Celso Cruz

Dr. Celso Cruz

orcid

Research Focus & Metrics

Academic Career Length

10Years (2017-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
2 January 2024 in The International Journal of Advanced Manufacturing Technology
Verified
Journal Article
Closed access
PDF file
CFChristian Félix-Martínez
Christian Félix-Martínez
JSJuan Manuel Salgado-López
Juan Manuel Salgado-López
ALAldo López-Martínez
Aldo López-Martínez
LGLuis Daniel García-Salas
Luis Daniel García-Salas
JGJuan González-Carmona
Juan González-Carmona
CCCelso Cruz
Celso Cruz

21 June 2024 in Applied Sciences
Verified
Journal Article
Open access
PDF file
IFISIDRO GUZMAN FLORES
ISIDRO GUZMAN FLORES
EGEverardo Efren Granda-Gutierrez
Everardo Efren Granda-Gutierrez
CCCelso Cruz
Celso Cruz
Héctor Manuel Hdz-GarcíaHéctor Manuel Hdz-García
Héctor Manuel Hdz-García
JDJ.C. Díaz-Guillén
J.C. Díaz-Guillén
DMDORA IRMA MARTINEZ
DORA IRMA MARTINEZ
This research investigates the heat treatment parameters of 6061-aluminum alloy to enhance its mechanical properties. The Taguchi design-of-experiments (DOE) method was employed to systematically examine the effects of solutionizing temperature, solutionizing time, aging temperature, and aging time on the tensile strength of the alloy. Mechanical testing suggested a major influence of solutionizing and aging temperatures on the ultimate tensile strength of the alloy. The samples subjected to a solutionizing temperature of 540 °C for 3 h, followed by aging at 170 °C for 18 h, exhibited the highest ultimate tensile strength (293.7 MPa). Conversely, the samples processed at the lowest levels of these parameters displayed the lowest ultimate tensile strength (193.7 MPa). Microstructural analysis confirmed the formation of equiaxed grains, strengthening precipitates, precipitate clusters, and β (Mg2Si) precipitates alongside Fe-Al-Si dispersoids. Energy-dispersive X-ray spectroscopy (EDS) analysis detected the presence of elemental precursors of β phase (Al-Mg-Si) and dispersoid-forming elements (Al-Fe-Si). X-ray diffraction spectroscopy (XRD) analysis revealed the persistence of the β phase in the alloy, indicating its contribution to the improved mechanical properties, which are mainly obtained by aging precipitation phases. Fracture analysis showed a ductile fracture mechanism, and examining fractured samples supported the findings of enhanced tensile properties resulting from the adequate selection of heat treatment parameters. We employed ANOVA (analysis of variance) to analyze the DOE results, using a multiple regression model to express the ultimate tensile strength of the alloy in terms of the variables used in the design. This yielded an adjusted coefficient of determination of 89.75%, indicating a high level of explained variability in the test data for evaluating the model’s predictive capacity.

1 March 2017 in Soldagem & Inspeção
Verified
Journal Article
Open access
PDF file
IFISIDRO GUZMAN FLORES
ISIDRO GUZMAN FLORES
BVBenjamin Vargas-Arista
Benjamin Vargas-Arista
JGJuan Jose Gasca-Dominguez
Juan Jose Gasca-Dominguez
CCCelso Cruz
Celso Cruz
MGMarco Antonio González-Albarrán
Marco Antonio González-Albarrán
JPJoaquin del Prado-Villasana
Joaquin del Prado-Villasana
The effect of torch weaving on the microstructure, tensile strength, impact resistance and fracturing in robotic welded joints using varing welding speeds, voltages and currents was evaluated through fractography using scanning electron microscopy, tension, impact and micro-hardness tests and optic microscopy. Results indicated that linear, sinusoidal and circular weavings favored an increase of the width of the HAZ as well as a slight increase in yield resistance accompanied by hardening in comparison with a triangular weave. The latter favored larger impact energy in the HAZ with less width, containing coarse-grained ferrite due to lower tensile strength and Vickers hardness. A circular weave generated the highest level of hardening and the lowest energy absorbed in the HAZ as a consequence of an increase in yield strength related to the fine needles of acicular ferrite. A linear weave favored the greatest width of the HAZ compared with other weld weavings due to heat accumulation along the fusion line of the welded joint. Hardening and loss of toughness were evaluated through fractographic analysis showing mixed fractures mainly composed of brittle fracturing made by transgranular cleavages with facets containing well defined river patterns.

