For improving the wear properties of NiCrAlY, the 10 wt %, 20 wt % and 30 wt % ZrO2-added NiCrAlY samples were prepared by ultrasonic-assisted direct laser deposition, respectively. The results showed that the ultrasonic-assisted direct laser deposition can realize the ZrO2-added NiCrAlY preparation. Furthermore, due to the cavitation effect and agitation of the ultrasound in the molten pool, ultrasonic-assisted could make the upper surface of the samples smoother and flatter, and it also improved the microstructural homogeneity. The microstructure was mainly composed of columnar dendrites, and most of ZrO2 particles were located in the intergranular regions. The principal phase constituents were found to contain γ-Ni and t-NiZr2, and the amorphous (Ni, Zr) intermetallic phase generated, because of more rapid solidification after ultrasound assisted. The microhardness was improved slightly with the increase of ZrO2 contents, rising from 407.9 HV (10% ZrO2) to 420.4 HV (30% ZrO2). Correspondingly, wear mass loss was decreased with the maximum drop 22.7% of 30% ZrO2 compared to that of 10% ZrO2, and wear mechanisms were mainly abrasive wear with slightly adhesive wear. After applying ultrasound, the oxide islands in samples disappeared, and more ceramic particles were retained. Thus, the hardness and wear performance of the samples were improved.
The preparation of a single crystal superalloy surface overlay welding coating to improve its high-temperature mechanical properties is of great significance for prolonging the service life of blades. This work selected two types of welding wire alloys, CoCrMo and CoCrW, to prepare coatings on the surface of a single crystal superalloy. A comparative study was conducted on their mechanical properties, such as tension, compression, fatigue, durability, and wear at a high temperature of 900 ℃, aiming to reveal the high-temperature mechanical properties of the two types of welding coatings. Results showed that the average high-temperature tensile strength of the CoCrMo welded specimen was smaller than that of the CoCrW welded specimen; the average high-temperature duration of CoCrMo welded specimens at 150 MPa was lower than the average duration of CoCrW welded specimens; the high-temperature fatigue life of CoCrMo welded specimens at 220 MPa was 7.186 × 105; and the average high-temperature wear rate of CoCrMo sample was 3.64 × 10−6 mm3·N−1·m−1. The CoCrW alloy was more wear resistant than CoCrMo. The hardness of CoCrMo welded joints gradually increased from the substrate to the heat-affected zone and then to the fusion zone, and was much higher in the fusion zone than in the CoCrW alloy.
1 October 2019 in IOP Conference Series: Materials Science and Engineering
Using selective laser melting technique, 3 sets of GH4169 samples were formed by various laser power and scanning speed to prepare mechanical properties test specimens. The defects and porosity of the samples were measured by CT inspection. The tensile test was carried out at room temperature. The fracture morphology of the tensile samples was observed by SEM and the fracture mechanism was analyzed. The results show that some samples have pores with largest size of 100μm, which have no effect on the subsequent tensile properties test. The tensile strength does not change significantly with the varying process parameters, and the highest strength could reach 1480MPa. The elongation and the reduction of area decrease gradually as the scanning speed increases, indicating that the plasticity of the material is descending. The fracture mechanism of the three sets specimens are ductile fractures, and the microscopic morphology shows distribution of equiaxed dimples.
Three types of CoCr alloy welding wires were deposited on the surface of a single-crystal alloy using gas tungsten arc-welding (GTAW) technology to enhance its wear resistance. Comparative studies were conducted on the microstructure, microhardness, friction and wear properties, and tensile properties of the deposited alloy layers. The results showed that the deposited CoCr alloy layers formed good metallurgical bonding with the substrate, and the microstructure mainly consisted of planar crystals, coarse columnar dendrites, and fine, dense equiaxed dendrites. The microhardness of joints formed by depositing CoCr alloy welding wires increased with increasing distance from the interface, exhibiting a distribution pattern where the center of the deposition layer had the highest hardness, followed by the interface, while the base material had the lowest hardness. The highest hardness of the deposited layers of the S1 alloy was 119.5 HRC, with significant fluctuations in the deposition layer area. The wear resistance was significantly improved after depositing, and decreased significantly with increasing service temperature. The tensile strengths of the three welding wires were similar. The joint strength gradually decreased as the test temperature increased, with the S12 alloy joint exhibiting superior performance at high temperatures.
To improve the high-temperature service performance of cladding layers on DD5 single crystal superalloy, this study comparatively investigated the effects of two cobalt-based filler wires, PMet931 and PMet994, on the microstructural evolution, hardness, high-temperature tensile properties, and friction and wear behavior of the cladding layers. The results show that PMet931, with a higher Ni content, exhibits better compositional compatibility and interfacial metallurgical compatibility with the DD5 Ni-based substrate. In contrast, the higher W, C, and Cr contents in PMet994 promote the formation of W/Cr-rich secondary phases and grain refinement, resulting in higher hardness and better high-temperature strength retention. Both filler wires can form continuous cladding layers on the DD5 surface. The PMet931 cladding layer shows a more homogeneous microstructure and a smoother interfacial transition, whereas the PMet994 cladding layer contains more secondary phases and exhibits more pronounced strengthening features. Mechanical testing indicates that PMet931 provides a better strength ductility balance at room temperature, while PMet994 shows higher strength and hardness retention over the range of 800–1050 °C, with a tensile strength at 1050 °C approximately 53% higher than that of PMet931. The friction and wear results show that the wear rate of the PMet994 cladding layer was significantly lower than that of the PMet931 cladding layer at 800 °C, whereas the difference between the two cladding layers decreased at higher temperatures. This study demonstrates that filler wire composition significantly affects the high-temperature performance of DD5 cladding layers by regulating secondary phase precipitation, interfacial compatibility, and microstructural stability.
CoCrMo-based alloy wires manufactured by powder metallurgy and casting processes for wear-resistant coatings of aerospace turbine blades are taken as the research objects in this study, and TIG hardfacing experiments are carried out. Microstructure characteristics of the two wires are systematically compared. Furthermore, microstructure differences among the hardfaced layer, transition zone and base metal are analyzed. High-temperature hardness, tensile strength, and stress rupture resistance, as well as friction and wear properties, are measured. The results indicate that favorable weldability is possessed by both wires, whereas obvious discrepancies are found in the morphology of the Laves phase. Better comprehensive mechanical properties are exhibited by hardfaced specimens deposited with powder metallurgy wire. Slightly superior friction and wear properties are shown by hardfaced specimens from cast wire. The intrinsic relationships among wire manufacturing processes, hardfaced specimen microstructures and mechanical properties are elucidated in this study. Theoretical guidance and experimental support are provided for the structural design and engineering application of CoCrMo-based alloy wires.