This review presents a comprehensive update of the biopolymer poly(3-hydroxybutyrate-co-3-hydroxyvalerate) (PHBV), emphasizing its production, properties, and applications. The overall biosynthesis pathway of PHBV is explored in detail, highlighting recent advances in production techniques. The inherent physicochemical properties of PHBV, along with its degradation behavior, are discussed in detail. This review also explores various blends and composites of PHBV, demonstrating their potential for a range of applications. Finally, the versatility of PHBV-based materials in multiple sectors is examined, emphasizing their increasing importance in the field of biodegradable polymers.
This study explores the characterization and application of poly(3-hydroxybutyrate-co-3-hydroxyvalerate) (PHBV) synthesized from organic residues, specifically milk and molasses. Six PHBV samples with varying 3-hydroxyvalerate (3HV) content (7%, 15%, and 32%) were analyzed to assess how 3HV composition influences their properties. Comprehensive characterization techniques, including NMR, FTIR, XRD, DSC, TGA, and tensile-stress test, were used to evaluate the molecular structure, thermal properties, crystalline structure, and mechanical behavior. Selected PHBV samples were fabricated into nanofibrous scaffolds via electrospinning, with uniform fibers successfully produced after parameter optimization. The electrospun scaffolds were further analyzed using DSC, GPC, and SEM. Biological evaluations, including cytotoxicity, in vitro drug release, and antibacterial activity tests, were also conducted. The results indicate that the electrospun PHBV scaffolds are biocompatible and exhibit promising properties for biomedical applications such as tissue engineering and drug delivery. This study demonstrates the potential of using organic residues to produce high-value biopolymers with tailored properties for specific applications.
This study investigates the impact of various nucleating agents on the crystallization behavior, thermal stability, and mechanical properties of poly(3-hydroxybutyrate-co-3-hydroxyhexanoate) (P3HBHHx) with 6 mol% 3-hydroxyhexanoate (3HHx) units. Nucleating agents, including boron nitride (BN), poly(3-hydroxybutyrate) (PHB), talc, ultrafine cellulose (UFC), and an organic potassium salt (LAK), were incorporated to enhance the crystallization performance. Differential scanning calorimetry (DSC) revealed that BN and PHB significantly increased the crystallization temperature and reduced the crystallization time by half, with BN exhibiting the highest nucleation efficiency. Isothermal kinetics modeled using the Avrami and Lauritzen–Hoffman theories confirmed faster crystallization and reduced nucleation barriers in nucleated samples. Polarized optical microscopy (POM) revealed that the nucleating agents altered the spherulite morphology and increased the growth rates. Under fast cooling, only BN induced crystallization, confirming its superior nucleation activity. Thermogravimetric analysis (TGA) indicated minimal changes in thermal stability, while mechanical testing showed a slight reduction in stiffness without compromising the tensile strength. Overall, BN emerged as the most effective nucleating agent for enhancing the P3HBHHx crystallization kinetics, providing a promising strategy for improving processing efficiency and reducing the cycle times in industrial applications.
This study explores the characterization and application of poly(3-hydroxybutyrate-co-3-hydroxyvalerate) (PHBV) synthesized from organic residues, specifically milk and molasses. Six PHBV samples with varying 3-hydroxyvalerate (3HV) content (7%, 15%, and 32%) were analyzed to assess how 3HV composition influences their properties. Comprehensive characterization techniques, including NMR, FTIR, XRD, DSC, TGA, and tensile-stress test, were used to evaluate the molecular structure, thermal properties, crystalline structure, and mechanical behavior. Selected PHBV samples were fabricated into nanofibrous scaffolds via electrospinning, with uniform fibers successfully produced after parameter optimization. The electrospun scaffolds were further analyzed using DSC, GPC, and SEM. Biological evaluations, including cytotoxicity, in vitro drug release, and antibacterial activity tests, were also conducted. The results indicate that the electrospun PHBV scaffolds are biocompatible and exhibit promising properties for biomedical applications, such as tissue engineering and drug delivery. This study demonstrates the potential of using organic residues to produce high-value biopolymers with tailored properties for specific applications.
Ultrasound micromolding (USM) is an emerging processing technology that offers advantages with regard to spatial resolution, material savings, minimum time residence, minimum exposure to high temperatures, and low cost. Recent advances have been focused on nodal point technology, which improves the homogeneity of the molded samples and the repeatability of the properties of processed specimens. The present work demonstrates the suitability of a modified USM technology to process the biodegradable poly(3-hydroxybutyrate) (P3HB), which is a polymer that has well-reported difficulties when processed by conventional methods. Specifically, conventional injection, microinjection, and USM technologies with and without nodal point configurations have been compared. Degradation studies and the evaluation of thermal and mechanical properties confirmed the successful preparation of P3HB microspecimens, maintaining their functional integrity with minimal molecular weight loss. Exfoliated clay structures were observed for P3HB nanocomposites incorporating the C20 and C166 clays and processed by USM. The results highlight the advantages of the modified USM technology, as conventional microinjection failed to produce nanocomposites of P3HB/C116 due to the enhanced degradation caused by C116.
Ultrasound micromolding (USM) is an emerging processing technology that offers advantages concerning spatial resolution, material saving, minimum time residence, minimum exposition to high temperatures and low cost. Recent advances have been focused to the point nodal tech-nology, which improves the homogeneity of the molded samples and the repeatability of the properties of processed specimens. The present work demonstrates the suitability of the modi-fied USM technology to process the biodegradable poly(3-hydroxybutyrate) (P3HB), which is a polymer that has well reported difficulties to be processed by conventional methods. Specifical-ly, conventional injection and microinjection, and USM technologies with and without point nodal configurations have been compared. Degradation studies and the evaluation of thermal and mechanical properties confirmed the successful preparation of P3HB micro-specimens, maintaining their functional integrity with minimal molecular weight loss. Exfoliated clay structures were observed for P3HB nanocomposites incorporating the C20 and C166 clays and processed by USM. The results point out the advantages of using the modified USM technology since C116 enhanced the P3HB degradation and consequently processed specimens were impos-sible to be obtained by conventional microinjection.