Catalysts based on CuAl-, CoAl-, and CuCoAl-layered hydroxides with M2+/Al = 2 and Cu/Co = 1 molar ratio were obtained. The effect of amount of cobalt on the structural properties, morphology, surface cations distribution, oxide phase formation, thermal stability of the samples and reduction of metals from them was studied. The effect of reaction conditions (temperature, time, pressure, solvent) and conditions of preliminary treatment of catalysts on their catalytic properties in furfural hydrogenation was established. High selectivity to furfuryl alcohol was observed for all the samples irrespective of pretreatment and reaction conditions. The synergetic effect in furfural hydrogenation between Co and Cu in the CuCoAlOx catalysts was revealed when ethanol is used as a solvent.
Ni(Mg)Al-layered hydroxides with molar ratios of (Ni + Mg)/Al = 2, 3, 4 and Ni/(Ni + Mg) = 0.1, 0.3, 0.5, 0.7 were synthesized by mechanochemical activation. It has been proven that the phase composition of the samples was presented by a single hydrotalcite phase up to Ni/(Ni + Mg) = 0.5. For the first time, catalysts based on Ni(Mg)Al-layered hydroxides prepared by a mechanochemical route have been studied in the reaction of furfural hydrogenation. The correlation between furfural conversion, the selectivity of the products, and the composition of the catalysts was established. The effect of phase composition, surface morphology, and microstructure on the activity of the catalysts was shown by XRD, SEM, and TEM. It was found that catalysts with Ni/(Ni + Mg) = 0.5 have the highest furfural conversion. Herewith, the product selectivity can be regulated by the (Ni + Mg)/Al ratio.