Kawkb Mohammed El tamimi

Dr. Kawkb Mohammed El tamimi

orcid

Research Focus & Metrics

Academic Career Length

5Years (2022-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
12 January 2022 in Polymers
Verified
Journal Article
Open access
PDF file
KTKawkb Mohammed El tamimi
Kawkb Mohammed El tamimi
DBDalia A. Bayoumi
Dalia A. Bayoumi
Mohamed Mohamed Zaky AhmedMohamed Mohamed Zaky Ahmed
Mohamed Mohamed Zaky Ahmed
IAIbrahim Albaijan
Ibrahim Albaijan
MEMohammed E. El-Sayed
Mohammed E. El-Sayed
The wear of acrylic denture teeth is a serious problem that can change the vertical dimensions of dentures. This study evaluates the effect of adding salinized nano ZrO2 particles on the microstructure, hardness, and wear resistance of acrylic denture teeth. Heat polymerizing polymethyl methacrylate resin was mixed with salinized ZrO2 at concentrations of 5 wt.% and 10 wt.%. Acrylic resin specimens without filler addition were used as a control group. SEM/EDS analyses were performed and the Vickers’ hardness was evaluated. Two-body wear testing was performed using a chewing simulator with a human enamel antagonist. After subjecting the samples to 37,500 cycles, both height loss and weight loss were used to evaluate the wear behavior. The microstructural investigation of the reinforced-denture teeth indicates sound nanocomposite preparation using the applied regime without porosity or macro defects. The addition of zirconium oxide nanofillers to PMMA at both 5% and 10% increased the microhardness, with values of up to 49.7 HV. The wear mechanism in the acrylic base material without nanoparticle addition was found to be fatigue wear; a high density of microcracks were found. The addition of 5 wt.% ZrO2 improved the wear resistance. Increasing the nanoparticles to 10 wt.% ZrO2 further improved the wear resistance, with no microcracks found.

1 June 2024 in The Saudi Dental Journal
Verified
Journal Article
Open access
KTKawkb Mohammed El tamimi
Kawkb Mohammed El tamimi
DBDalia A. Bayoumi
Dalia A. Bayoumi
RARafif AlShenaiber
Rafif AlShenaiber
IAIBRAHIM ALJULAYFI
IBRAHIM ALJULAYFI
Mohamed Mohamed Zaky AhmedMohamed Mohamed Zaky Ahmed
Mohamed Mohamed Zaky Ahmed
MEMohammed E. El-Sayed
Mohammed E. El-Sayed
This in vitro study aimed to evaluate the additive manufacturing (AM) of cobalt chromium Co-Cr and titanium Ti alloy clasps for clinical use. After scanning the Ni-Cr die of the first molar, Akers' clasps were designed using computer-aided design/ computer-aided manufacturing (CAD/CAM). The clasps were manufactured from Co-Cr-W dental alloy and Ti-6Al-4V alloy powder using AM machines. Then, they were divided into two groups. The initial retentive force of the clasps was measured using a universal testing machine. Cyclic loading of the clasps was carried out by a specially designed insertion-removal testing apparatus in wet condition up to 5000 cycles. Retentive force was measured at 1000, 2000, 3000, 4000, and 5000 cycles. Moreover, the intaglio surface of each clasp was scanned using the scanner; and superimposition between the pre- and post-cycling clasp files was performed to evaluate deformation after cyclic loading. The fitting surfaces of retentive clasp tips were examined with a scanning electron microscope (SEM). Finally, it has been found that the initial retentive force for the Co-Cr group was 10.81 ± 0.37 N, and for the Ti group was 5.41 ± 0.18 N. Additionally, during the testing periods, both Co-Cr and Ti clasps continued to lose retentive force within the cycles of placement and removal. This effect was more prominent in the Co-Cr than in the Ti clasps. The distances between pre- and post-cycling in the retentive arm were -0.290 ± 0.11 mm and -0.004 ± 0.01 mm in Co-Cr and Ti alloys, respectively, and in the reciprocal arm were -0.072 ± 0.04 mm and -0.032 ± 0.04 mm in Co-Cr and Ti alloys, respectively. The retentive force required to remove the Ti clasps was found to be significantly lower than those required to dislodge the Co-Cr clasps. Co-Cr and Ti clasps lost significant amounts of retentive force from the initial use to the 3.5-year periods of simulated clinical use.

22 July 2024 in Journal of Prosthodontics
Verified
Journal Article
Closed access
MEMohammed E. Elsayed
Mohammed E. Elsayed
DEDalia A. El‐Bayoumi
Dalia A. El‐Bayoumi
AHAhmed M. Hebeshi
Ahmed M. Hebeshi
KTKawkb Mohammed El tamimi
Kawkb Mohammed El tamimi

25 May 2026 in BMC Oral Health
Verified
Journal Article
Open access
KTKawkb Mohammed El tamimi
Kawkb Mohammed El tamimi
DBDalia A. Bayoumi
Dalia A. Bayoumi
MAMohamed M. Z. Ahmed
Mohamed M. Z. Ahmed
MHMohamed I. A. Habba
Mohamed I. A. Habba
SZSherif E. Zahra
Sherif E. Zahra
MEMohammed E. El-Sayed
Mohammed E. El-Sayed
Background: Additive manufacturing of cobalt–chromium (Co–Cr) and titanium (Ti-6Al-4 V) alloys is increasingly used in prosthetic dentistry. Acidic oral environments associated with gastroesophageal reflux disease (GERD) may negatively influence the surface integrity and corrosion resistance of dental materials. This in vitro study assessed the effects of simulated gastric acid on the corrosion resistance, surface morphology, and topographical changes of selective laser melting (SLM) Co–Cr and Ti-6Al-4 V alloys. Methods: Thirty-two additively manufactured specimens ( n = 16 per alloy) were randomly distributed into acidic (pH 1.2) and neutral control (pH 6.7 distilled water) subgroups ( n = 8). A cyclic static immersion protocol was used to simulate GERD-related acid exposure. Specimens in the acidic group were immersed for 2 min in acidic solution, rinsed without scrubbing to preserve the delicate surface topography, and stored in distilled water at 37 °C, repeated six times daily over nine days with a 24-hour interval maintained between each daily cycle. Control specimens were stored continuously in distilled water at 37 °C. Surface morphology, elemental composition, and topography were evaluated using scanning electron microscopy (SEM) and Abbott–Firestone curve analysis. Results: In the Co–Cr alloy, immersion in an acidic solution resulted in a decrease in the percentage of all elements, except O, which increased to 6.37 ± 1.77%, with the change being statistically significant ( P ≤ 0.05). In contrast, Ti-6Al-4 V also showed a decrease in all elements after immersion, with O rising to 2.26 ± 1.22%, although no changes were statistically significant ( P ≥ 0.05). SEM images indicated more oxide deposits on Co-Cr in an acidic solution, which also showed a notable increase in surface roughness, whereas Ti-6Al-4 V exhibited greater stability. The Abbott–Firestone analysis further confirmed that Co-Cr underwent more significant changes in peak formation and exploitation zones than Ti-6Al-4 V did in acidic environments. Conclusions: Under simulated gastric acid exposure, Ti-6Al-4 V alloys exhibited superior corrosion resistance and surface stability compared with Co–Cr alloys. These findings support the clinical preference for Ti-6Al-4 V in dental restorations for patients experiencing frequent acidic challenges, such as those with severe GERD.