In this paper, the MIG welding process is utilized to weld a 3 mm thick 5052 aluminum alloy plate by using ER5356 welding wire as filler. The effects of different welding speeds on the microstructure and mechanical properties of the weld are systematically studied utilizing a metallographic microscope, x-ray diffractometer, scanning electron microscope, room temperature tensile, and microhardness. It was found that there were pore defects in the samples at lower or higher welding speeds, and there was no penetration at the maximum welding speed. When the welding speed is 650 mm min−1, the weld is well-formed, the surface is flat without pores, the fish scale is evenly distributed, and the weld shows good penetration. The intermetallic compounds of all the welds are mainly composed of α(Al), Mg2Si, Al3Fe, and Al3Mg2. The mechanical properties of the samples show that the hardness of the weld reaches the maximum value of 56.7HV at this welding speed, and the tensile strength and elongation are 210 MPa and 14.3%, respectively. The fracture is located at the junction of the base metal and the heat-affected zone, and the fracture type showed typical ductile fracture.
This work attempts to develop a theoretical model in combination with the representative volume element (RVE) theory for realizing rapid fatigue limit prediction. Within the thermodynamic framework, it is believed that two components, namely anelastic and microplastic behaviors, which correspond to recoverable and non-recoverable microstructural motions, contribute to temperature variation during high-cycle fatigue. Based on this, the constitutive equation of the response relationship between the temperature rise evolution and the stress amplitude of metallic materials can be deduced in combination with the heat balance equation. Meanwhile, a determination approach for the thermographic experimental data for accurate fatigue limit estimation is developed by combining it with a statistical method. Finally, the experimental data of metallic specimens and welded joints were utilized to validate the proposed model, and the results demonstrated great agreement between experimental and predicted data.
The welding of TC4 titanium alloy sheets with a thickness of 1 mm was successfully accomplished by a swinging laser. The microstructure and mechanical properties of the welding seam under different swing amplitudes were studied. In this paper, the microstructure, phase composition, mechanical properties, and fracture morphology of the weld with swing frequency of 50 Hz and different swing amplitudes (0.2 mm, 1 mm, 2 mm, and 3 mm) were tested and analyzed. The results show that basket-weave microstructures are present in the fusion zone of welds under different oscillation amplitudes, but the morphology of martensite within the basket-weave differs. The weld microstructure is mainly composed of acicular α′ martensite, initial α phase, secondary α phase, and residual β phase. The hardness of the weld is higher than that of the base metal, and the overall hardness decreases from the weld center to the base metal. When the oscillation amplitude A = 1 mm, the weld microstructure has the smallest average grain size, the highest microhardness (388.86 HV), the largest tensile strength (1115.4 MPa), and quasi-cleavage fracture occurs. At an oscillation amplitude of A = 2 mm, the tensile specimen achieves the maximum elongation of 14%, with ductile fracture as the dominant mechanism.
The microstructure, phase composition, hardness, and tensile properties of the Ti-48Al-2Cr-5Nb alloy have been systematically investigated using laser additive manufacturing technology. Results indicate that both the as-deposited and annealed microstructures contain both the α2 (Ti3Al) and γ (TiAl) phases. As the annealing temperature increased, the structure changed significantly from a large block structure to a fine equiaxed structure and finally to a large lamellar structure. Nevertheless, the amount and distribution of precipitation of α2 phase are obviously different, especially during the annealing at 1260 °C, where the fine α2 phases are evenly distributed on the γ phase matrix. The hardness value of the as-deposited sample is the highest, with a HV value of 484 at the room temperature, while the hardness value of the annealed sample at 1260 °C is the smallest, with a HV value of 344. An annealed sample at 1260 °C exhibits the highest tensile strength and elongation at room temperature, with values of 598 MPa and 2.1%, respectively. These values are increased by 1.15 times and 1.4 times compared to the as-deposited sample (519 MPa, 1.5%).
26 April 2025 in Journal of Materials Engineering and Performance