The inluence of the heat treatment conditions and of the time of hydrothermal treatment at 210°С on the phase composition and size of crystallites and nanoparticles of lanthanum orthophosphate (LaPO4) was considered. The heating conditions in the course of hydrothermal synthesis of LaPO4 influence the structural transition of lanthanum orthophosphate of rhabdophane structure into the phase of monazite structure, and also the particle morphology and crystallite size. The phase of monazite structure with the crystallite size of approximately 12 nm without rhabdophane impurity is formed after hydrothermal treatment at 210°С for 30 min in the case of microwave heating of the hydrothermal fluid. When using external heating of autoclaves, at the same temperature inside the autoclave, the mean size of the crystallites of the monazite phase formed is 17 nm.
23 January 2024 in Inorganic Chemistry Communications
Phase transformations during high-energy ball milling, a tool of mechanochemistry, are interesting due to the possible production of metastable phases without the need for artificially introducing high temperatures and pressures. In our work, the transformation of calcite to aragonite in an eggshell is studied in detail. The presence of organic material, in either the naturally present eggshell membrane, or artificially supplied L-cysteine, was found to be crucial for the phase transformation to occur, its decomposition leading to a pressure increase necessary for aragonite formation. The presence of sulfur in the organics seems to be crucial, as corroborated by much lower phase transformation extent when utilizing sulfur-free organics for comparison. The degree of the transformation in an eggshell was strongly dependent on the used milling conditions. The optimization was assessed using the Taguchi method, namely using a 44 orthogonal array. The optimized parameters encompassed milling time, sample mass, milling speed and duration of breaks and it was shown that sample mass has a decisive effect on the amount of obtained aragonite. Under the most efficient conditions, 73.7% of aragonite was obtained. Prolonging milling until 4 hours further boosts the transformation, reaching 89.9% of aragonite, but further milling leads to the collapse of the aragonite structure and pure calcite was observed after 5 hours.
A study of the processes in which lanthanum orthophosphate nanocrystalline powders with rhabdophane and monazite structure and crystallite size of about 10 nm are formed demonstrated that, at temperatures of up to 500°C, nanocrystalline lanthanum orthophosphate with rhabdophane structure loses crystal hydrate water and is transformed at 520–540°C to a nanocrystalline phase with monazite structure. This transition is not associated with as change in the crystallite size because nanocrystals of the anhydrous lanthanum orthophosphate phase with monazite structure retain a size of about 10 nm both at the instant of the structural transformation and up to temperatures of 600–700°C. The technological modes were determined in which nanocrystalline lanthanum orthophosphate powders with monazite structure can be obtained and the powders are used for sintering of ceramic materials with porosity on the level of 5–7%.
24 February 2025 in Journal of Physics and Chemistry of Solids