Radiative cooling, an emerging technology that reflects sunlight and emits radiation into outer space, has gained much attention due to its energy-efficient nature and broad applicability in buildings, photovoltaic cells, and vehicles. This study focused on fabricating SiO2-polymethyl methacrylate (PMMA) and TiO2-SiO2-PMMA thick films via the blade-coating method. The investigation aimed to improve cooling performance by adding TiO2 particles to increase the coverage area and utilize the TiO2 reflectance ability. The characterizations of the emissivity/absorptivity, solar reflectance, and microstructure of the thick films were conducted by using ultraviolet–visible/near-infrared (UV-Vis/NIR) diffuse reflection spectroscopy and scanning electron microscopy, respectively. Experimental results revealed that the maximum temperature drops of approximately 9.4 and 9.8 °C were achieved during the daytime period for SiO2-PMMA and TiO2-SiO2-PMMA thick films. The total solar radiation reflectivity increased from 71.7 to 75.6% for SiO2-PMMA radiative cooling thick films after adding TiO2. These findings underscored the potential of TiO2-SiO2-PMMA thick films in advancing radiative cooling technology and cooling capabilities across various applications.
The freeze-drying method creates a scaffold with a composite mesoporous structure with many advantages. However, everyday materials such as β-tricalcium phosphate (β-TCP) have been used as an orthopedic implant for canine tribal bone defects for decades, for instance, for grafting material of even shapes to form an implant for our teeth. However, this material is still not entirely expected to be the best implant due to its high biodegradability. Besides that, using the piezoelectric effect on the bone can lead to more efficiency in cell growth and a faster healing time for patients. Based on this phenomenon, a scaffold composite with a piezoelectric material such as barium titanate (BaTiO3/BT) has been tested. Based on the BT/β-TCP ratio, the scaffold composite of BT and β-TCP produces a porous structure with porosity ranging from 30.25 ± 11.28 to 15.25 ± 11.28 μm. The BT/β-TCP ratio influences the samples’ pore type, which affects each sample’s mechanical properties. In our result, the scaffold of 45.0 wt% BT/45.0 wt% β-TCP/10.0 wt% collagen has achieved a significant value of 0.5 MPa for maximum stress with a sufficient pore size of 25.32 ± 8.05 μm. Finally, we performed a viability test to see the sample’s piezoelectric effect, which showed that the piezoelectric effect does increase bone healing time when tested by growing MC3T3-E1 cells on the samples.
Biocomposite materials are widely implemented in various applications in clinical dentistry and orthopedics since it is possible to combine multiple materials by relying on their compatibility. Ceramic-based materials have osteogenic and osteoconductive features owing to their inorganic constituents with dental and bone tissue. β-tricalcium phosphate (β-TCP) and bioactive glass have excellent biocompatibility, bioresorbability, and bioactivity. In this study, β-TCP and BG powders were fabricated by spray pyrolysis (SP) and spray drying (SD). These fabrication methods are suitable for the mass production and synthesis of spherical particles. At first, β-TCP and BG spherical particles were synthesized by SP and characterized using X-ray diffraction (XRD), Fourier transform infrared spectroscopy (FT-IR), and scanning electronic microscopy (SEM). After that, these powders were granulated with the different weight ratios of β-TCP/BG = 100/0, 75/25, 50/50, 25/75, and 0/100 by SD. The resulting granulation powders were characterized using XRD, FT-IR, and SEM to investigate phase compositions and microstructures. In addition, cytotoxicity was investigated using the MTT assay.