Materials with high barrier properties against oxygen are required for the packaging of many sensitive foods. Since commodity polymers lack these properties, additional barrier materials are used in plastic-based barrier packaging. These are usually more expensive than commodity polymers and, in higher fractions, also make recycling more difficult. Current developments, therefore, aim at barrier layers that are as thin as possible but retain the barrier properties. One approach is to incorporate nanoparticles into these layers. In this study, the barrier properties of nanocomposite coatings, consisting of unmodified polyvinyl alcohol (PVA), and dispersed stick-shaped halloysite (Hal) or platelet-shaped montmorillonite (MMT) silicate nanoparticles, were investigated. The PVA was dissolved in aqueous nanoparticle dispersions, which were prepared by mechanical shearing, to produce the so-called “nanolacquer.” Nanolacquers with nanoparticle concentrations of 7, 30, and 47 vol% with respect to PVA were applied in a single process step with k-bar on a polypropylene substrate film. The integration of 30 vol% platelet-shaped MMT enhances the barrier performance in comparison to pure PVA by a factor of 12 and 17 for oxygen and helium, respectively. Scanning electron microscopy (SEM) shows a homogeneous distribution and a parallel alignment of the nanoparticles within the coated layer. An increase in the crystallinity of PVA was observed due to the nanoparticle integration as demonstrated by x-ray diffraction (XRD) measurements. The investigation by Fourier transform infrared (FTIR) spectroscopy and the activation energy of the permeation coefficient indicate an interaction between the nanoparticles and the PVA. The theoretically calculated values for barrier enhancement accord well with the experimental values, which emphasizes that the gas barrier improvement for oxygen and helium is mainly dominated by the tortuous path effect.
The integration of platelet-shaped montmorillonite particles to improve the oxygen barrier of polyvinyl-alcohol-based barrier layers is state-of-the-art, but research on roll-to-roll coatings of such composite barrier lacquers has not been widely published. In this study, two different coating techniques, slot-die and reverse gravure, were used on a roll-to-roll scale to apply barrier lacquers comprising polyvinyl alcohol and montmorillonite. The lacquers were analyzed regarding viscosity at certain shear rates and surface energy and the dried coating layers regarding oxygen barrier, surface morphology, and particle orientation. Low permeability coefficients delivering a high oxygen barrier of 0.14 and 0.12 were achieved for the coating layers with slot-die and reverse gravure coating, respectively. It turned out that the properties of the barrier lacquer need to be adjusted to the coating technique to achieve high oxygen barrier performance. By tailoring the barrier lacquer formulation, the orientation of the platelet-shaped montmorillonite particles can be achieved using both techniques. A low solid content of down to 3 is preferable for the premetered slot-die coating, because it results in low agglomeration quantity in the coating layer. A high solid content of up to 9 is preferable for the self-metered reverse gravure coating to assure a homogeneously coated layer.
In addition to the mechanical properties and barrier performance, one of the key properties of flexible films used in food packaging is the resistance of their gas barrier layer to buckling and bending. Testing the gas barrier before and after mechanical stress is time-consuming and resource-intensive, but important to assure a certain gas barrier during the whole life time of the package until food consumption. The aim of this study was, on the one hand, to identify the most significant influencing factors of a composite lacquer formulation and coating on its buckling resistance and, on the other hand, to show a fast and efficient method to identify defects occurring during buckling. The influence of mechanical stress was simulated via Gelbo-Flex treatment, and the samples were examined and evaluated before and after using light microscopy. The evaluation was verified with scanning electron microscopy (SEM) and helium barrier measurement. Polyethylene terephthalate (PET) and polyethylene (PE) films were coated with composite barrier lacquers made of polyvinyl alcohol (PVA) and montmorillonite (MMT) and the wet coating layer thickness (20, 40, 80, and 130 μm) and the composition of the coating were changed. It was found that thin coatings are more resistant to buckling than thick coatings. It was also shown that a higher proportion of MMT in the coating layer leads to a better gas barrier, but poorer buckling resistance. Additionally, it was found that soft PE films are already subjected to high stresses during the coating process, which means that barrier coatings do not build up ideally. However, the barrier-coated soft film withstood mechanical stress better and lost less barrier by a lower factor than the counterpart on the basis of PET. To conclude, the evaluation of the buckling resistance with microscopy offers an efficient method during lacquer development; however, the final decision on the right lacquer composition is dependent on many factors.