8 September 2022 in Materials
Verified
Journal Article
Open access
PDF file
IFISIDRO GUZMAN FLORES
ISIDRO GUZMAN FLORES
EGEverardo Efren Granda-Gutierrez
Everardo Efren Granda-Gutierrez
CCCelso Cruz
Celso Cruz
DMDORA IRMA MARTINEZ
DORA IRMA MARTINEZ
BVBenjamín Vargas
Benjamín Vargas
LFLeonardo FLORES
Leonardo FLORES
In this paper, the analysis of electrochemical corrosion performance and mechanical strength of weld joints of aluminum 6061 in two-heat treatment conditions was performed. The joints were produced by gas metal arc welding in pulsed mode. The original material exhibited precipitates of β and β” phases in a volume fraction (Vf) of 2.35%. When it was subjected to a solubilization process, these phases were present in a Vf = 2.97%. This increase is due to their change in shape and distribution in clusters within the aluminum matrix. After the welding process, the best sample in the solubilization condition reached 117 MPa, while the original material achieved 104 MPa, but all samples showed a fracture in the fusion zone. This is attributed to the heat input that produces high and low hardness zones along the heat-affected zone and the welding zone, respectively. Moreover, the change in microstructure and phase composition creates a galvanic couple, susceptible to electrochemical corrosion, which is more evident in the heat-affected zone than in the other weld regions, exhibiting uniform and localized corrosion, as was evident by electrochemical impedance spectroscopy. The heat from the welding process negatively affects the corrosion resistance, mainly in the heat-affected zone.

19 February 2020 in Continuum Mechanics and Thermodynamics
Verified
Journal Article
Closed access
PDF file
CCCelso Cruz
Celso Cruz
Alireza Akhavan-SafarAlireza Akhavan-Safar
Alireza Akhavan-Safar
LSL. F. M da Silva
L. F. M da Silva
MAM. R. Ayatollahi
M. R. Ayatollahi

22 October 2020 in Journal of Adhesion Science and Technology
Verified
Journal Article
Closed access
CCCelso Cruz
Celso Cruz
BVBenjamin Vargas
Benjamin Vargas
SCSelene Capula
Selene Capula
GTGerardo Terán
Gerardo Terán
IFISIDRO GUZMAN FLORES
ISIDRO GUZMAN FLORES
EGEverardo Efren Granda-Gutierrez
Everardo Efren Granda-Gutierrez
An alternative of repairment by means of Lord DC-80 adhesive and metallic patch on two API5L-X52 pipes steel with 10 mm in thickness, 122 mm outside diameter and 750 mm length, which were damaged by mechanically longitudinal crack with 5 mm depth is presented. Repaired pipes were submitted to pressure testing (0.68–9.8 MPa) and 3D-FEM was used to calculate the Von Mises stress and strain. Results indicated that measured strain was smaller than the allowed strain, then no yielding occurred. Pressure tests revealed that leakage occurred at 9.8 MPa, where seals failed but not the pipe or repaired assembly. FEM results showed that the adhesive served to join the steel patch and pipeline, which operated as a component that lead to lower stresses regarding to the internal pressure in pipeline. The Von Mises stress values increased with the increment of pressure resulting that for 9.8 MPa, the greatest stress was reached at both edges of the API-X52 piping, followed by metallic patch and finally, the adhesive with the lowest values. Cracked pipelines within the analyzed dimension sizes did not present integrity problems and it did not fail. This kind of repairment could be safely used for pipes that present external defects.