In our study, transparent and conductive films of NiOx were successfully deposited by sol-gel technology. NiOx films were obtained by spin coating on glass and Si substrates. The vibrational, optical, and electrical properties were studied as a function of the annealing temperatures from 200 to 500 °C. X-ray Photoelectron (XPS) spectroscopy revealed that NiO was formed at the annealing temperature of 400 °C and showed the presence of Ni+ states. The optical transparency of the films reached 90% in the visible range for 200 °C treated samples, and it was reduced to 76–78% after high-temperature annealing at 500 °C. The optical band gap of NiOx films was decreased with thermal treatments and the values were in the range of 3.92–3.68 eV. NiOx thin films have good p-type electrical conductivity with a specific resistivity of about 4.8 × 10−3 Ω·cm. This makes these layers suitable for use as wideband semiconductors and as a hole transport layer (HTL) in transparent solar cells.
This work presents a facile sol–gel method for the deposition of ZnO and ZnO:Mg films. The films are spin coated on silicon and quartz substrates. The impact of magnesium concentrations (0, 0.5, 1, 2 and 3 wt%) and post-annealing treatments (300–600 °C) on the film’s structural, vibrational and optical properties is investigated. Undoped ZnO films crystallize in the wurtzite phase, with crystallite sizes ranging from 9.1 nm (300 °C) to 29.7 nm (600 °C). Mg doping deteriorates the film crystallization and shifting of 002 peak towards higher diffraction angles is observed, indicating the successful incorporation of Mg into the ZnO matrix. ZnO:Mg films (2 wt%) possess the smallest crystallite size, ranging from 6.2 nm (300 °C) to 25.2 nm (600 °C). The highest Mg concentration (3 wt%) results into a segregation of the MgO phase. Lattice constants, texture coefficients and Zn–O bond lengths are discussed. The diminution of the c lattice parameter is related to the replacement of Zn2+ by Mg2+ in the ZnO host lattice. The vibrational properties are studied by Fourier transform infrared (FTIR) spectroscopy. IR lines related to Mg–O bonds are found for ZnO:Mg films with dopant concentrations of 2 and 3 wt%. The optical characterization showed that the transmittance of ZnO:Mg thin films increased from 74.5% (undoped ZnO) to about 89.1% and the optical band gap energy from 3.24 to 3.56 eV. Mg doping leads to a higher refractive index compared to undoped ZnO films. The FESEM (field emission scanning electron microscopy) technique is used for observation of the surface morphology modification of ZnO:Mg films. The doped ZnO films possess a smoother grained surface structure, opposite to the wrinkle-type morphology of undoped sol–gel ZnO films. The smoother surface leads to improved transparency of ZnO:Mg films.
Sol-gel spin coating method was employed for depositing TiO2 and Ag-doped TiO2 films. The effects of Ag doping and the annealing temperatures (300–600 °C) were studied with respect to their structural, morphological, vibrational, and optical properties. Field Emission Scanning Electron microscopy (FESEM) investigation exhibited the grained, compact structures of TiO2-based films. Ag incorporation resulted in a rougher film surface. X-ray diffraction (XRD) results confirmed the formation of Ag nanoparticles and AgO phase, along with anatase and rutile TiO2, strongly depending on Ag concentration and technological conditions. AgO fraction diminished after high temperature annealing above 500 °C. The vibrational properties were characterized by Fourier Transform Infrared (FTIR) spectroscopy. It was found that silver presence induced changes in IR bands of TiO2 films. UV–VIS spectroscopy revealed that the embedment of Ag NPs in titania matrix resulted in higher absorbance across the visible spectral range due to local surface plasmon resonance (LSPR). Ag doping reduced the optical band gap of sol-gel TiO2 films. The optical and plasmonic modifications of TiO2:Ag thin films by the number of layers and different technological conditions (thermal and UV treatment) are discussed.
A sol–gel deposition approach was applied for obtaining nanostructured Li-doped ZnO thin films. ZnO:Li films were successfully spin-coated on quartz and silicon substrates. The evolution of their structural, vibrational, and optical properties with annealing temperature (300–600 °C) was studied by X-ray diffraction (XRD), Fourier Transform Infrared (FTIR), UV-VIS spectroscopic, and field emission scanning electron microscopic (FESEM) characterization techniques. It was found that lithium doping maintains the wurtzite arrangement of ZnO, with increasing crystallite sizes when increasing the annealing temperature. Analysis of the FTIR spectra revealed a broad main absorption band (around 404 cm−1) for Li-doped films, implying the inclusion of Li into the ZnO lattice. The ZnO:Li films were transparent, with slightly decreased transmittance after the use of higher annealing temperatures. The porous network of undoped ZnO films was transformed to a denser, grained, packed structure, induced by lithium doping.
TiO2 and TiO2-NiO films were successfully derived by a sol–gel dip coating technology. The impact of the thermal treatments (300–600 °C) on the structural, optical and electrochromic properties was investigated. X-ray diffraction (XRD) analysis showed that TiO2 films were polycrystalline and evolved in the anatase phase. The composite TiO2-NiO films, treated at annealing temperatures below 500 °C, contained anatase titania, a small inclusion of cubic NiO and an amorphous fraction. The formation of NiTiO3 was exposed after the highest annealing at 600 °C. The presence of Ti-O-Ni bonds was determined in the composite films by Fourier-transform infrared (FTIR) spectroscopy. The optical properties and the optical band gap of TiO2-NiO films were investigated and discussed. The transparency of the electrochromic TiO2-NiO films was 76.8 and 78.3% in the 380–700 nm spectral range after film thermal treatments at 300 and 500 °C. NiO incorporation led to the narrowing of the optical band gap. The electrochromic (EC) properties of the composite films were improved compared to TiO2 films. They had higher diffusion coefficients. Their color efficiencies are 37.6 (550 nm) and 52.2 cm2/C (600 nm).