Powder metallurgy (PM) components are widely used in the auto industry due to the advantage of net-shape forming, low cost, and high efficiency. Still, usage of PM components is limited in the auto industry when encountering rigorous situations, like heavy load, due to lower strength, hardness, wear resistance, and other properties compared to wrought components due to the existence of massive pores in the PM components. In this study, through combining the powder metallurgy process and rolling process, the pores in the PM components were decreased and a homogenous densified layer was formed on the surface, which resulted in the enhancement of the strength, hardness, wear resistance, and other properties, which can expand its range of application. In this paper, we study the impact of different rolling feeds on the performance of the components’ surfaces. We found that with the increase of the rolling feed, the depth of the densified layer increased.
In this investigation, the surface-rolling process was performed to improve the performance of PM (powder metallurgy) parts. Different rolling temperatures were applied and the effect of rolling temperature on the microstructure and mechanical properties of the surface dense layers in the samples were investigated. In the study, room temperature and temperatures of 100 °C, 200 °C, 300 °C were studied during the rolling process. The results confirmed that the sample prepared with a pre-heated temperature of 200 °C had the lowest porosity at the surface area. It also exhibited the highest surface hardness and wear resistance. The optimum rolling temperature was determined to be 200 °C and the related mechanism was discussed.
In recent years, the rolling densification process has become increasingly widely used to strengthen powder metallurgy parts. The original composition of the rolled powder metallurgy blank has a significant effect on the rolling densification technology. The present work investigated the effects of different carbon contents (0 wt. %, 0.2 wt. %, 0.45 wt. %, and 0.8 wt. %) on the rolling densification. The selection of the raw materials in the surface rolling densification process was analyzed based on the pore condition, structure, hardness, and friction performance of the materials. The results show that the 0.8 wt. % carbon content of the surface rolling material can effectively improve the properties of iron-based powder metallurgy parts. The samples with 0.8 wt. % carbon have the highest surface hardness (340 HV0.1) and the lowest surface friction coefficient (0.35). Even if the dense layer depth is 1.13 mm, which is thinner than other samples with low carbon content, it also meets the requirements for powder metallurgy parts such as gears used in the auto industry.