The application potential of additive manufacturing nickel-based superalloys in aeroengines and gas turbines is extensive, and evaluating their mechanical properties is crucial for promoting the engineering application in load-bearing components. In this study, Hastelloy X alloy was prepared using the laser powder bed fusion process combined with solution heat treatment. The tensile and high cycle fatigue properties were experimentally investigated at room temperature as well as two typical elevated temperatures, 650 °C and 815 °C. It was found that, during elevated-temperature tensile deformation, the alloy exhibits significant serrated flow behavior, primarily observed during the initial stage of plastic deformation at 650 °C but occurring throughout the entire plastic deformation process at 815 °C. Notably, when deformation is small, sawtooth fluctuations are significantly higher at 815 °C compared to 650 °C. Irregular subsurface lack of fusion defects serve as primary sources for fatigue crack initiation in this alloy including both single-source and multi-source initiation mechanisms; moreover, oxidation on fracture surfaces is more prone to occur at elevated temperatures, particularly at 815 °C.
The preparation of a single crystal superalloy surface overlay welding coating to improve its high-temperature mechanical properties is of great significance for prolonging the service life of blades. This work selected two types of welding wire alloys, CoCrMo and CoCrW, to prepare coatings on the surface of a single crystal superalloy. A comparative study was conducted on their mechanical properties, such as tension, compression, fatigue, durability, and wear at a high temperature of 900 ℃, aiming to reveal the high-temperature mechanical properties of the two types of welding coatings. Results showed that the average high-temperature tensile strength of the CoCrMo welded specimen was smaller than that of the CoCrW welded specimen; the average high-temperature duration of CoCrMo welded specimens at 150 MPa was lower than the average duration of CoCrW welded specimens; the high-temperature fatigue life of CoCrMo welded specimens at 220 MPa was 7.186 × 105; and the average high-temperature wear rate of CoCrMo sample was 3.64 × 10−6 mm3·N−1·m−1. The CoCrW alloy was more wear resistant than CoCrMo. The hardness of CoCrMo welded joints gradually increased from the substrate to the heat-affected zone and then to the fusion zone, and was much higher in the fusion zone than in the CoCrW alloy.
This work revealed the mechanism of microstructure evolution on tensile properties in selective laser melted (SLM) GH3536 superalloys in the range of room temperature to 1000 °C. The results showed that SLM-GH3536 alloy exhibited isotropic tensile properties along X, Z, and 45° directions. The carbide at the grain boundary changed from banded to granular, resulting in a significant decrease in tensile strength at elevated temperatures, and the fracture mode transitioned from a mixed fracture to transgranular fracture.
The anisotropy of mechanical properties in SLMed alloy is very important. In order to realize the homogeneity of the microstructure and mechanical properties of GH3536 alloy prepared by selective laser melting (SLM), the as-deposited samples were treated by hot isostatic pressing and then forged at different temperatures. The microstructure, grain size, room- and high- temperature tensile properties, and endurance properties of the samples were studied. The results showed that the microstructure of the sample was mainly equiaxed austenite phase, and granular carbides were precipitated inside the grains after forging treatment, resulting in the anisotropy of the sample almost disappearing. The grain boundary phase difference distribution was most concentrated at 60°. The grain size was less than 10 μm, and a large number of twins were formed. With the increase in forging temperature, the yield strength, tensile strength, and contraction of area of the samples changed little, and the properties parallel to the z-axis (parallel samples) and vertical to the z-axis (vertical samples) were almost the same. In particular, the yield strength, tensile strength, and contraction of area in the transverse and vertical samples were almost at the same level. Judging from the elongation after fracture and the contraction of area, the properties of the samples showed characteristics of anisotropy after a high temperature endurance test.
This work investigated the 0Cr16Ni5Mo1 stainless steel using laser selective melting (SLM) technology and explored the effect of the tempering temperature on the microstructure and properties. After the tempering treatment, the quenched martensite transformed from a metastable to steady state, and residual austenite was formed. The results indicated that the elongation of the transverse specimen showed an upward trend as the tempering temperature increased, while the elongation of the longitudinal specimen first increased and then decreased. The fracture mode was ductile. There was an obvious fiber, radial, and shear lip zone on the fracture surface of transverse specimens. When the tempering temperature was 650 °C, the shear lip area of the fracture surface was the largest. For longitudinal specimens, there was no obvious zoning on the fracture surface.
Nickel-based GH3536 alloys prepared by laser powder bed fusion (LPBF) exhibit a mismatch between strength and ductility during the tensile process, which severely restricts their engineering applications in the aerospace field. In order to optimize their performance, this study adopted hot isostatic pressing (HIP) and subsequent heat treatment (HT) to modify the material. The microstructural evolution of the HIP+HT-treated GH3536 alloy during deformation, including grain rotation, grain boundary migration, and dislocation slip transfer behaviors, was systematically investigated at room temperature using in situ tensile experiments. The relationship between the microstructure and mechanical properties was elucidated in greater depth by combining theoretical calculations. The experimental results show that after HIP+HT treatment, the elongation of the alloy increased significantly from 36.5% in the as-built LPBF condition to 45.3 ± 1.6% without a significant reduction in ultimate tensile strength. The plasticity enhancement is mainly attributed to the elimination of defects and the formation of annealing twins. In addition, the formation of substructures inside the grains also delays the fracture of the specimen to some extent. This study is expected to provide a reference for the subsequent optimization of the mechanical properties of alloys via heat treatment processes.