Catalysts based on CuAl-, CoAl-, and CuCoAl-layered hydroxides with M2+/Al = 2 and Cu/Co = 1 molar ratio were obtained. The effect of amount of cobalt on the structural properties, morphology, surface cations distribution, oxide phase formation, thermal stability of the samples and reduction of metals from them was studied. The effect of reaction conditions (temperature, time, pressure, solvent) and conditions of preliminary treatment of catalysts on their catalytic properties in furfural hydrogenation was established. High selectivity to furfuryl alcohol was observed for all the samples irrespective of pretreatment and reaction conditions. The synergetic effect in furfural hydrogenation between Co and Cu in the CuCoAlOx catalysts was revealed when ethanol is used as a solvent.
Ni(Mg)Al-layered hydroxides with molar ratios of (Ni + Mg)/Al = 2, 3, 4 and Ni/(Ni + Mg) = 0.1, 0.3, 0.5, 0.7 were synthesized by mechanochemical activation. It has been proven that the phase composition of the samples was presented by a single hydrotalcite phase up to Ni/(Ni + Mg) = 0.5. For the first time, catalysts based on Ni(Mg)Al-layered hydroxides prepared by a mechanochemical route have been studied in the reaction of furfural hydrogenation. The correlation between furfural conversion, the selectivity of the products, and the composition of the catalysts was established. The effect of phase composition, surface morphology, and microstructure on the activity of the catalysts was shown by XRD, SEM, and TEM. It was found that catalysts with Ni/(Ni + Mg) = 0.5 have the highest furfural conversion. Herewith, the product selectivity can be regulated by the (Ni + Mg)/Al ratio.
Simulation of diffraction patterns for 1D disordered crystals was used to investigate the structure of the initial CO32− containing MgGa LDHs with a different Mg2+/(Mg2+ + Ga3+) ratio equal to 0.67, 0.75, and 0.80; mixed oxides obtained by calcination of LDHs at a temperature of 550 °C; and the hydroxide obtained by hydration of MgGa oxide with the Mg2+ content of 0.80. The initial LDHs contain lamellar inclusions of manasseite structure (polytype 2H1) in the hydrotalcite structure (3R1). A loss of water at 200 °C leads to the formation of a metastable dehydrated phase where layers are packed, as in polytypes 3R2 and 1H, with turbostratic disorder. The structure of mixed oxides is also layered and consists of periclase-like octahedral layers and spinel-like octahedral-tetrahedral layers. Hydration of the oxides results in restoring the initial layered hydrotalcite structure (polytype 3R1) for Mg2+ mole fractions 0.67 and 0.75. For the Mg2+ content of 0.80, the phase composition is represented by the hydroxide with hydrotalcite structure and the layered mixed hydroxide with the alternation of hydrotalcite and brucite lamellar domains, which was also revealed by calculation of diffraction patterns using models of 1D disordered crystals.
Single phase CuCoMgAl-layered hydroxides were obtained by making fine adjustment to their composition through changing the (Co + Cu)/Mg = 0.5; 1; 2; 3 and Co/Cu = 0.5; 1; 2 ratios. The rise of Co/Cu in systems contributed to the increase in their thermal stability. CuCoMgAl-catalysts showed high selectivity of carbonyl group hydrogenation in furfural and 5-hydroxymethylfurfural. In furfural hydrogenation, the selectivity to furfuryl alcohol was more than 99%, and in 5-hydroxymethylfurfural hydrogenation, the selectivity to 2,5-hydroxymethyl furfural was 95%. The surface of the samples with different Co/Cu after calcination and reduction was the same and had a «core-shell» structure (TEM). «Core» consisted of Cu and Co metallic particles. «Shell» consisted of CuCoMgAlOx mixed no-stoichiometric spinel oxides. There was no sintering or change in size of the metallic particles after the reaction. For the sample with Co/Cu = 1, their phase composition after reaction remained unchangeable. The increase of Co/Cu led to the formation of an X-ray amorphous phase after the reaction. This suggests the decrease in structural stability of this sample. The obtained results prove the prospects of using bimetallic CoCu-systems for hydrogenation of furan aldehydes, and opens up new directions for further research and improvement.
The essay considers historical aspects of the appearance and development of methods for catalytic hydrogenation of organic compounds, starting from the works by P. Sabatier and V.N. Ipatieff. Particular attention is paid to the results of synthesis and investigation of hydrogenation metal catalysts based on Ni, Pd and Pt since they are significant for practical application. Modern trends and promising lines of investigation in the field of hydrogenation processes and catalysts are revealed.
Catalysts based on CoCuMgAl mixed oxides were synthesized and studied in the hydrogenations of furfural and 5-hydroxymethylfurfural under different conditions. The changes in the structural properties of the catalysts at different stages of their preparation were studied using a set of physical methods (XRD, SEM, and TEM). It was shown that the fine regulation of the chemical compositions of the mixed oxides (i.e., changes in the Co/Cu ratio) made it possible to vary the structure, morphology, and catalytic properties of the samples. The phase composition of catalysts with Co/Cu = 1 did not change during the catalytic reaction, although the initial catalysts had a less-homogeneous morphology. 5-hydroxymethylfurfural conversion was higher for the samples with Co/Cu = 1. Furfural conversion increased when raising the Co/Cu ratio. The selectivity toward furfuryl alcohol for the catalyst with Co/Cu = 2 under mild conditions of furfural hydrogenation was more than 99%. The results obtained are important for the development of the scientific foundations of the preparation of hydrogenation catalysts with a fine-tunable composition in order to obtain the desired hydrogenation products.