Full metal-ceramic composite beads containing different amounts of niobium and alumina, particularly 100 vol% alumina, 100 vol% niobium, and 95/5 vol% niobium/alumina, were produced by the alginate gelation process. The suspension for bead fabrication contained sodium alginate as gelling agent and was added dropwise into a calcium chloride solution to trigger the consolidation process. After debinding in air, sintering of the composite beads was performed under inert atmosphere. Samples in green and sintered state were analyzed by digital light microscopy and scanning electron microscopy equipped with energy dispersive X-ray spectroscopy. Investigations by mercury intrusion porosimetry revealed that pure alumina beads featured smaller pores compared to composite beads, although the open porosities were comparable. The fracture strength was evaluated on single beads. Contrary to the pure alumina, the composite beads showed a clear plastic deformation. Pure niobium beads showed a ductile behavior with very large deformations. XRD analyses revealed the presence of calcium hexaluminate and beta-alumina as minor phases in the alumina beads, while the composite ones contained about 25 wt% of impurities. The impurities comprised NbO arising from the oxidation, and β-Nb2C, from the reaction with the residual sodium alginate.
The objective of this study was to investigate the variability of flexural strength for flame-sprayed ceramic components and to determine which two-parametric distribution function was best suited to represent the experimental data. Moreover, the influence of the number of tested specimens was addressed. The stochastic nature of the flame-spraying process causes a pronounced variation in the properties of potential components, making it crucial to characterise the fracture statistics. To achieve this, this study used two large data sets consisting of 1000 flame-sprayed specimens each. In addition to the standard Weibull approach, the study examined the quality of representing the experimental data using other two-parametric distribution functions (Normal, Log-Normal, and Gamma). To evaluate the accuracy of the distribution functions and their characteristic parameters, random subsamples were generated by resampling of the experimental data, and the results were assessed based on the sampling size. It was found that the experimental data were best represented by either the Weibull or Gamma distribution, and the quality of the fit was correlated with the number of positive and negative outliers. The Weibull fit was more sensitive to positive outliers, whereas the Gamma fit was more sensitive to negative outliers.