The interest in inorganic foundry binders has been rising steadily in recent times due to their favorable environmental characteristics. This paper compares the mold quality and cast quality attained with different inorganic binders. Three different types of sand and five different inorganic binders were used for the mold quality study. Of the inorganic binders, there was liquid sodium silicate used in different hardening methods, a geopolymer binder, and also solid sodium silicate. The mold quality was assessed through bending strength, residual bending strength, tensile strength, and loss on ignition measurement. A total of 12 castings were made using molds of different binders and sand materials. The cast quality was then assessed by tracking changes in dimension and the surface quality of final castings. Inorganic binders performed well in terms of mold strength and very well in terms of loss on ignition but there is room for improvement in the surface quality of the castings attained.
11 June 2020 in International Journal of Metalcasting
Efficient manufacturing of tooling and patterns is an essential part of a good foundry process. Traditional patternmaking methods have been honed to almost perfection during the years. Additive manufacturing has been growing as an industry and presents many new possibilities for the foundry industry. However, many additive manufacturing technologies do not currently provide usable sizes and scales for foundries to properly use. Fused granular fabrication (FGF) in conjunction with finish machining might provide an answer to this issue, with printing volumes and speeds many times of those compared to filament-based fused deposition modeling printing. In this work, some traditional patternmaking materials are compared to a FGF manufactured one based on polylactic acid and cellulose blend, and their characteristics are discussed. 3D scanning of as-printed geometry shows variations inherent to material extrusion methods, while the final machined state shows comparable results to traditional polyurethane model material. The combination of high-volume material extrusion with machining to final dimensions might allow more utilization of additive manufacturing in patternmaking, especially when combined with high-performance polymer materials.
20 October 2017 in International Journal of Metalcasting
Renewed interest in inorganic binders for sand molding has also intensified research on different forms of it. In this study, solid inorganic sodium silicate binder was tested with different additives to see how these affected the silica mold quality. The five additives used were: glucose, sucrose, boric acid, aluminum oxide and iron(III)oxide powders. The mold quality was assessed through tests like bending strength, tensile strength, hot distortion, wear resistance, gas evolution and collapsibility tests. In addition, SEM imaging was done on some select mold fracture samples. In the end, a casting trial was carried out followed by a surface roughness and defects analysis. A reduction in mold strength was noticed with glucose and boric acid, while collapsibility was improved by glucose, sucrose and boric acid additives. Casting trials have shown the best surface finish to be obtained with sucrose additive. All the casts in general showed some penetration; however, repeat casts have proven that altering some casting parameters could result in casts with excellent surface finish using solid silicates.
5 November 2019 in Materials Science and Technology
The influence of ferritic and pearlitic microstructures to dynamic strain aging (DSA) of ductile iron was investigated by means of strain-controlled cyclic tests performed at temperatures ranging from room temperature to 450°C, strain rates of 10−5 to 10−2 s−1 and at three different strain amplitudes along with tensile tests. Results indicated that all tested microstructures exhibit strain aging effects at elevated temperatures in some form, similar to ferritic-pearlitic steels. Additionally, static tensile tests show hardening at intermediate temperatures, minima in elongation and serrations in stress–strain curves. Cyclic data indicates DSA related changes in stresses at 250°C and 350°C at smaller strain rates, while the effects become more suppressed at higher strain rates.