In order to investigate the influence of recycling agent composition on the recycling effect of aged asphalt in the cold recycling process, the design and optimization of cold recycling agent composition were performed through the central composite design-response surface method combined with the dynamic shear rheometer (DSR) test and the bending beam rheometer (BBR) test. The molecular weight distribution and component changes in aged asphalt before and after the addition of a cold recycling agent were also analyzed by gel permeation chromatography (GPC) and hydrogen-flame ionization test. The results showed that the permeable cold recycling agent has a recycling effect on the aged asphalt, but its effectiveness is greatly affected by recycling agent composition. The best recycling effect was achieved when the ratio of aromatic oil and penetrant in the cold recycling agent was 61.2:38.8, respectively. In terms of the recycling agent and aromatic functional groups in the aromatic oil, the aromatics in the recycling agent are derived from the aromatic oils, and the penetrant is only fused and permeated with the aromatic oils. After the admixture of the cold recycling agent, the penetrant in the recycling agent allows the aromatic oil to enter the aged asphalt at room temperature. The light components volatilized by aging are replenished, allowing the aged asphalt to recover some of its properties.
To effectively utilize waste mask materials in road engineering and minimize resource waste, the melt-blown fabric (MBF) of waste masks was utilized to modify the virgin bitumen. The preparation process of MBF-modified bitumen was investigated, and the physical and rheological properties of bitumen were measured. Subsequently, the blending mechanism during preparation and the dispersion morphology of the modifier were explored. Finally, the pavement performance of the mixture was investigated, and a radar chart analysis was performed to quantitatively assess the effects of MBF modification. Results suggested that the recommended preparation process of shear time, shear rate, and shear temperature was 170 °C, 4000 r/min, and 15 min, respectively. MBF enhanced the high-temperature stability of the binder and weakened the temperature susceptibility. The modification was primarily a physical process. No network structure and agglomeration formed in the bitumen after modification. The addition of MBF significantly improved the resistance of the asphalt mixture to a high-temperature deformation and water damage but harmed its low-temperature crack resistance. The comprehensive assessment results of 0% (), 1% (), 3% (), and 5% () MBF to improve the properties of the mixture were in the following order: , where the impact of 3% MBF was the most significant, followed by 5% and 1% MBF.