In this study, we investigated the potential of multilayer TCO structures, specifically those made up of Indium Tin Oxide (ITO) and Indium Zinc Oxide (IZO), for crystalline silicon heterojunction solar cells (SHJ). We used the radiofrequency (RF) magnetron sputtering method to deposit various thin-film structures under various deposition temperatures and evaluated their electrical, optical, and morphological properties. The objective was to obtain films with lower sheet resistances and higher transmittances than those of single-layer thin films. Our results show that the ITO/IZO/ITO/IZO/ITO multilayer film structure deposited at 200 °C achieves the best sheet resistance of 18.5 Ohm/sq and a high optical transmittance of over 90% at a 550 nm wavelength. This indicates that multilayer TCO structures have the potential to be more optically and electrically efficient, and that they can improve the performance of optoelectronic devices. Finally, a power conversion efficiency of 17.46% was obtained for a silicon heterojunction (SHJ) solar cell fabricated using an ITO/IZO/ITO/IZO/ITO multilayer film structure deposited at 200 °C as a front TCO. Our study provides valuable insights into the field of TCOs and offers a promising avenue for future research.
This study examined the impact of temperature optimization on indium tin oxide (ITO) films in monolithic HJT/perovskite tandem solar cells. ITO films were deposited using magnetron sputtering at temperatures ranging from room temperature (25 °C) to 250 °C. The sputtering target was ITO, with a mass ratio of In2O3 to SnO2 of 90% to 10%. The effects of temperature on the ITO film were analyzed using X-ray diffraction (XRD), spectroscopic ellipsometry, and sheet resistance measurements. Results showed that all ITO films exhibited a polycrystalline morphology, with diffraction peaks corresponding to planes (211), (222), (400), (440), and (622), indicating a cubic bixbyite crystal structure. The light transmittance exceeded 80%, and the sheet resistance was 75.1 Ω/sq for ITO deposited at 200 °C. The optical bandgap of deposited ITO films ranged between 3.90 eV and 3.93 eV. Structural and morphological characterization of the perovskite solar cell was performed using XRD and FE-SEM. Tandem solar cell performance was evaluated by analyzing current density-voltage characteristics under simulated sunlight. By optimizing the ITO deposition temperature, the tandem cell achieved a power conversion efficiency (PCE) of 16.74%, resulting in enhanced tandem cell efficiency.
The main focus of our study is to examine and report the room-temperature enhancement of the optoelectronic and photoresponsive performance of ZnO materials induced by dual doping with Al and In, achieved by tailoring the materials' structural and morphological characteristics. Structural analyses confirmed the formation of the hexagonal wurtzite ZnO phase, while doping induced noticeable modifications in the microstructure and morphology of the films. The crystallite size was found to decrease from 54.96 nm for undoped ZnO to 38.66 nm for ZnO/1.0% Al/1.0% In films, indicating dopant-induced grain refinement. Also, morphological analysis revealed that the particle thickness decreased from ∼400.1 to ∼201.6 nm, resulting in an increased surface:volume ratio. We conducted a systematic investigation focusing primarily on their persistent photoconductivity characteristics. Further analyses were performed to examine the detailed mechanisms of photocurrent generation, to observe photonic memory effects, to determine photosensor properties and device sensitivity, and to assess the effects of traps. The sensor devices were tested under a UV light source with a wavelength of 400 nm and an intensity of 75 μW/cm2, within the range of -5 to 5 V. In a dark environment, the current of the undoped ZnO film was 4.35 × 10-6 A, while in the 1.0% Al/1.0% In dual-doped device, this value increased approximately 11 times under UV illumination, reaching 2.11 × 10-4 A and yielding the highest photocurrent. Fast decay component τ1 showed similarity across all samples, varying between 24.74 and 35.68 s. The slow decay time (τ2) determining the memory capacity of the devices was measured as 302.89 s for undoped ZnO, while in the 1.0% Al/1.0% In doped sample, this time constant increased to 533.31 s, reaching its highest value. Our findings provide a basis for designing advanced photoactive materials for use in optoelectronic applications. They also indicate the optimal doping ratio for ZnO doped with 1.0% Al and In, supporting its potential use in photonic memory applications, such as multilevel data storage and optical programming.
This article presents an investigation into the structural, optical, and electrical properties of Indium Tin Oxide (ITO) films that were deposited utilizing various plasma powers. The transmittance values in the visible region were measured, revealing that the ITO film deposited at 2050 W exhibited the highest transmittance (81%). Additionally, the sheet resistance values of all films were analyzed, indicating that the ITO film deposited at 2050 W had the lowest sheet resistance (64.9 Ω/sq). By means of XRD analysis, the structural properties of the films were meticulously scrutinized, and the distinctive diffraction peaks associated with the ITO films were successfully identified. Notably, the ITO film deposited at 2050 W demonstrated superior performance compared to the other films deposited using various plasma powers. Finally, we report a noteworthy efficiency of 17.03% achieved in the SHJ solar cell fabricated with the ITO film deposited at 2050 W on a 5x5 cm2 n-type Si substrate.