The issue of heavy metal pollution has gradually emerged as a significant global concern. Microbial fuel cells (MFCs) hold immense potential for clean energy production and pollutant treatment. However, their limited power generation efficiency hampers the large-scale implementation of MFCs. The porous microstructure of biochar and the excellent physical and chemical properties of rutile render both materials promising catalysts with positive potential. In this study, we employed biochar as a carrier for rutile to fabricate a novel rutile–biochar (Rut-B) composite material, investigating its efficacy in enhancing MFC power generation efficiency as a cathode catalyst, as well as its application in heavy metal pollutant degradation. Scanning electron microscopy (SEM) results confirmed the successful preparation of biochar-loaded rutile composites. The MFC achieved maximum current density and power density values of 152.26 mA/m2 and 9.88 mW/m2, respectively—an increase of 102.7% and 224% compared to the control group without the addition of Rut-B. Furthermore, the biochar-loaded rutile MFC exhibited excellent performance in degrading heavy metal pollutants; within 7 h, the Pb2+ degradation rate reached 92.4%, while the Zn2+ degradation rate reached 84%. These rates were significantly higher than those observed in the control group, by factors of 437.2% and 345%, respectively. The cyclic degradation experiments also demonstrated the outstanding stability of the system over multiple cycles. In summary, this study successfully combined natural rutile with biochar to create an efficient electrode catalyst that not only enhances electricity generation performance but also provides an environmentally friendly and cost-effective approach for remediating heavy metal pollution.
Iron tailings, the major solid waste generated during iron ore beneficiation, possess substantial resource potential, but their utilization remains limited. Although iron tailings can adsorb Cr(VI)-containing oxyanions, their aggregation in aqueous systems restricts adsorption kinetics, resulting in only 24.4% Cr(VI) removal at an initial concentration of 30 mg/L. In this study, an economical biochar–iron tailings composite was synthesized via a one-step pyrolysis method, with biochar serving as a carbon framework to disperse iron tailings and enhance Cr(VI) removal. The composite achieved approximately 50% Cr(VI) removal at 30 mg/L, representing a significant improvement compared with raw iron tailings. In simulated acidic mine wastewater, under optimized conditions of pH 2, a dosage of 0.8 g/L, and 10 mg/L Cr(VI), the composite removed over 95% of Cr(VI) within 8 h and reached 99.95% removal after 24 h. These results demonstrate that biochar effectively alleviates iron tailings aggregation and improves adsorption performance while maintaining a relatively low treatment cost. This biochar–iron tailings composite provides a promising strategy for Cr(VI)-contaminated wastewater treatment and the high-value utilization of iron tailings.
The Huoyanshan Cu-Zn volcanogenic massive sulfide (VMS) deposit, located in the North Qilian Orogenic Belt, China, is of significant economic importance. This study provides new constraints on the ore-forming processes through high-resolution in situ trace element and sulfur isotope analyses of pyrite and sphalerite using LA-(MC)-ICP-MS. Petrographic and geochemical investigations identified three distinct generations of pyrite (Py l to Py III). Early-stage Py I and Py II are characterized by high trace element contents (Au, As, Bi, Cu, Pb), elevated Co/Ni ratios (>1–10), and enriched δ34S values (+4.98‰ to +7.47‰). These signatures indicate precipitation from high-temperature, reduced magmatic–hydrothermal fluids influenced by thermochemical sulfate reduction (TSR). Late-stage Py IIl exhibits markedly lower Co/Ni ratios (<0.1) and lighter δ34S values (+3.72‰ to 3.89‰). This geochemical shift reflects a transition toward a cooler, more oxidized environment driven by the incursion and mixing of ambient seawater as the hydrothermal system waned. Trace element geochemistry of sphalerite reveals an average crystallization temperature of 265.8 °C (derived from the “GGIMFis” geothermometer), consistent with fluid inclusion data and representing a thermal “snapshot” of the waning hydrothermal stage. Systematic discriminant analysis using Ga/In, Ge/In, and Co-Ni-As systematics further confirms a strong magmatic–hydrothermal affiliation.