The utilization of TiB2 particle reinforcement in aluminium matrix composites, particularly with Al6063, has been explored in this study for its resilience to mechanical erosion, low oxidation rate, and excellent heat conductivity. The composite was produced using stir casting with 9 wt% TiB2. The investigation focuses on wear behaviour, examining three key process parameters such as load, sliding speed, and covering sliding distance across four settings to identify the optimal combination for achieving a favourable wear rate. Statistical analysis of variance reveals significant differences among the tested parameters. Conclusively, the study highlights the superiority of the grey-fuzzy approach over a simple grey relational grade in validating decision-making for wear performance attributes. The research identifies the ost significant grey relational grade and grey fuzzy grade values as 0.913 and 0.902, respectively. These values correspond to optimal operating conditions, specifically a 15 N load, a sliding speed of 15 m/s, and a sliding distance of 1200 m. The findings underscore the efficacy of the grey-fuzzy technique in authenticating decision-making processes related to wear performance characteristics, emphasizing its superiority over relying solely on a plain grey relational grade.
14 August 2019 in Journal of the Brazilian Society of Mechanical Sciences and Engineering
The ultrasonic-assisted stir-casting method has effectively prepared A356 alloy/AlN composites. The ultrasonic treatment and integration of AlN particles are shown to greatly enhance the mechanical and wear characteristics of the matrix via grain refinement. By incorporating 9 vol.% of AlN reinforced particles, the average grain size of A356 alloy was decreased from 36 μm to 10 μm. Additionally, the hardness and tensile strength experienced a respective rise of 60.6% and 32%. With an increase in the volume percentage of AlN particles, it is found that both the wear rate and the friction coefficient decreased. It is also observed that the A356 alloy displayed severe wear, whereas the composites exhibited moderate wear.