One-dimensional (1D) SnO2 nanostructures, as n-type semiconductors with a wide band gap, exhibit unique photoelectric properties that offer potential applications in electronic, photoelectric, gas sensing, and energy generation devices. A detailed study of template-free reaction systems is essential to regulate and efficiently synthesise 1DSnO2 nanostructures. This study employed the hydrothermal method to prepare 1DSnO2 nanostructures, with SnCl4·5H2O as the tin source. The impact of various experimental conditions on SnO2 morphology is analysed. Here, 1DSnO2 nanostructures were characterised by analytical methods such as X-ray powder diffraction, transmission electron microscopy, scanning electron microscopy, and field emission double-beam electron microscopy. The results confirmed the formation of 1DSnO2 nanostructures with a mixed morphology of nanorods and nanowires. The nanorods exhibited a length of 422.87 ± 110.15 nm, a width of 81.4 ± 16.75 nm, and an aspect ratio of 5:1, whereas the nanowires displayed a length of 200 ± 45.24 nm, a width of 15 ± 5.62 nm, and an aspect ratio of 13:1. With the addition of 50 mg of polyvinylpyrrolidone and seed crystal, the acquisition time of the 1DSnO2 nanostructures decreased from 48 to 12 h. The 1DSnO2 nanostructures were efficiently obtained without a template, laying the foundation for large-scale production and application.
AgW materials exhibit excellent properties and are widely used as contact materials in low- and medium-voltage switches. In this study, a pre-sintering and infiltration method was employed to pre-sinter W powder with Cu, Ni, and (Cu+Ni) additions in the low temperature range of 950–1050 °C. The low-temperature sintering behaviours of W skeletons with different additives were investigated. Subsequently, AgW (70 wt%), AgW (75 wt%), AgW (80 wt%), and AgW (85 wt%) materials were prepared through infiltration at 1050 °C. The microstructure morphology and physical properties of high-W contact materials were investigated using a metallographic microscope and scanning electron microscope. The mechanism of low-temperature sintering–infiltration of high-W contact materials was elucidated. The results indicate that pure W and 1% Cu-added W skeletons experience minimal linear shrinkage within the temperature range of 950–1050 °C. The linear shrinkage curves of W skeletons with different additives coincided under the conditions of 950–1000 °C/90 min. At 1050 °C, after sintering for 150 min, the particle boundaries in the W skeleton were fully spheroidised, with a dihedral angle of 120°. At 1050 °C and after 150 min of infiltration, cross-sectional micrographs of the AgW material revealed the presence of irregular Ni layers, where Ni spatially enveloped/encapsulated Ag. With an increase in the W content, the electrical conductivity and relative density of AgW (70–85) materials decreased, whereas the hardness of the materials increased.
AgW materials exhibit excellent properties and are widely used as contact materials in low- and medium-voltage switches. In this study, a pre-sintering and infiltration method was employed to pre-sinter W powder with Cu, Ni, and (Cu+Ni) addition in the low temperature range of 950–1050 °C. The low-temperature sintering behaviours of W skeletons with different additives were investigated. Subsequently, AgW70, AgW75, AgW80, and AgW85 materials were prepared through infiltration at 1050 °C. The microstructure morphology and physical properties of high-W contact materials were investigated using a metallographic microscope and scanning electron microscope. The mechanism of low-temperature sintering-infiltration of high-W contact materials was elucidated. The results indicated that pure W and 1% Cu-added W skeletons experience minimal linear shrinkage within the temperature range of 950–1050 °C. The linear shrinkage curves of W skeletons with different additives coincided under the conditions of 950–1000 °C/90 min. At 1050 °C, after sintering for 150 min, the particle boundaries in the W skeleton were fully spheroidised, with a dihedral angle of 120°. At 1050 °C and after 150 min of infiltration, cross-sectional micrographs of the AgW material revealed the presence of irregular Ni layers, where Ni spatially enveloped/encapsulated Ag. With an increase in the W content, the electrical conductivity and relative density of AgW(70–85) materials decreased, whereas the hardness of the materials increased.