High-entropy alloys (HEAs) are new alloy systems that leverage solid solution strengthening to develop high-strength structural materials. However, HEAs are typically cast alloys, which may suffer from large as-cast grains and entrapped porosity, allowing for opportunities to further refine the microstructure in a non-melting near-net shape solid-state additive manufacturing process, additive friction stir deposition (AFSD). The present research compares the microstructure and mechanical behavior of the as-deposited AFSD Al0.35CoCrFeNi to the cast heat-treated properties to assess its viability for structural applications for the first time. Scanning electron microscopy (SEM) revealed the development of fine particles along the layer interfaces of the deposit. Quasi-static and intermediate-rate compression testing of the deposited material revealed a significant strain-rate sensitivity with a difference in yield strength of ~400 MPa. Overall, the AFSD process greatly reduced the grain size for the Al0.35CoCrFeNi alloy and approximately doubled the strength at both quasi-static and intermediate strain rates.
Quasi-static and high-rate tensile experiments were used to examine the strain rate sensitivity of laser-directed energy deposition (L-DED)- and additive friction stir deposition (AFSD)-formed AerMet 100 ultrahigh-strength steel-additive manufactured builds. Electron backscattered diffraction (EBSD) revealed similar as-deposited grain sizes between the two AM processes at approximately 24 μm and 17 μm for the L-DED and AFSD samples, respectively. The strain hardening rate, θ, revealed little change in the overall hardening observed in the L-DED and AFSD materials, with a consistent hardening in the quasi-static samples and three identifiable regions in that of the high-rate tested materials. The L-DED deposited materials displayed average ultimate tensile strength values of 1835 and 2902 MPa for the 0.001 s−1 and 2500 s−1 strain rates, respectively and the AFSD deposited materials displayed ultimate tensile strength values of 1928 and 3080 MPa for the 0.001 s−1 and 2500 s−1 strain rates, respectively. Overall, the strength for both processes displayed a positive strain rate sensitivity, with increases in strength of ~1000 MPa for both processes. Fractography revealed significant solidification voids in the laser DED material and poor layer adhesion in the AFSD material.