With the continuous exploitation of bauxite mineral resources, Guangxi bauxite faces many difficulties in alumina production due to its characteristics of high silicon content, high iron content, and a low Al-Si ratio. In view of this, this study is closely related to the key link of bauxite pre-desiliconization and strives to break free from the status quo to improve the aluminum/silicon ratio and help optimize the subsequent alumina-refining process. In the work presented in this paper, the unique mineralogy of Guangxi bauxite was comprehensively considered, covering its complex mineral composition and fine distribution characteristics. The barium hydroxide pre-desilication technology was first used for in-depth experimental exploration, and the silicon removal efficiency under different working conditions was systematically compared. The system compared the silicon removal effect and the associated aluminum loss under different working conditions. The results of this study will lay a solid foundation for the rational and efficient development of bauxite in Guangxi, which is expected to reduce the cost of alumina production, improve the economic benefits for the Guangxi aluminum industry, simultaneously strengthen the efficiency of resource recycling, accelerate the sustainable development of the industry, and provide a useful reference example for subsequent similar studies.
The AZ31B Magnesium alloy matrix syntactic foams containing Al2O3 hollow spheres (Al2O3 − HS) were successfully synthesized by the process of gravity infiltration casting. Extremely high chemical activity of magnesium melt with ceramics at high temperature makes it challenging to synthesize Mg-matrix syntactic foams (MgSFs) by casting. In this work, Al2O3 − HS were coated with MgO using MgCl2 solution after high-temperature calcination to successfully prevent the interfacial reaction. The porosity of the syntactic foams is strongly influenced by the concentration of the MgCl2 solution because it determines the coverage of Al2O3 − HS with the MgO coating and survival of particles. The maximum porosity of the syntactic foam was 41.64 vol.%, and the corresponding density is 1.17 g/cm3. At the MgCl2 solution coating concentration of 0.15 g/ml, the plateau stress of the syntactic foam reaches the maximum value of 55.96 MPa, the energy absorption capacity was 39.27 MJ/m3, and the maximum energy absorption was 26.06 kJ/kg. These properties are comparable to some MgSFs prepared by other methods in recent years.