This study aimed to determine the validity of the digital photocolorimetric (PCM) method in matching the color of human teeth. First, two Vitapan Classical shade guides, each containing 16 shade guide teeth, were visually shade matched, and digital photographs of each three pair of shade guide teeth were taken in a color matching booth. Secondly, visual shade matching of the upper central incisors of 48 subjects was performed by two prosthodontists independently in a chair, using the Vitapan Classical shade guide. The three closest shade guide teeth were visually selected and ranked in order of preference, for which digital photographs were taken under ceiling daylight-corrected fluorescent lighting. All digital images were analyzed on a computer screen using software to calculate the color difference between the reference tooth and other teeth in the same digital image. The percent color matching for the shade guide teeth and human teeth was 88% and 75%, respectively. There was no statistically significant difference in matching the tooth color between the shade guide teeth and human teeth. The digital PCM method is valid for the range of human teeth based on the Vitapan Classical shade guide. This method enhances communication with the laboratory personnel in matching the tooth color.
This study was conducted to test the hypothesis that heat-bonding with a liner positively affects the bond strength and fracture resistance of an implant-supported glass–ceramic crown bonded to a zirconia abutment produced by a computer-aided design/computer-aided milling (CAD/CAM) procedure. Lithium disilicate-reinforced Amber Mill-Q glass ceramic blocks were bonded to 3 mol% yttria stabilized tetragonal zirconia polycrystal (3Y-TZP) blocks by heat-bonding with a liner or cementation with a dual-cure self-adhesive resin cement for a microtensile bond strength test. CAD/CAM implant-supported glass ceramic crowns were produced using Amber Mill-Q blocks and bonded to a milled 3Y-TZP zirconia abutments by heat-bonding or cementation for a fracture test. A statistical analysis was conducted to investigate the significant differences between the experimental results. The mode of failure was analyzed using high-resolution field emission scanning electron microscopy. Chemical bonding was identified at the interface between the zirconia ceramic and liner. The mean tensile bond strength of the liner-bonded group was significantly higher than that of the cement-bonded group. The initial chipping strength of the liner-bonded group was significantly higher than that of the cement-bonded group, although no statistically significant difference was found for the fracture strength. The mode of failure was mixed with cohesive fracture through the liner, whereas the cement-bonded group demonstrated adhesive failure at the interface of bonding.