Salami Sagiroglu

Dr. Salami Sagiroglu

orcid

Research Focus & Metrics

Academic Career Length

3Years (2024-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
25 November 2024 in Materials
Verified
Journal Article
Open access
KBKhaled A. A. Babay
Khaled A. A. Babay
İEİsmail Esen
İsmail Esen
SSSalami Sagiroglu
Salami Sagiroglu
HAHayrettin AHLATCI
Hayrettin AHLATCI
EKEsma Keskin
Esma Keskin
This study explored how post-casting heat treatment and forging affected the tribological and microstructural characteristics of 0.20% beryllium (Be)-added CuAl10Ni5Fe4 alloys. The heat-treated CuAl10Ni5Fe4 microstructure exhibits a copper-rich α (alpha)-solid-solution phase, a martensitic β (beta)-phase, and diverse intermetallic κ (kappa)-phases, such as leaf-shaped κI, thin κIII, and black globs. Adding 0.20% beryllium to CuAl10Ni5Fe4 alloys enhanced the dendritic arm thickness, needle-like shape, and κ-phase quantities. Significant κIV- and κII-phase precipitation was observed in the tempered β-phase. Beryllium improves the aluminum matrix’s microstructure. Forging greatly reduced the microstructural thickness of CuAl10Ni5Fe4 and CuAl10Ni5Fe4-0.20% Be alloys. The forging process also developed new κIV-phases. Wear resistance and hardness improved with beryllium. The CuAl10Ni5Fe4-0.20% Be alloy had the highest hardness values (235.29 and 255.08 HB) after solution treatment (ST) and tempering (T) after casting and forging (F). The CuAl10Ni5Fe4-0.20% alloy with Be added had the best wear after solution treatment, tempering, and forging. The CuAl10Ni5Fe4-0.20% Be alloy demonstrated a 0.00272 g weight loss, a 1.36 × 10−8 g/N*m wear rate, and a 0.059 friction coefficient at 10,000 m after forging (F).

25 February 2026 in Materials Science
Verified
Journal Article
Open access
PDF file
AIAbubaker J. A. Irhayim
Abubaker J. A. Irhayim
İEİsmail Esen
İsmail Esen
SSSalami Sagiroglu
Salami Sagiroglu
EKEsma Keskin
Esma Keskin
HAHayrettin AHLATCI
Hayrettin AHLATCI
VKVolkan Karakurt
Volkan Karakurt
This study examined how post-casting heat treatment (solution treatment and tempering) and forging affected the corrosion and microstructural properties of the nickel aluminium bronze (CuAl10Ni5Fe4) with 0.20 % and 0.40% titanium addition. Heat-treated CuAl10Ni5Fe4 alloy microstructures showed copper-rich α-solid solution, martensitic β-phase, and intermetallic κ-phases, such as flake-shaped κI, fine κIII, and black globular κIV. Adding 0.20 % and 0.40 % titanium to CuAl10Ni5Fe4 alloys reduced dendritic arm thickness and increased κ phase abundance. Additionally, significant κIV and κII precipitations were observed in the tempered β phase. Tempering β may cause martensitic β to split into tiny α and κIII phases. The grain refinement of the CuAl10Ni5Fe4, CuAl10Ni5Fe4-0.20 % Ti, and CuAl10Ni5Fe4-0.40 % Ti alloys was significantly noticeable after forging. The alloys retained the same α, β, and κ phases seen in the heat-treated alloys after forging. Titanium's refining effect increased the hardness of the alloy into which it was incorporated. Increased stiff phases, such as tempered β and fine κIV, contribute to increased hardness. The forging process enhanced the hardness of all three alloys. Forged and heat treated CuAl10Ni5Fe4-0.40 % Ti alloy had the highest hardness with 243.50 HB and 256.18 HB, respectively. The microstructural phases α, β, and κ significantly impact the corrosion behaviour of CuAl10Ni5Fe4 alloy. The CuAl10Ni5Fe4-0.40 % Ti alloy after forging had the lowest 24-hour weight loss of 0.003326 mg/dm2. The CuAl10Ni5Fe4 alloy loses the most weight (0.013659 mg/dm²) following heat treatment (S.T.+T) after 24 hours. The minimal corrosion rate for the CuAl10Ni5Fe4-0.40 % Ti alloy after forging was 0.003916 mg/(dm2·day) after 72 hours. Due to stratification, corrosion creates craters. Pitted or porous structures and craters are common. All alloys show a decrease in these structures after forging. The formation of the CuCl2 phase is believed to occur in regions experiencing pitting corrosion.