increases significantly, and nearly linearly increases with the strain rate in its logarithmic form, while at a strain rate lower than 10−5 s−1, the value of ∂lnε˙/∂τ* is nearly a constant. The grain boundary sliding mechanism was incorporated into the plastic deformation during the stress relaxation test, and the strain rate sensitivity and activation volume obtained by stress relaxation after modification agree well with that obtained by the strain rate jump test.

12 April 2024 in Materials
Verified
Journal Article
Open access
PDF file
MWMingliang Wang
Mingliang Wang
ZBZeyu Bian
Zeyu Bian
AZAilin Zhu
Ailin Zhu
CYCai Yulong
Cai Yulong
DZDongdong Zhang
Dongdong Zhang
HWHaowei Wang
Haowei Wang
This work has studied the co-addition of Sc and Zr elements into the Al-1.75wt%Fe-1.25wt%Ni eutectic alloy. The changes in the microstructure, electrical conductivity, and Vickers hardness of the Al-1.75wt%Fe-1.25wt%Ni-0.2wt%Sc-0.2wt%Zr alloy during heat treatment were studied. The results showed that two-step aging can effectively improve the aging response of the alloy over the single-step aging method. This was ascribed to the minimization of the diffusion difference between Sc and Zr elements. Furthermore, the homogenization treatment can also improve the aging response of the alloy by alleviating the uneven distribution of Sc and Zr. Nevertheless, the micro-alloyed elements exceeded the solid solubility limit in the Al-1.75wt%Fe-1.25wt%Ni-0.2wt%Sc-0.2wt%Zr alloy, and their strengthening effect has ever achieved the best prospect. Finally, both Sc and Zr contents were reduced simultaneously, and the aging response of the Al-1.75wt%Fe-1.25wt%Ni-0.15wt%Sc-0.1wt%Zr alloy was improved by optimized heat treatment. The underlying mechanisms for this alloy design and the corresponding microstructure–mechanical property relationship were analytically discussed.